# US 2025/0159852 A1 · Plasmonic/transition metal carbo-chalcogenides coating for a flexible, deep and multi-bands electromagnetic interference shielding application

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0159852 A1
- Document ID: US20250159852A1
- Status: Published application
- Kind: A1
- Application number: 18/938,963
- Filed: 2024-11-06
- Published: 2025-05-15
- Earliest claimed: 2023-11-10
- Assignees: Qatar Foundation for Education, Science and Community Development
- Applicants: Qatar Foundation for Education, Science and Community Development
- Inventors: Brahim Aïssa; Alessandro Sinopoli; Khaled Mahmoud
- Web page: https://patentgrep.com/patent/US20250159852A1

## CPC

- H05K 9/0088: {comprising a plurality of shielding layers; combining different shielding material structure}
- H05K: PRINTED CIRCUITS; CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS

## Abstract

A composite material for electromagnetic interference shielding is provided. The composite material comprises an electrically conductive microscale films based on Transition Metal Carbo-Chalcogenides (Nb2S2C) stack layers. The stack is effective to provide a substantial electromagnetic interference (EMI) shielding. Once decorated with special metallic nanoparticles made mainly with noble metals including Au, Ag and Pd, this efficiency against the EMI is even enhanced. The disclosed technology introduces a special coating that can be applied to electronic devices and materials. This coating acts as a shield that protects these devices from different types of interference that can disrupt their signals and performance. This coating can work on devices that bend or move, and effectively blocks interference across a wide range of frequencies. As such, the disclosed technology keeps devices working smoothly even in places with a lot of electronic “noise” without restricting their flexibility or range of use.

## Claims

### Claim 1

A composite material for electromagnetic interference shielding, the composite material comprising an electrically conductive microscale film including transition metal carbo-chalcogenides stack layers.

### Claim 2 (depends on 1)

The composite material for electromagnetic interference shielding from claim 1, wherein the composite material for electromagnetic interference shielding further includes a noble metal.

### Claim 3 (depends on 2)

The composite material for electromagnetic interference shielding from claim 2, wherein the noble metal is Au.

### Claim 4 (depends on 2)

The composite material for electromagnetic interference shielding from claim 2, wherein the noble metal is Ag.

### Claim 5 (depends on 2)

The composite material for electromagnetic interference shielding from claim 2, wherein the noble metal is Pb.

### Claim 6

A method of creating a composite material comprising an electrically conductive nanoscale film including transition metal carbo-chalcogenides stack layers, the method comprising:
dissolving a Transition Metal Carbo-Chalcogenides (TMCC) in deionized (DI) water to result in a solution;
stirring the solution;
applying probe sonification to the solution;
adding a material to the solution to result in a mixture;
stirring the mixture;
applying probe sonification to the mixture;
transferring the mixture to a container;
heating the mixture;
centrifugating the mixture;
washing the mixture; and
freeze drying the mixture.

### Claim 7 (depends on 6)

The method of claim 6, wherein 50 mg of TMCC are dissolved in 50 mL of DI water.

### Claim 8 (depends on 6)

The method of claim 6, wherein the solution is stirred for 5 minutes and the probe sonification is applied for 10 minutes.

### Claim 9 (depends on 6)

The method of claim 6, wherein the material is 19.7 mg of one of AgNO3, HAuCl4.3H2O, or Pd(acac) 2.

### Claim 10 (depends on 6)

The method of claim 6, wherein the mixture is stirred for 5 minutes and the probe sonification is applied for 10 minutes.

### Claim 11 (depends on 6)

The method of claim 6, wherein the container is a 100 mL Teflon container.

### Claim 12 (depends on 6)

The method of claim 6, wherein the mixture is heated to 160° C.

### Claim 13 (depends on 12)

The method of claim 12, wherein the mixture is heated with a gradual heat ramp-up of 2° C. per minute.

### Claim 14 (depends on 13)

The method of claim 13, wherein the mixture is heated over 12 hours.

### Claim 15 (depends on 6)

The method of claim 6, wherein the mixture is centrifugated at 2000 RCF.

### Claim 16 (depends on 6)

The method of claim 6, wherein the mixture is centrifugated for 5 minutes.

### Claim 17 (depends on 6)

The method of claim 6, wherein the mixture is freeze-dried for 48 hours.