# US 2025/0158222 A1 · Crosslinked polyolefin separators for batteries that cycle lithium ions and methods of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158222 A1
- Document ID: US20250158222A1
- Status: Published application
- Kind: A1
- Application number: 18/508,844
- Filed: 2023-11-14
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Nathaniel HARDIN; Fang Dai; Xingcheng Xiao; YIfan Zhao
- Web page: https://patentgrep.com/patent/US20250158222A1

## CPC

- H01M 50/417: Polyolefins
- C08J 3/28: Treatment by wave energy or particle radiation
- C08J 5/18: Manufacture of films or sheets
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/434: Ceramics
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/449: having a layered structure
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- C08J 2323/06: Polyethene
- C08J 2323/12: Polypropene
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A battery that cycles lithium ions includes a negative electrode, a positive electrode, and a separator sandwiched between opposed major facing surfaces of the negative and positive electrodes. The separator has an open microporous structure and includes a polyolefin having a crosslinked structure. When the separator is heated at a temperature of greater than or equal to about 145 degrees Celsius for about 1 hour, the separator has thermal shrinkage in directions parallel to the opposed major facing surfaces of the negative and positive electrodes of less than or equal to about 5%. The separator may be manufactured from a precursor film having an open microporous structure and comprising linear or branched chain polyolefin molecules. The precursor film may be exposed to a source of free radicals such that covalent bonds form between the polyolefin molecules and form a crosslinked polyolefin having a relatively high molecular weight.

## Claims

### Claim 1

A battery that cycles lithium ions, the battery comprising:
a negative electrode;
a positive electrode spaced apart from the negative electrode, the negative electrode and the positive electrode having opposed major facing surfaces; and
a separator having an open microporous structure and being sandwiched between the opposed major facing surfaces of the negative electrode and the positive electrode, the separator comprising a polyolefin having a crosslinked structure and, when the separator is heated at a temperature of greater than or equal to about 145 degrees Celsius for about 1 hour, the separator has thermal shrinkage in directions parallel to the opposed major facing surfaces of the negative electrode and the positive electrode of less than or equal to about 5%.

### Claim 2 (depends on 1)

The battery of claim 1, wherein, when the separator is heated at a temperature of greater than or equal to about 200 degrees Celsius for about 1 hour, the separator has thermal shrinkage in a direction parallel to the opposed major facing surfaces of the negative electrode and the positive electrode of less than or equal to about 10%.

### Claim 3 (depends on 1)

The battery of claim 1, wherein the polyolefin comprises polyethylene, polypropylene, or a combination thereof.

### Claim 4 (depends on 1)

The battery of claim 1, wherein the polyolefin has a crosslinking degree of greater than or equal to about 10% and less than or equal to about 80%.

### Claim 5 (depends on 1)

The battery of claim 1, wherein the polyolefin has a crosslinking degree of greater than or equal to about 60% and less than or equal to about 70%.

### Claim 6 (depends on 1)

The battery of claim 1, wherein the separator further comprises a ceramic material.

### Claim 7 (depends on 1)

The battery of claim 1, wherein the separator has a thickness of greater than or equal to about 5 micrometers and less than or equal to about 500 micrometers.

### Claim 8 (depends on 1)

The battery of claim 1, further comprising:
a non-aqueous polar aprotic organic solvent infiltrating the open microporous structure of the separator.

### Claim 9

A method of manufacturing a battery that cycles lithium ions, the method comprising:
exposing a precursor film having an open microporous structure and comprising linear or branched chain polyolefin molecules to a source of free radicals such that covalent bonds form between the polyolefin molecules and form a separator comprising a crosslinked polyolefin having a relatively high molecular weight, as compared to that of the linear or branched chain polyolefin molecules in the precursor film;
sandwiching the separator between opposed major facing surfaces of a negative electrode and a positive electrode; and
infiltrating the separator with an electrolyte.

### Claim 10 (depends on 9)

The method of claim 9, wherein the precursor film comprises polyethylene, polypropylene, or a combination thereof.

### Claim 11 (depends on 9)

The method of claim 9, wherein exposing the precursor film to the source of free radicals comprises irradiating the precursor film with an electron beam, plasma, ionizing radiation, non-ionizing radiation, or a combination thereof.

### Claim 12 (depends on 9)

The method of claim 9, wherein exposing the precursor film to the source of free radicals comprises irradiating the precursor film with an electron beam or gamma radiation, and wherein the precursor film is exposed to the source of free radicals in the presence of water.

### Claim 13 (depends on 9)

The method of claim 9, wherein exposing the precursor film to the source of free radicals comprises applying a chemical crosslinking agent to the precursor film.

### Claim 14 (depends on 13)

The method of claim 13, wherein the chemical crosslinking agent comprises a peroxide, benzophenone, or a combination thereof.

### Claim 15 (depends on 13)

The method of claim 13, wherein exposing the precursor film to the source of free radicals further comprises irradiating the precursor film with non-ionizing radiation.

### Claim 16 (depends on 9)

The method of claim 9, wherein the precursor film is exposed to the source of free radicals in an inert gas environment or in a subatmospheric pressure environment.

### Claim 17 (depends on 9)

The method of claim 9, wherein the crosslinked polyolefin has a crosslinking degree of greater than or equal to about 10% and less than or equal to about 80%.

### Claim 18 (depends on 9)

The method of claim 9, wherein the crosslinked polyolefin has a crosslinking degree of greater than or equal to about 60% and less than or equal to about 70%.

### Claim 19 (depends on 9)

The method of claim 9, wherein the precursor film further comprises a ceramic material.

### Claim 20 (depends on 9)

The method of claim 9, wherein the precursor film has a thickness of greater than or equal to about 5 micrometers and less than or equal to about 500 micrometers.