# US 2025/0158220 A1 · Method for Manufacturing Separator, Separator Obtained Therefrom and Electrochemical Device Including the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158220 A1
- Document ID: US20250158220A1
- Status: Published application
- Kind: A1
- Application number: 18/837,996
- Filed: 2023-02-14
- Published: 2025-05-15
- Earliest claimed: 2022-02-14
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Joo-Sung Lee; Sun-Mi Jin
- Web page: https://patentgrep.com/patent/US20250158220A1

## CPC

- H01M 10/052: Li-accumulators
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/431: Inorganic material
- H01M 50/434: Ceramics
- H01M 50/443: Particulate material
- H01M 50/446: Composite material consisting of a mixture of organic and inorganic materials
- H01M 50/451: comprising layers of only organic material and layers containing inorganic material
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for manufacturing a separator disperses inorganic particles homogeneously in a slurry. The separator obtained by this method causes low aggregation of the inorganic particles to show reduced defects of surface protrusions in its appearance and can provide excellent physical properties. This method for manufacturing a separator includes preparing a slurry containing inorganic particles, a binder polymer and a solvent. The method additionally includes; carrying out dispersion of the inorganic particles in the slurry, and the dispersion is carried out by using two types of dispersion instruments of a contact type dispersion instrument and a non-contact type dispersion instrument. The contact type dispersion instrument includes beads having an average particle diameter at least 200 times larger than the average particle diameter (D50) of the inorganic particles. The method additionally includes applying the slurry to at least one surface of a polymer porous support, followed by drying.

## Claims

### Claim 1

A method for manufacturing a separator, comprising the steps of:
preparing a slurry containing inorganic particles, a binder polymer, and a solvent;
carrying out dispersion of the inorganic particles in the slurry, wherein the dispersion is carried out by using two types of dispersion instruments of a contact type dispersion instrument and a non-contact type dispersion instrument, and the contact type dispersion instrument includes beads having an average particle diameter at least 200 times larger than the average particle diameter (D50) of the inorganic particles;
applying the slurry to at least one surface of a polymer porous support; and drying the slurry.

### Claim 2 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the contact type dispersion instrument comprises beads having an average particle diameter 2000-4000 times larger than the average particle diameter (D50) of the inorganic particles.

### Claim 3 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the dispersion is carried out in the contact type dispersion instrument first, and then is carried out in the non-contact type dispersion instrument.

### Claim 4 (depends on 3)

The method for manufacturing a separator according to claim 3, wherein the inorganic particles in the slurry has a particle size distribution (PSD) in which the ratio of the inorganic particles having a particle diameter at least 10 times larger than the average particle diameter (D50) of the inorganic particles is 5% or less, after carrying out the dispersion in the contact type dispersion instrument.

### Claim 5 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the contact type dispersion instrument includes a bead mill, a ball mill, a spike mill, a basket mill, an attrition mill, or a combined dispersion process of two or more of them.

### Claim 6 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the non-contact type dispersion instrument is a high-pressure homogenizer.

### Claim 7 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the dispersion using the non-contact type dispersion instrument is carried out under a pressure condition ranging from 5 to −200 MPa.

### Claim 8 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the beads have an average particle diameter (D50) of 0.5 mm or more.

### Claim 9 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the bead is a zirconia bead, an alumina bead, an yttria-stabilized zirconia (YSZ) bead, a titania bead, or two or more of them.

### Claim 10 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the inorganic particles have an average particle diameter of 0.01-1.0 μm.

### Claim 11 (depends on 1)

A separator obtained by the method as defined in claim 1.

### Claim 12 (depends on 11)

An electrochemical device comprising:
a positive electrode;
a negative electrode; and
the separator as defined in claim 11; interposed between the positive electrode and the negative electrode.

### Claim 13 (depends on 12)

The electrochemical device according to claim 12, wherein the electrochemical device is a lithium secondary battery.

### Claim 14 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the inorganic particles are Al2O3.

### Claim 15 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the binder polymer is at least one of polyvinylidene fluoride (PVDF) binder polymer or cyanoethylpullulan.

### Claim 16 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the binder polymer has a glass transition temperature (Tg) ranging from −200 to 200° C.

### Claim 17 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein a weight ratio of the inorganic particles to the binder polymer ranges from 50:50 to 99:1.

### Claim 18 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the polymer porous support includes a polyolefin polymer.

### Claim 19 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the applying the slurry to the at least one surface of the polymer porous support step includes slot coating the slurry.

### Claim 20 (depends on 1)

The method for manufacturing a separator according to claim 1, wherein the applying the slurry to the at least one surface of the polymer porous support step includes dip coating the slurry.