# US 2025/0158049 A1 · Positive electrode material, preparation method thereof, and applications

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158049 A1
- Document ID: US20250158049A1
- Status: Published application
- Kind: A1
- Application number: 18/534,681
- Filed: 2023-12-10
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: AESC Japan Ltd.
- Applicants: AESC Japan Ltd.
- Inventors: Le Yu; Qian Li; Wenbin Lyu
- Web page: https://patentgrep.com/patent/US20250158049A1

## CPC

- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- H01M 4/0407: {by coating on an electrolyte layer}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The disclosure proposes a positive electrode material, a preparation method thereof, and applications. The positive electrode material at least includes a positive electrode active material including LiNi0.5Mn1.5O4; and a coating layer coated on the positive electrode active material, wherein the coating layer includes a halide solid electrolyte, and the chemical formula of the halide solid electrolyte is Liz+aZr1-aFeaCl6-x-yBrxIy, in which 0<a≤0.5; x=0 to 6, y=0 to 6, x+y≤6. The disclosure proposes the positive electrode material, the preparation method thereof, and the applications, which can improve the rate performance and the cycle performance of a lithium-ion battery.

## Claims

### Claim 1

A positive electrode material, at least comprising:
a positive electrode active material comprising LiNi0.5Mn1.5O4; and
a coating layer coated on the positive electrode active material, wherein the coating layer comprises a halide solid electrolyte, and a chemical formula of the halide solid electrolyte is Liz+aZr1-aFeaCl6-x-yBrxIy, wherein 0<a≤0.5; x=0 to 6, y=0 to 6, x+y≤6.

### Claim 2 (depends on 1)

The positive electrode material of claim 1, wherein a molar ratio of iron atoms on a surface of the positive electrode material measured by an energy dispersive X-ray spectrometer is 0.2% to 5%.

### Claim 3 (depends on 1)

The positive electrode material of claim 1, wherein a chemical formula of the halide solid electrolyte is Li2.3Zr0.7Fe0.3Cl6.

### Claim 4 (depends on 1)

The positive electrode material of claim 1, wherein the positive electrode active material is in a secondary spherical form or a single crystal form.

### Claim 5 (depends on 4)

The positive electrode material of claim 4, wherein a median particle diameter D50 of the positive electrode active material in the secondary spherical form is 10 μm to 40 km.

### Claim 6 (depends on 4)

The positive electrode material of claim 4, wherein a median particle diameter D50 of the positive electrode active material in the single crystal form is 1 μm to 16 km.

### Claim 7

A preparation method for a positive electrode material, at least comprising:
mixing corresponding amounts of compounds comprising Li, Zr, and Fe according to a chemical formula of a halide solid electrolyte, grinding, and performing a first sintering to obtain the halide solid electrolyte; and
blending the halide solid electrolyte and a positive electrode active material according to a mass ratio and performing a second sintering to obtain a positive electrode material.

### Claim 8 (depends on 7)

The preparation method for the positive electrode material of claim 7, wherein the mass ratio of the halide solid electrolyte and the positive electrode active material is (0.1 to 1.2):(99.9 to 98.8).

### Claim 9 (depends on 7)

The preparation method for the positive electrode material of claim 7, wherein conditions for the blending comprises: a mixing speed of 100 rpm to 10000 rpm, and a mixing time of 1 h to 48 h.

### Claim 10 (depends on 7)

The preparation method for the positive electrode material of claim 7, wherein for the first sintering, a temperature is 250° C. to 350° C., and a sintering time is 3 h to 5 h.

### Claim 11 (depends on 7)

The preparation method for the positive electrode material of claim 7, wherein for the second sintering, a temperature is 200° C. to 500° C., and a sintering time is 6 h to 18 h.

### Claim 12 (depends on 1)

A lithium-ion battery comprises the positive electrode material of claim 1.

### Claim 13 (depends on 12)

An electronic device comprises the lithium-ion battery of claim 12.