# US 2025/0161883 A1 · Porous hollow fiber membrane and method for producing porous hollow fiber membrane

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0161883 A1
- Document ID: US20250161883A1
- Status: Published application
- Kind: A1
- Application number: 18/953,113
- Filed: 2024-11-20
- Published: 2025-05-22
- Earliest claimed: 2023-11-21
- Assignees: Asahi Kasei Kabushiki Kaisha
- Applicants: Asahi Kasei Kabushiki Kaisha
- Inventors: Norihito TANAKA; Yuki MIKI
- Web page: https://patentgrep.com/patent/US20250161883A1

## CPC

- B01D 69/08: Hollow fibre membranes (manufacture of hollow fibres D01D5/24, D01F1/08)
- B01D 67/0018: {Thermally induced processes [TIPS]}
- B01D 67/0027: {by stretching}
- B01D 67/003: {by selective elimination of components, e.g. by leaching}
- B01D 69/02: characterised by their properties
- B01D 71/34: Polyvinylidene fluoride
- B01D 2323/20: Plasticizers
- B01D 2323/24: Use of template or surface directing agents [SDA]
- B01D 2323/30: Cross-linking
- B01D 2323/34: Use of radiation
- B01D 2325/24: Mechanical properties, e.g. strength
- B01D 2325/52: Crystallinity
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)

## Abstract

The present disclosure provides a porous hollow fiber membrane that exhibits blocking performance and water permeability performance suitable for filtration applications, as well as having excellent chemical resistance. In order to provide a solution to the above issue, the porous hollow fiber membrane of the present disclosure is made of a thermoplastic resin, wherein the crystallization onset temperature is 140° C. or lower, and the enthalpy of crystal fusion at and below the crystallization onset temperature is 10 J/g or less.

## Claims

### Claim 1

A porous hollow fiber membrane made of a thermoplastic resin,
wherein a crystallization onset temperature is 140° C. or lower, and an enthalpy of crystal fusion at and below the crystallization onset temperature is 10 J/g or less.

### Claim 2 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein the enthalpy of crystal fusion of the entire porous hollow fiber membrane is less than 58 J/g.

### Claim 3 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein the enthalpy of crystal fusion of a peak appearing on a high temperature side of a crystal fusion main peak of the porous hollow fiber membrane is 0.1 J/g or more.

### Claim 4 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein a temperature of the peak appearing on the high temperature side of the crystal fusion main peak of the porous hollow fiber membrane is at least 10° C. higher than a temperature of the crystal fusion main peak.

### Claim 5 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein a degree of crystallinity of the porous hollow fiber membrane is less than 60%.

### Claim 6 (depends on 2)

The porous hollow fiber membrane according to claim 2, wherein the enthalpy of crystal fusion at and below the crystallization onset temperature is 15% or less of the enthalpy of crystal fusion of the entire porous hollow fiber membrane.

### Claim 7 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein a weight average molecular weight (Mw) of the thermoplastic resin is 400 kDa or less.

### Claim 8 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein the thermoplastic resin comprises a polyvinylidene fluoride-based resin.

### Claim 9 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein the porous hollow membrane has an inner diameter of less than 0.75 mm and a compressive strength of 0.3 MPa or more.

### Claim 10 (depends on 1)

The porous hollow fiber membrane according to claim 1, wherein the porous hollow fiber membrane has a percent of reverse units of 9% or more.