# US 2025/0158097 A1 · Concentrated vrfb electrolyte composition and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158097 A1
- Document ID: US20250158097A1
- Status: Published application
- Kind: A1
- Application number: 18/840,837
- Filed: 2023-02-23
- Published: 2025-05-15
- Earliest claimed: 2022-02-23
- Assignees: Largo Clean Energy Corp.
- Applicants: Largo Clean Energy Corp.
- Inventors: Michael L. PERRY
- Web page: https://patentgrep.com/patent/US20250158097A1

## CPC

- C01G 31/00: Compounds of vanadium
- H01M 8/08: Fuel cells with aqueous electrolytes
- B01D 61/58: Multistep processes
- H01M 8/188: {by recharging of redox couples containing fluids; Redox flow type batteries}
- B01D 61/002: {Forward osmosis or direct osmosis}
- B01D 61/025: {Reverse osmosis; Hyperfiltration}
- B01D 2311/04: Specific process operations in the feed stream; Feed pretreatment
- B01D 2311/263: Chemical reaction
- B01D 2311/2642: Aggregation, sedimentation, flocculation, precipitation or coagulation
- H01M 2300/0011: Sulfuric acid-based
- Y02E 60/50: Fuel cells
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

There is disclosed a method for producing a concentrated VRFB electrolyte composition. The method comprises the following steps: (a) mixing a vanadium, oxide, water and aqueous H2SO4 in sufficient quantities to produce a reaction mixture comprising a vanadium sulfate at a concentration at least 3.0 M and a total sulfate concentration of at least 2 times the concentration of the vanadium sulfate; (b) maintaining the reaction mixture at an initial temperature that substantially avoids precipition of reaction solids; (c) allowing the reaction mixture to reach ambient temperature: and (d) increasing the viscosity of the reaction mixture to produce the concentrated VRFB electrolyte composition. There is also disclosed a concentrated VRFB electrolyte composition. The concentrated VRFB electrolyte is believed to provide advantages include reduced shipping costs, logistics and on-site capital costs at the facility using the VRFBs.

## Claims

### Claim 1

A method for producing a concentrated VRFB electrolyte composition comprising the steps of:
(a) mixing a vanadium oxide, water and aqueous H2SO4 in sufficient quantities to produce a reaction mixture comprising a vanadium sulfate at a concentration at least 3.0 M and a total sulfate concentration of at least 2 times the concentration of the vanadium sulfate;
(b) maintaining the reaction mixture at an initial temperature that substantially avoids precipitation of reaction solids;
(c) allowing the reaction mixture to reach ambient temperature; and
(d) increasing the viscosity of the reaction mixture to produce the concentrated VRFB electrolyte composition.

### Claim 2 (depends on 1)

The method defined in claim 1, wherein the vanadium oxide comprises one or both of V2O5 and V2O3.

### Claim 3 (depends on 1)

The method defined in claim 1, wherein Step (a) comprises mixing a vanadium oxide, water and aqueous H2SO4 in sufficient quantities to produce a reaction mixture comprising a vanadium sulfate at a concentration in the range of from about 3.0 M to about 5.0 M and a total sulfate concentration of at least two times the concentration of the vanadium sulfate.

### Claim 4 (depends on 1)

The method defined in claim 1, wherein, in Step (a), the concentration of total sulfate is from 2 to 4 times the concentration of the vanadium sulfate.

### Claim 5 (depends on 1)

The method defined in claim 1, wherein the initial temperature in Step (b) is at least about 50° C.

### Claim 6 (depends on 1)

The method defined in claim 1, wherein the ambient temperature in Step (c) is in the range of from about 15° C. to about 40° C.

### Claim 7 (depends on 1)

The method defined in claim 1, wherein, prior to Step (c), the reaction mixture is dispensed into a storage container, and the reaction mixture is dispensed into a shipping container.

### Claim 8 (depends on 1)

The method defined in claim 1, wherein the concentrated VRFB electrolyte composition is in the form of a gel product.

### Claim 9 (depends on 1)

The method defined in claim 1, wherein prior to Step (c), the reaction mixture is subjected to a sub-process to produce a purified reaction mixture which is subjected to Step (d), wherein the purification sub-process comprises the following steps:
(i) providing the reaction mixture from Step (b) which comprises a precipitation valence and contains at least one impurity that precipitates out of the reaction mixture when the valence of the reaction mixture is at or below the precipitation valence;
(ii) reducing the reaction mixture to a valence below the precipitation valence so as to cause the at least one impurity to precipitate out of the reaction mixture as a precipitate; and
(iii) mechanically separating the precipitate reaction mixture to produce the purified reaction mixture.

