# US 2025/0160222 A1 · Deuterium-treated resistive random-access memory (rram) devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0160222 A1
- Document ID: US20250160222A1
- Status: Published application
- Kind: A1
- Application number: 18/510,346
- Filed: 2023-11-15
- Published: 2025-05-15
- Earliest claimed: 2023-11-15
- Assignees: TetraMem Inc.
- Applicants: TetraMem Inc.
- Inventors: Minxian Zhang; Mingche Wu; Ning Ge
- Web page: https://patentgrep.com/patent/US20250160222A1

## CPC

- H10N 70/041: {Modification of switching materials after formation, e.g. doping (shaping H10N70/061)}
- H10B 63/00: Resistance change memory devices, e.g. resistive RAM [ReRAM] devices
- H10B 63/30: {comprising selection components having three or more electrodes, e.g. transistors}
- H10B 63/80: {Arrangements comprising multiple bistable or multi-stable switching components of the same type on a plane parallel to the substrate, e.g. cross-point arrays}
- H10N 70/023: {by chemical vapor deposition, e.g. MOCVD, ALD}
- H10N 70/026: {by physical vapor deposition, e.g. sputtering}
- H10N 70/20: Multistable switching devices, e.g. memristors
- H10N 70/24: {based on migration or redistribution of ionic species, e.g. anions, vacancies}
- H10N 70/826: {adapted for essentially vertical current flow, e.g. sandwich or pillar type devices}
- H10N 70/841: {Electrodes}
- H10N 70/8833: {Binary metal oxides, e.g. TaOx}
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The present disclosure provides resistive random-access memory (RRAM) devices and methods for making the same. An RRAM device may include a first electrode, a second electrode including a conductive material, and a switching oxide layer fabricated between the first electrode and the second electrode. The switching oxide layer is deuterium treated and contains deuterium. In some embodiments, the switching oxide layer includes a base oxide and a dopant oxide that is more chemically stable than the base oxide. The first electrode includes a non-reactive material that is not reactive to the base oxide or the dopant oxide. In some embodiments, the base oxide is Ta2O5, and the dopant oxide is Al2O3, SiO2, ZrO2, Sc2O3, or Y2O3. The RRAM device may further include an interface layer fabricated between the switching oxide layer and the second electrode. The interface layer is deuterium treated.

## Claims

### Claim 1

A resistive random-access memory (RRAM) device, comprising:
a first electrode;
a second electrode comprising a conductive material; and
a switching oxide layer fabricated between the first electrode and the second electrode, wherein the switching oxide layer comprises at least one transition metal oxide, and wherein the switching oxide layer comprises deuterium.

### Claim 2 (depends on 1)

The RRAM device of claim 1, wherein the switching oxide layer comprises a base oxide and a dopant oxide that is more chemically stable than the base oxide, wherein the first electrode comprises a non-reactive material that is not reactive to the base oxide or the dopant oxide.

### Claim 3 (depends on 2)

The RRAM device of claim 2, wherein the base oxide comprises HfOx or TaOy, wherein x≤2.0, wherein y≤2.5, and wherein the dopant oxide comprises at least one of Al2O3, SiO2, ZrO2, Sc2O3, or Y2O3.

### Claim 4 (depends on 3)

The RRAM device of claim 3, wherein the first electrode comprises at least one of titanium nitride, tantalum nitride, platinum, palladium, iridium, or ruthenium.

### Claim 5 (depends on 4)

The RRAM device of claim 4, wherein the second electrode further comprises a layer of titanium and a layer of tantalum.

### Claim 6 (depends on 1)

The RRAM device of claim 1, further comprising an interface layer positioned between the switching oxide layer and the second electrode, wherein the interface layer is deuterium-treated.

### Claim 7 (depends on 6)

The RRAM device of claim 6, wherein the interface layer positioned between the switching oxide layer and the second electrode comprises a discontinuous film of a dielectric material, wherein at least a portion of the second electrode is deposited on the switching oxide layer.

### Claim 8 (depends on 6)

The RRAM device of claim 6, wherein the second electrode is fabricated on the deuterium-treated interface layer.

### Claim 9

A method for fabricating an RRAM device, comprising:
fabricating, on a first electrode, a switching oxide layer;
performing deuterium treatment on the switching oxide layer; and
fabricating a second electrode on the deuterium-treated switching oxide layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein the switching oxide layer comprises a base oxide and a dopant oxide, wherein the dopant oxide is more chemically stable than the base oxide.

### Claim 11 (depends on 10)

The method of claim 10, wherein the base oxide comprises TaOy or HfOx, wherein x≤2.0, wherein y≤2.5, wherein the dopant oxide comprises at least one of Al2O3, SiO2, ZrO2, Sc2O3, or Y2O3.

### Claim 12 (depends on 11)

The method of claim 11, wherein fabricating the switching oxide layer comprises performing physical vapor deposition (PVD) using a single target comprising the base oxide and the dopant oxide and a single power source.

### Claim 13 (depends on 11)

The method of claim 11, wherein fabricating the switching oxide layer comprises performing a physical vapor deposition (PVD) co-sputtering process.

### Claim 14 (depends on 11)

The method of claim 11, wherein fabricating the switching oxide layer comprises depositing the base oxide and the dopant oxide using an atomic layer deposition (ALD) process.

### Claim 15 (depends on 10)

The method of claim 10, further comprising fabricating an interface layer on the switching oxide layer and performing deuterium treatment on the interface layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein the second electrode is fabricated on the deuterium-treated interface layer.

### Claim 17 (depends on 16)

The method of claim 16, wherein the interface layer comprises a discontinuous film of a dielectric material, wherein at least a portion of the second electrode is deposited on the switching oxide layer comprising the base oxide and the dopant oxide.

### Claim 18 (depends on 17)

The method of claim 17, wherein the dielectric material comprises at least one of Al2O3, SiO2, ZrO2, Sc2O3, or Y2O3.

### Claim 19 (depends on 9)

The method of claim 9, further comprising:
fabricating a first interface layer comprising a first dielectric material on the first electrode, wherein the switching oxide layer is fabricated on the first interface layer;
fabricating a second interface layer comprising a second dielectric material on the switching oxide layer;
performing deuterium treatment on the second interface layer; and
fabricating the second electrode on the deuterium-treated second interface layer.

### Claim 20 (depends on 9)

The method of claim 9, further comprising fabricating an interface layer on the first electrode, wherein the interface layer comprises a discontinuous film of a dielectric material, and wherein the switching oxide layer is fabricated on the interface layer.