# US 2025/0158116 A1 · Polymer solid electrolyte and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158116 A1
- Document ID: US20250158116A1
- Status: Published application
- Kind: A1
- Application number: 18/832,503
- Filed: 2023-05-31
- Published: 2025-05-15
- Earliest claimed: 2022-05-31
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Sunghyun NAM; Jung Pil LEE; Hyeaeun HAN; Dong Kyu KIM
- Web page: https://patentgrep.com/patent/US20250158116A1

## CPC

- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- C08J 5/22: Films, membranes or diaphragms
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0564: the electrolyte being constituted of organic materials only
- H01M 2300/0082: Organic polymers
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A polymer solid electrolyte and a manufacturing method therefor are provided. The polymer solid electrolyte comprises a cross-linked structure formed by a cross-linkable functional group, the cross-linked structure including (a) a cross-linking between the cross-linkable functional groups, (b) a cross-linking between the cross-linkable functional group and a solvent, and (c) a bonding between the cross-linkable functional group and a lithium salt, and thereby having a reduced crystallinity and improving ion conductivity even without using a separate plasticizer.

## Claims

### Claim 1

A polymer solid electrolyte comprising a polymer containing a cross-linkable functional group; a lithium salt; and a solvent,
wherein the polymer solid electrolyte comprises a cross-linked structure; and an amorphous polymer chain containing the cross-linkable functional group, and
wherein the cross-linked structure comprises (a) a crosslinking between the cross-linkable functional groups, (b) a crosslinking between the cross-linkable functional group and the solvent, and (c) a bonding between the cross-linkable functional group and the lithium salt.

### Claim 2 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein
(a) the crosslinking between the cross-linkable functional groups comprises a hydrogen bond,
(b) the crosslinking between the cross-linkable functional group and the solvent comprises a hydrogen bond, and
(c) the bonding between the cross-linkable functional group and the lithium salt comprises a bond by Lewis acid-base interaction.

### Claim 3 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the cross-linkable functional group comprises one or more selected from the group consisting of a hydroxyl group, a carboxyl group, and an amide group.

### Claim 4 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the polymer containing the cross-linkable functional groups comprises one or more selected from the group consisting of polyvinyl alcohol(PVA), gelatin, methylcellulose, agar, dextran, poly(vinyl pyrrolidone), poly(ethylene oxide), poly(acryl amide), starch-carboxymethyl cellulose, hyaluronic acid-methylcellulose, chitosan, poly(N-isopropylacrylamide), and amino-terminated polyethylene glycol (amino-terminated PEG).

### Claim 5 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein a weight average molecular weight (Mw) of the polymer containing the cross-linkable functional groups is 80,000 g/mol to 130,000 g/mol.

### Claim 6 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the polymer containing the cross-linkable functional groups comprises polyvinyl alcohol(PVA).

### Claim 7 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the lithium salt comprises one or more selected from the group consisting of (CF3SO2)2NLi (lithium bis(trifluoromethanesulfonyl)imide, LiTFSI), (FSO2)2NLi (lithium bis(fluorosulfonyl)imide, LiFSI), LiNO3, LiOH, LiCl, LiBr, LiI, LiClO4, LiBF4, LiB10Cl10, LiPF6, LiCF3SO3, LiCF3CO2, LiAsF6, LiSbF6, LiAlCl4, CH3SO3Li, CF3SO3Li, LiSCN, and LiC(CF3SO2)3.

### Claim 8 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the molar ratio of lithium ([Li]) of the lithium salt to the cross-linkable functional group ([G]) of the polymer, [Li]/[G], is more than 0.1 and less than 0.5.

### Claim 9 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the solvent comprises water.

### Claim 10 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the polymer solid electrolyte is in the form of a free-standing film or a coating layer.

### Claim 11 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein an ionic conductivity of the polymer solid electrolyte is 10−4 S/cm or more.

### Claim 12 (depends on 1)

The polymer solid electrolyte according to claim 1, wherein the polymer solid electrolyte further comprises a liquid electrolyte.

### Claim 13

A method for preparing a polymer solid electrolyte, the method comprising:
(S1) forming a solution by adding a lithium salt to a polymer solution including a polymer containing a cross-linkable functional group and a solvent;
(S2) forming a coating film by applying the solution on a substrate; and
(S3) forming a polymer solid electrolyte by freezing and thawing the coating film.

### Claim 14 (depends on 13)

The method for preparing the polymer solid electrolyte according to claim 13, wherein the polymer solid electrolyte comprises a cross-linked structure,
wherein the cross-linking structure comprises (a) a cross-linking between the cross-linkable functional groups, (b) a cross-linking between the cross-linkable functional group and the solvent, and (c) a bonding between the cross-linkable functional group and the lithium salt,
wherein (a) the crosslinking between the cross-linkable functional groups comprises a hydrogen bond,
(b) the crosslinking between the cross-linkable functional group and the solvent comprises a hydrogen bond, and
(c) the bonding between the cross-linkable functional group and the lithium salt comprises a bond by Lewis acid-base interaction.

### Claim 15 (depends on 13)

The method for preparing the polymer solid electrolyte according to claim 13, wherein the freezing is carried out at −30° C. to −10° C.

### Claim 16 (depends on 13)

The method for preparing the polymer solid electrolyte according to claim 13, wherein the thawing is carried out at 15° C. to 35° C.

### Claim 17 (depends on 1)

An all-solid battery comprising the polymer solid electrolyte of claim 1.