# US 2025/0158067 A1 · Secondary battery and method for manufacturing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158067 A1
- Document ID: US20250158067A1
- Status: Published application
- Kind: A1
- Application number: 18/832,293
- Filed: 2023-10-18
- Published: 2025-05-15
- Earliest claimed: 2022-10-18
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: In Hyouk SUNG; Dong Wook SUNG; Kyung Ryun KA; Min Ji KIM; Ji Su LEE
- Web page: https://patentgrep.com/patent/US20250158067A1

## CPC

- H01M 4/622: {being polymers}
- H01M 50/489: Separators, membranes, diaphragms or spacing elements inside the cells, characterised by their physical properties, e.g. swelling degree, hydrophilicity or shut down properties
- H01M 4/0402: {Methods of deposition of the material}
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 10/049: {Processes for forming or storing electrodes in the battery container}
- H01M 10/058: Construction or manufacture
- H01M 50/403: Manufacturing processes of separators, membranes or diaphragms
- H01M 50/414: Synthetic resins, e.g. thermoplastics or thermosetting resins
- H01M 50/449: having a layered structure
- H01M 50/461: {with adhesive layers between electrodes and separators}
- H01M 50/609: Arrangements or processes for filling with liquid, e.g. electrolytes
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed is a secondary battery that can increase the adhesive force between the anode and the separator on an electrolyte. The secondary battery includes an anode, a cathode, a separator which is between the anode and the cathode and includes a porous substrate and a coating layer on at least one surface of the porous substrate, and an electrolyte, The anode contains a binder polymer including a first repeating unit, the coating layer includes a second repeating unit, and the first repeating unit and the second repeating unit are bonded to each other.

## Claims

### Claim 1

A secondary battery comprising:
an anode;
a cathode;
a separator between the anode and the cathode and comprising a porous substrate and a coating layer on at least one surface of the porous substrate;
and an electrolyte,
wherein the anode comprises a binder polymer comprising a first repeating unit, the coating layer comprises a second repeating unit, and the first repeating unit and the second repeating unit are bonded to each other.

### Claim 2 (depends on 1)

The secondary battery of claim 1, wherein the anode comprises silicon-containing active material particles.

### Claim 3 (depends on 1)

The secondary battery of claim 1, wherein the binder polymer comprises polyacrylamide.

### Claim 4 (depends on 1)

The secondary battery of claim 1, wherein the coating layer is between the anode and the porous substrate.

### Claim 5 (depends on 1)

The secondary battery of claim 1, wherein the second repeating unit is a derivative of a crosslinking agent.

### Claim 6 (depends on 5)

The secondary battery of claim 5, wherein the crosslinking agent is a compound comprising a carbon-carbon double bond at both ends.

### Claim 7 (depends on 6)

The secondary battery of claim 6, wherein the crosslinking agent is at least one selected from the group consisting of N,N′-methylenebisacrylamide, N,N′-bisacrylylcystamine, and N,N′-diallyltartardiamide.

### Claim 8 (depends on 1)

The secondary battery of claim 1, further comprising a crosslinked matrix formed from the first repeating unit and the second repeating unit, wherein the crosslinked matrix has a degree of crosslinking of 5 to 15%.

### Claim 9 (depends on 1)

The secondary battery of claim 1, wherein the anode is adhered to the separator, and an adhesive force of the anode to the separator is 10 to 15 gf/20 mm.

### Claim 10

A method for manufacturing a secondary battery, the method comprising:
coating a composition for forming a coating layer on at least one surface of a porous substrate and then drying the composition for forming the coating layer to manufacture a separator; and
forming an anode from an anode slurry on one surface of the separator,
wherein the composition for forming the coating layer comprises an initiator and a crosslinking agent, and the anode slurry comprises a binder polymer.

### Claim 11 (depends on 10)

The method of claim 10, wherein a content of the crosslinking agent is 0.01 to 0.10 parts by weight based on 100 parts by weight of the binder polymer.

### Claim 12 (depends on 10)

The method of claim 10, wherein a content of the binder polymer is 5 to 15% by weight based on a weight of a total solid content contained in the anode slurry.

### Claim 13 (depends on 10)

The method of claim 10, wherein the composition for forming the coating layer further comprises a polymerization reaction catalyst.

### Claim 14 (depends on 10)

The method of claim 10, further comprising:
forming a cathode on another surface of the separator to manufacture an electrode assembly;
introducing the electrode assembly into a battery case, and then injecting an electrolyte into the battery case; and
placing the battery case into which the electrolyte has been injected into a chamber at a temperature of 40 to 80° C. to perform a crosslinking reaction.

### Claim 15 (depends on 1)

The secondary battery of claim 1, wherein the first repeating unit is the same as the second repeating unit.

### Claim 16 (depends on 1)

The secondary battery of claim 1, wherein the first repeating unit is different from the second repeating unit.

### Claim 17 (depends on 8)

The secondary battery of claim 8, wherein the degree of crosslinking of the crosslinked matrix is 7 to 12%.

### Claim 18 (depends on 6)

The secondary battery of claim 6, wherein the crosslinking agent is at least one selected from the group consisting of N,N′-methylenebisacrylamide and N,N′-bisacrylylcystamine.

### Claim 19 (depends on 10)

The method of claim 10, wherein a content of the crosslinking agent is 0.03 to 0.07 parts by weight based on 100 parts by weight of the binder polymer.

### Claim 20 (depends on 10)

The method of claim 10, wherein a content of the binder polymer is 5 to 10% by weight based on a weight of a total solid content contained in the anode slurry.