# US 2025/0158138 A1 · High energy all-solid-state battery cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158138 A1
- Document ID: US20250158138A1
- Status: Published application
- Kind: A1
- Application number: 19/025,848
- Filed: 2025-01-16
- Published: 2025-05-15
- Earliest claimed: 2024-11-21
- Assignees: GM Global Technology Operations LLC
- Applicants: GM Global Technology Operations LLC
- Inventors: Qili SU; Meiyuan Wu; Zhe Li; Haijing Liu
- Web page: https://patentgrep.com/patent/US20250158138A1

## CPC

- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/623: {fluorinated polymers}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 50/431: Inorganic material
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An all-solid-state battery cell includes C cathode electrodes including a cathode active material layer arranged on at least one side of a cathode current collector, A anode electrodes including an anode active material layer and an anode current collector, and S separators comprising a sulfide membrane, where C, A, and S are integers greater than one. A lithium layer arranged between the anode current collector and the anode active material layer. The cathode active material, the anode active material, and the separator are densified prior to arranging the lithium layer and the anode current collector adjacent to the anode active material layer.

## Claims

### Claim 1

An all-solid-state battery cell comprising:
C cathode electrodes including a cathode active material layer arranged on at least one side of a cathode current collector;
A anode electrodes including an anode active material layer and an anode current collector;
S separators comprising a sulfide membrane, where C, A, and S are integers greater than one; and
a lithium layer arranged between the anode current collector and the anode active material layer, wherein the cathode active material, the anode active material, and the separator are densified prior to arranging the lithium layer and the anode current collector adjacent to the anode active material layer.

### Claim 2 (depends on 1)

The all-solid-state battery cell of claim 1, wherein:
the lithium layer has a thickness in a range from 2 μm to 20 μm, and
the lithium layer comprises one of a continuous planar layer, a mesh layer, and a striped layer.

### Claim 3 (depends on 1)

The all-solid-state battery cell of claim 1, wherein the anode active material layer includes silicon particles in a range from 70 to 90 wt %, a sulfide electrolyte in a range from 10 to 30 wt %, and a binder in a range from 0.1 to 5 wt %.

### Claim 4 (depends on 3)

The all-solid-state battery cell of claim 3, wherein:
the sulfide electrolyte comprises Li6PS5Cl; and
the binder comprises polytetrafluoroethylene (PTFE).

### Claim 5 (depends on 1)

The all-solid-state battery cell of claim 1, wherein the cathode active material layer comprises cathode active material in a range from 68 to 90 wt %, a sulfide electrolyte in a range from 10 to 30 wt %, and a binder in a range from 0.1 to 3 wt %.

### Claim 6 (depends on 5)

The all-solid-state battery cell of claim 5, wherein:
the cathode active material comprises LiNixMnyCo1-x-yOz (where 0.95>x≥0.6; y≥0.05);
the sulfide electrolyte comprises Li6PS5Cl; and
the binder comprises polytetrafluoroethylene (PTFE).

### Claim 7 (depends on 6)

The all-solid-state battery cell of claim 6, wherein the cathode active material is coated with LiNbO3.

### Claim 8 (depends on 1)

The all-solid-state battery cell of claim 1, wherein the sulfide membrane includes sulfide electrolyte, a binder, a lithium salt, and a filler.

### Claim 9 (depends on 8)

The all-solid-state battery cell of claim 8, wherein the sulfide membrane includes the sulfide electrolyte in a range from 85 to 99 wt %, the binder in a range from 1 to 10 wt %, the lithium salt in a range from 0 to 5 wt %, and the filler in a range from 0.1 to 1 wt %.

### Claim 10 (depends on 9)

The all-solid-state battery cell of claim 9, wherein:
the sulfide electrolyte comprises Li6PS5Cl; and
the binder comprises poly (ethylene oxide) (PEO).

### Claim 11

A method for fabricating an all-solid-state battery cell, comprising:
supplying a first free-standing film including a cathode active material layer;
supplying a second free-standing film including an anode active material layer;
supplying a third free-standing film comprising a sulfide membrane;
densifying the first free-standing film, the second free-standing film, and the third free-standing film;
arranging a lithium layer and an anode current collector adjacent to the anode active material layer; and
arranging a cathode current collector adjacent to the cathode active material layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein:
the lithium layer has a thickness in a range from 2 μm to 20 μm, and
the lithium layer comprises one of a continuous planar layer, a mesh layer, and a striped layer.

### Claim 13 (depends on 11)

The method of claim 11, wherein the anode active material layer includes silicon particles in a range from 70 to 90 wt %, a sulfide electrolyte in a range from 10 to 30 wt %, and a binder in a range from 0.1 to 5 wt %.

### Claim 14 (depends on 13)

The method of claim 13, wherein:
the sulfide electrolyte comprises Li6PS5Cl; and
the binder comprises polytetrafluoroethylene (PTFE).

### Claim 15 (depends on 11)

The method of claim 11, wherein the cathode active material layer comprises cathode active material in a range from 68 to 90 wt %, a sulfide electrolyte in a range from 10 to 30 wt %, and a binder in a range from 0.1 to 3 wt %.

### Claim 16 (depends on 15)

The method of claim 15, wherein:
the cathode active material comprises LiNixMnyCo1-x-yOz (where 0.95>x≥0.6; y≥0.05);
the sulfide electrolyte comprises Li6PS5Cl; and
the binder comprises polytetrafluoroethylene (PTFE).

### Claim 17 (depends on 16)

The method of claim 16, wherein the cathode active material is coated with LiNbO3.

### Claim 18 (depends on 11)

The method of claim 11, wherein the sulfide membrane includes sulfide electrolyte in a range from 85 to 99 wt %, a binder in a range from 1 to 10 wt %, lithium salt in a range from 0 to 5 wt %, and filler in a range from 0.1 to 1 wt %.

### Claim 19 (depends on 18)

The all-solid-state battery cell of claim 18, wherein:
the sulfide electrolyte comprises Li6PS5Cl; and
the binder comprises poly (ethylene oxide) (PEO).

### Claim 20

An all-solid-state battery cell for a vehicle, comprising:
C cathode electrodes comprising including a cathode active material layer arranged on at least one side of a cathode current collector,
wherein the cathode active material layer comprises cathode active material including LiNixMnyCo1-x-yO2 (where 0.95>x>0.6; y>0.05) in a range from 68 to 90 wt %, sulfide electrolyte comprising Li6PS5Cl in a range from 10 to 30 wt %, and a binder comprising polytetrafluoroethylene in a range from 0.1 to 3 wt %;
A anode electrodes including an anode active material layer and an anode current collector,
wherein the anode active material layer includes silicon particles in a range from 70 to 90 wt %, sulfide electrolyte including Li6PS5Cl in a range from 10 to 30 wt %, and a binder comprising polytetrafluoroethylene in a range from 0.1 to 5 wt %;
S separators comprising a sulfide membrane, where C, A, and S are integers greater than one,
wherein the sulfide membrane includes sulfide electrolyte including Li6PS5Cl, a binder including poly (ethylene oxide) (PEO), a lithium salt, and a filler; and
a lithium layer arranged between the anode current collector and the anode active material layer.