# US 2025/0158146 A1 · Method for recovering valuable metals from positive electrode of waste lithium iron phosphate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158146 A1
- Document ID: US20250158146A1
- Status: Published application
- Kind: A1
- Application number: 18/421,950
- Filed: 2024-01-24
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: Shenzhen Huineng Energy Storage Materials Engineering Research Center Co., LTD.; National Engineering Research Center of Advanced Energy Storage Materials (Shenzhen) Co., Ltd.
- Applicants: Shenzhen Huineng Energy Storage Materials Engineering Research Center Co., LTD.; National Engineering Research Center of Advanced Energy Storage Materials (Shenzhen) Co., Ltd.
- Inventors: Faping ZHONG; Chihuan HE; Subin JIANG; Hongbing LIU; Jiqun ZHU; Shuifa TAN
- Web page: https://patentgrep.com/patent/US20250158146A1

## CPC

- H01M 6/52: Reclaiming serviceable parts of waste cells or batteries {, e.g. recycling}
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- B01D 5/0003: {by using heat-exchange surfaces for indirect contact between gases or vapours and the cooling medium}
- B01D 5/0087: {Recirculating of the cooling medium}
- B01D 5/009: {Collecting, removing and/or treatment of the condensate}
- C01D 15/08: Carbonates; Bicarbonates
- C01F 7/56: Chlorides (containing fluorine C01F7/52)
- C01G 49/10: Halides {(C01G49/0018 takes precedence)}
- C21B 15/006: {By a chloride process}
- C22B 1/02: Roasting processes (C22B1/16 takes precedence)
- C22B 1/08: Chloridising roasting
- C22B 1/24: Binding; Briquetting {; Granulating}
- C22B 7/002: {by treating with halogens, sulfur or compounds thereof; by carburising, by treating with hydrogen (hydriding)}
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 7/006: {Wet processes}
- C22B 26/12: Obtaining lithium
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- B01D 53/002: {by condensation}
- C01P 2006/80: Compositional purity
- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Provided is a method for recovering valuable metals from a positive electrode of waste lithium iron phosphate. The method includes: subjecting a waste lithium iron phosphate battery to discharging and disassembly; subjecting a lithium iron phosphate positive plate obtained by the disassembly to breaking, followed by high temperature treatment; uniformly mixing a product obtained by the high temperature treatment with a carbon material, and roasting a mixture in a high-purity Cl2 atmosphere; subjecting a gas phase product obtained by the roasting to fractional quenching and condensation to recover ferric chloride and aluminum chloride separately; and subjecting a solid phase product obtained by the roasting to water leaching and filtration to obtain a lithium chloride aqueous solution, and then adding sodium carbonate to precipitate lithium carbonate. As a one-step carbothermal chlorination method is adopted in combination with a two-stage quenching and condensation process in the present invention, the use of acidic solutions during recovery of valuable metals from the lithium iron phosphate positive electrode can be avoided, and the use of large amounts of alkaline solutions or extraction agents to separate and recover chlorides step by step is also not required. The method of the present invention has the advantages of a high metal recovery rate, a low comprehensive cost and good economic benefits, social benefits and environmental protection benefits.

## Claims

### Claim 1

A method for recovering valuable metals from a positive electrode of waste lithium iron phosphate, sequentially comprising the following steps:
(1) subjecting a waste lithium iron phosphate battery to discharging and disassembly to obtain a lithium iron phosphate positive plate;
(2) subjecting the lithium iron phosphate positive plate to breaking, followed by high temperature treatment in an air atmosphere;
(3) uniformly mixing a product obtained by the high temperature treatment with a carbon material by ball milling, then transferring a mixture to a sintering device, introducing high-purity Cl2 after vacuumizing the sintering device, and heating and roasting the mixture in the Cl2 atmosphere;
(4) enabling a gas phase product produced in the roasting process to sequentially pass through a quenching and condensation separation device 1 and a quenching and condensation separation device 2; introducing SiCl4 that is preheated to 220-240° C. and flows backward with the gas phase product into a heat exchange tube of the quenching and condensation separation device 1, and recovering condensed FeCl3 in a deposition chamber of the quenching and condensation separation device 1; and introducing SiCl4 that is preheated to 100-120° C. and flows backward with the gas phase product into a heat exchange tube of the quenching and condensation separation device 2, and recovering condensed AlCl3 in a deposition chamber of the quenching and condensation separation device 2; and
(5) subjecting a solid phase product obtained by the roasting in step (3) to water leaching, stirring and filtration to obtain a LiCl aqueous solution, and then adding sodium carbonate into the LiCl aqueous solution to recover and precipitate Li2CO3.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in step (2), the lithium iron phosphate positive plate has an average particle size of equal to or less than 3 mm after the breaking.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in step (2), the high temperature treatment is performed at a heating rate of 5-10° C./min and a temperature of 400-600° C., and the temperature is maintained for 3-6 h.

### Claim 4 (depends on 1)

The method according to claim 1, wherein in step (3), the carbon material comprises at least one of graphite, carbon black, carbon fibers, carbon nanotubes and amorphous carbon.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in step (3), the mass ratio of the product obtained by the high temperature treatment to the carbon material is 10:1 to 5:1.

### Claim 6 (depends on 1)

The method according to claim 1, wherein in step (3), the high-purity Cl2 is introduced at a rate of 10-50 mL/min.

### Claim 7 (depends on 1)

The method according to claim 1, wherein in step (3), the roasting is performed in two stages; the roasting in the first stage is performed at a heating rate of 3-5° C./min and a temperature of 180-300° C., and the temperature is maintained for 1-3 h; and the roasting in the second stage is performed at a heating rate of 5-10° C./min and a temperature of 350-550° C., and the temperature is maintained for 3-6 h.

### Claim 8 (depends on 1)

The method according to claim 1, wherein in step (4), before introduced into the heat exchange tube of the quenching and condensation separation device 2, the SiCl4 is preheated to 100-120° C. first, and the SiCl4 is introduced into the heat exchange tube of the quenching and condensation separation device 2 at a flow rate of 5-10 mL/min.

### Claim 9 (depends on 1)

The method according to claim 1, wherein in step (4), before introduced into the heat exchange tube of the quenching and condensation separation device 1, the SiCl4 is preheated to 220-240° C. first, and the SiCl4 is introduced into the heat exchange tube of the quenching and condensation separation device 1 at a flow rate of 5-10 mL/min.

### Claim 10 (depends on 1)

The method according to claim 1, wherein in step (5), water used in the water leaching is deionized water; and the water leaching and the stirring are performed for 1-4 h.