# US 2025/0160035 A1 · Manufacturing method of cigs light absorption layer for solar cell using chemical vapor deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0160035 A1
- Document ID: US20250160035A1
- Status: Published application
- Kind: A1
- Application number: 18/558,735
- Filed: 2022-04-28
- Published: 2025-05-15
- Earliest claimed: 2021-05-11
- Assignees: Mecaroenergy Co., Ltd.
- Applicants: Mecaroenergy Co., Ltd.
- Inventors: Hea Yong KWON; Hyuk Kyoo JANG; Gyu Hyun LEE; Tae Yeop JEON; Seung Hyun LEE; Tae Woo EOM
- Web page: https://patentgrep.com/patent/US20250160035A1

## CPC

- H10F 71/128: {Annealing}
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- C23C 16/18: from metallo-organic compounds
- C23C 16/30: Deposition of compounds, mixtures or solid solutions, e.g. borides, carbides, nitrides
- C23C 16/305: {Sulfides, selenides, or tellurides}
- C23C 16/56: After-treatment
- H10F 10/167: comprising Group I-III-VI materials, e.g. CdS/CuInSe2 [CIS] heterojunction photovoltaic cells
- H10F 77/12: Active materials
- H10F 77/126: {comprising only Group I-III-VI chalcopyrite materials, e.g. CuInSe2, CuGaSe2 or CuInGaSe2 [CIGS]}
- H10P 14/203: {using transformation of metal, e.g. oxidation or nitridation}
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3241: {being conductive materials}
- Y02E 10/541: CuInSe2 material PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition consists of: forming a lower electrode on an upper surface of a substrate; forming a copper thin film with a copper precursor on an upper surface of a lower electrode formed through the lower electrode forming step; forming an indium thin film with an indium precursor on an upper surface of a copper thin film layer formed through the copper thin film forming step; forming a gallium thin film with a gallium precursor on an upper surface of an indium thin film layer formed through the indium thin film forming step; and heat-treating in selenium atmosphere a laminate on which a gallium thin film layer is formed through the gallium thin film forming step.

## Claims

### Claim 1

A manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition, consisting of: a lower electrode forming step of forming a lower electrode on an upper surface of a substrate; a copper thin film forming step of forming a copper thin film with a copper precursor on an upper surface of a lower electrode formed through the lower electrode forming step; an indium thin film forming step of forming an indium thin film with an indium precursor on an upper surface of a copper thin film layer formed through the copper thin film forming step; a gallium thin film forming step of forming a gallium thin film with a gallium precursor on an upper surface of an indium thin film layer formed through the indium thin film forming step; and a heat treatment step of heat-treating in selenium atmosphere a laminate on which a gallium thin film layer is formed through the gallium thin film forming step.

### Claim 2

A manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition, consisting of: a lower electrode forming step of forming a lower electrode on an upper surface of a substrate; a copper thin film forming step of forming a copper thin film with a copper precursor on an upper surface of a lower electrode formed through the lower electrode forming step; a gallium thin film forming step of forming a gallium thin film with a gallium precursor on an upper surface of a copper thin film layer formed through the copper thin film forming step; an indium thin film forming step of forming an indium thin film with an indium precursor on an upper surface of a gallium thin film layer formed through the gallium thin film forming step; and a heat treatment step of heat-treating in selenium atmosphere a laminate on which an indium thin film layer is formed through the indium thin film forming step.

### Claim 3 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the copper precursor consists of one or more selected from the group consisting of bis(acetylacetonato)copper, bis(2,2,6,6-tetramethylheptanedionato)copper, bis(hexafluoroacetylacetonato)copper, (vinyl trimethylsilyl)(hexafluoroacetylacetonate)copper, (vinyl trimethylsilyl)(acetylacetonato)copper, (vinyl trimethylsilyl)(2,2,6,6-tetramethylheptandionato)copper, (vinyl triethylsilyl)(acetylacetonato)copper, (vinyl triethylsilyl)(2,2,6,6-tetramethylheptandionato)copper, and (vinyl triethylsilyl)(hexafluoroacetylacetonate)copper.

### Claim 4 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the indium precursor consists of one or more selected from the group consisting of trimethylindium, triethylindium, triisopropylindium, tributylindium, tri-tert-ibutylindium, trimethoxyindium, triethoxyindium, triisopropoxyindium, dimethyl isopropoxy indium, diethyl isopropoxy indium, dimethyl ethyl indium, diethyl methyl indium, dimethyl isopropyl indium, diethy isopropyl indium, and dimethyl tert-butyl indium.

