# US 2025/0158105 A1 · Lithium-ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158105 A1
- Document ID: US20250158105A1
- Status: Published application
- Kind: A1
- Application number: 18/765,558
- Filed: 2024-07-08
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Applicants: Toyota Jidosha Kabushiki Kaisha
- Inventors: Ryo ASAKURA; Shinya SHIOTANI; Sakina KANEKO
- Web page: https://patentgrep.com/patent/US20250158105A1

## CPC

- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/38: of elements or alloys
- H01M 4/387: {Tin or alloys based on tin}
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 2004/027: {Negative electrodes}
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium-ion secondary battery that utilizes metal lithium deposition-dissolution reactions includes a cathode layer, an anode layer and an electrolyte layer between the cathode layer and the anode layer, the cathode layer includes a cathode active material that is arranged to absorb and desorb lithium ions, the anode layer includes a silver (Ag) element, a tin (Sn) element, and a lithium (Li) element, and a molar ratio of the Sn element to the Ag element (Sn/Ag) contained in the anode layer is 0.09 or higher and 0.17 or lower.

## Claims

### Claim 1

A lithium-ion secondary battery that utilizes metal lithium deposition-dissolution reactions, the lithium-ion secondary battery comprising:
a cathode layer;
an anode layer; and
an electrolyte layer between the cathode layer and the anode layer, wherein:
the cathode layer includes a cathode active material that is arranged to absorb and desorb lithium ions;
the anode layer includes a silver element, a tin element, and a lithium element; and
a molar ratio of the tin element to the silver element contained in the anode layer is 0.09 or higher and 0.17 or lower.

### Claim 2 (depends on 1)

The lithium-ion secondary battery according to claim 1, wherein:
the lithium-ion secondary battery includes an anode current collector on an opposite side of the anode layer from the electrolyte layer; and
when the anode layer is equally divided into two parts parallel to a layer surface of the anode layer, and a region on a side of the anode current collector is defined as a first region and a region on a side of the electrolyte layer is defined as a second region, content of the tin element in the second region of the anode layer is greater than content of the tin element in the first region of the anode layer.

### Claim 3 (depends on 1)

The lithium-ion secondary battery according to claim 1, wherein, when the lithium-ion secondary battery is fully charged, a composition ratio of lithium in a lithium-silver alloy produced in the anode layer is 94 mol % or more and 97 mol % or less.

### Claim 4 (depends on 3)

The lithium-ion secondary battery according to claim 3, wherein the electrolyte layer is a solid electrolyte layer containing a sulfide-based solid electrolyte.

### Claim 5

A lithium-ion secondary battery that utilizes metal lithium deposition-dissolution reactions, the lithium-ion secondary battery comprising:
a cathode layer;
an anode layer; and
an electrolyte layer between the cathode layer and the anode layer, wherein:
the cathode layer includes a cathode active material that is arranged to absorb and desorb lithium ions;
the anode layer includes a metal tin layer containing elemental tin, and a metal silver layer containing elemental silver in order from a side of the electrolyte layer; and
a molar ratio of a tin element to a silver element contained in the anode layer is 0.09 or higher and 0.17 or lower.