### Claim 10 (depends on 9)

The method defined in claim 9, wherein, prior to Step (ii), the reaction mixture is subjected to a dilution step to produce a diluted reaction mixture, wherein the dilution step results in the diluted reaction mixture comprising vanadium sulfate at a concentration less than 3.0 M and a total sulfate concentration of at least 2 times the concentration of the vanadium sulfate.

### Claim 11 (depends on 10)

The method defined in claim 10, wherein the dilution step results in the diluted reaction mixture having a total sulfate concentration that is from 2 to 4 times the concentration of the vanadium sulfate.

### Claim 12 (depends on 11)

The method defined in claim 11, wherein the diluted reaction mixture is subjected to Steps (ii) and (iii) to produce a diluted, purified reaction mixture; the diluted, purified reaction mixture is subjected to a concentration step to produce the purified reaction mixture and the purified reaction mixture has a concentration of vanadium sulfate of at least 3.0 M and a total sulfate concentration of at least two times the concentration of the vanadium sulfate.

### Claim 13 (depends on 12)

The method defined in claim 12, wherein the concentration step is conducted using reverse osmosis to produce an extracted aqueous liquid from the diluted, purified reaction mixture, wherein the extracted aqueous liquid is used in the dilution step to produce the diluted, reaction mixture, and wherein the extracted aqueous liquid is used as the only diluent in the dilution step to produce the diluted, reaction mixture.

### Claim 14 (depends on 12)

The method defined in claim 12, wherein the dilution step and the concentration step are conducted in an osmosis module and wherein the osmosis module is configured to pass an aqueous liquid from the diluted, purified reaction mixture through a reverse osmosis membrane into the reaction mixture prior to Step (ii) to produce: (1) the diluted reaction mixture on the other side of the reverse osmosis membrane and (2) the purified reaction mixture on the opposite side of the reverse osmosis membrane, and wherein the osmosis module is configured to use a pressure gradient to modulate the rate of transfer of aqueous liquid through the reverse osmosis membrane.

### Claim 15 (depends on 1)

The method defined in claim 1, wherein Step (d) comprises contacting the reaction mixture with a nucleation center, and wherein the nucleation center comprises a solid, a liquid or a mixture of liquid and a solid.

### Claim 16 (depends on 15)

The method defined in claim 15, wherein the nucleation center is selected from the group consisting of a porous particulate material, a microporous particulate material, a carbon felt, a carbon powder, a zeolite, a VOSO4 salt, vanadium salt, a high crystallinity vanadium salt or a low-crystallinity vanadium salt and any mixture of two or more of these.

### Claim 17 (depends on 15)

The method defined in claim 15, wherein the nucleation center is used in an amount of at least about 0.1 mg/mL.

### Claim 18 (depends on 1)

The method defined in claim 1, wherein Step (d) is conducted with mixing of the reaction mixture and wherein mixing during Step (d) is done for a period of at least about 15 minutes.

### Claim 19 (depends on 1)

The method defined in claim 1, wherein: (i) the concentrated VRFB electrolyte composition produced in Step (d) has a densification level (DL) which is at least 30% and (ii) the densification level is calculated as follows: DL=(Volumeremoved water/Volumetotal electrolyte)×100%.

### Claim 20 (depends on 1)

The concentrated VRFB electrolyte composition produced according to the method defined in claim 1.

### Claim 21 (depends on 20)

A method for producing a VRFB electrolyte composition comprising the step of contacting the concentrated VRFB electrolyte composition defined in claim 20 with an aqueous liquid.

### Claim 22 (depends on 21)

The method defined in claim 21, wherein the aqueous liquid is added in an amount to produce the VRFB electrolyte composition comprising vanadium sulfate at a concentration less than 3.0 M and a total sulfate concentration of at least 2 times the concentration of the vanadium sulfate.

### Claim 23

A composition, the composition comprising vanadium sulfate at a concentration at least 3.0 M and a total sulfate concentration of at least 2 times the concentration of the vanadium sulfate, wherein the composition is in the form a gel or a semi-solid and/or has a viscosity of at least 100 mPa.s at 20° C.

### Claim 24 (depends on 23)

The composition defined in claim 23, wherein the purified reaction mixture has a concentration of vanadium sulfate of at least 3.0 M and a total sulfate concentration of at least two times the concentration of the vanadium sulfate.

### Claim 25

(canceled)

### Claim 26