### Claim 5 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the gallium precursor consists of one or more selected from the group consisting of trimethylgallium, triethylgallium, triisopropylgallium, tributylgallium, tri-tert-ibutylgallium, trimethoxygallium, triethoxygallium, triisopropoxygallium, dimethyl isopropoxy gallium, diethyl isopropoxy gallium, dimethyl ethyl gallium, diethyl methyl gallium, dimethyl isopropyl gallium, diethy isopropyl gallium, and dimethyl tert-butyl gallium.

### Claim 6 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the copper precursor, the indium precursor, and the gallium precursor are supplied under conditions where the temperature of a canister is −40 to 100° C. and the temperature of a supply line is room temperature to 200° C.

### Claim 7 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the copper thin film, the indium thin film, and the gallium thin film are formed in a state in which a substrate temperature is from 100 to 500° C.

### Claim 8 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the copper thin film, the indium thin film, and the gallium thin film are formed at a pressure of 5 mTorr to 500 Torr.

### Claim 9 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the selenium atmosphere is formed by vaporizing a selenium precursor or metal selenium.

### Claim 10 (depends on 9)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 9, wherein the selenium precursor consists of one or more selected from the group consisting of dimethyl selenide, diethyl selenide, diisopropyl selenide, di-tert-butyl selenide, dimethyl diselenide, diethyl diselenide, diisopropyl diselenide, di-tert-butyl diselenide, tert-butyl isopropyl selenide, and tert-butyl selenol.

### Claim 11 (depends on 9)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 9, wherein the vaporized selenium precursor or the vaporized metal selenium is supplied through a carrier gas consisting of one or more selected from the group consisting of argon, helium, and nitrogen.

### Claim 12 (depends on 1)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 1, wherein the heat treatment step is performed at a temperature of 300 to 650° C.

### Claim 13 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the copper precursor consists of one or more selected from the group consisting of bis(acetylacetonato)copper, bis(2,2,6,6-tetramethylheptanedionato)copper, bis(hexafluoroacetylacetonato)copper, (vinyl trimethylsilyl)(hexafluoroacetylacetonate)copper, (vinyl trimethylsilyl)(acetylacetonato)copper, (vinyl trimethylsilyl)(2,2,6,6-tetramethylheptandionato)copper, (vinyl triethylsilyl)(acetylacetonato)copper, (vinyl triethylsilyl)(2,2,6,6-tetramethylheptandionato)copper, and (vinyl triethylsilyl)(hexafluoroacetylacetonate)copper.

### Claim 14 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the indium precursor consists of one or more selected from the group consisting of trimethylindium, triethylindium, triisopropylindium, tributylindium, tri-tert-ibutylindium, trimethoxyindium, triethoxyindium, triisopropoxyindium, dimethyl isopropoxy indium, diethyl isopropoxy indium, dimethyl ethyl indium, diethyl methyl indium, dimethyl isopropyl indium, diethy isopropyl indium, and dimethyl tert-butyl indium.

### Claim 15 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the gallium precursor consists of one or more selected from the group consisting of trimethylgallium, triethylgallium, triisopropylgallium, tributylgallium, tri-tert-ibutylgallium, trimethoxygallium, triethoxygallium, triisopropoxygallium, dimethyl isopropoxy gallium, diethyl isopropoxy gallium, dimethyl ethyl gallium, diethyl methyl gallium, dimethyl isopropyl gallium, diethy isopropyl gallium, and dimethyl tert-butyl gallium.

### Claim 16 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the copper precursor, the indium precursor, and the gallium precursor are supplied under conditions where the temperature of a canister is −40 to 100° C. and the temperature of a supply line is room temperature to 200° C.

### Claim 17 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the copper thin film, the indium thin film, and the gallium thin film are formed in a state in which a substrate temperature is from 100 to 500° C.

### Claim 18 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the copper thin film, the indium thin film, and the gallium thin film are formed at a pressure of 5 mTorr to 500 Torr.

### Claim 19 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the selenium atmosphere is formed by vaporizing a selenium precursor or metal selenium.

### Claim 20 (depends on 2)

The manufacturing method of a CIGS light absorption layer for solar cell using chemical vapor deposition according to claim 2, wherein the heat treatment step is performed at a temperature of 300 to 650° C.