# US 2025/0158048 A1 · Positive electrode material and preparation method and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158048 A1
- Document ID: US20250158048A1
- Status: Published application
- Kind: A1
- Application number: 18/527,384
- Filed: 2023-12-04
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: AESC Japan Ltd.
- Applicants: AESC Japan Ltd.
- Inventors: Le Yu; Qian Li; Wenbin Lyu
- Web page: https://patentgrep.com/patent/US20250158048A1

## CPC

- H01M 4/366: {as layered products}
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0068: inorganic
- H01M 2300/008: Halides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention provides a positive electrode material and a preparation method and an application thereof. The positive electrode material at least includes: a positive electrode active material; and a coating layer coating the positive electrode active material, the coating layer including a halide solid electrolyte; wherein: the positive electrode active material includes nLi2MnO3·(1−n)LiMnaCobNicO2, and 0.2≤n≤0.5, a+b+c=1; a chemical formula of the halide solid electrolyte is Li2+mZr1−mFemCl6−x−yBrxIy, and 0<m≤0.5; x=0 to 6, y=0 to 6, x+y≤6. The invention provides a positive electrode material and a preparation method and an application thereof that may improve the interface stability between a positive electrode sheet and a solid electrolyte and improve a stability and a cycle performance of a lithium-ion battery.

## Claims

### Claim 1

A positive electrode material, at least comprising:
a positive electrode active material; and
a coating layer coating the positive electrode active material, the coating layer comprising a halide solid electrolyte;
wherein: the positive electrode active material comprises nLi2MnO3·(1−n)LiMnaCobNicO2, and 0.2≤n≤0.5, a+b+c=1; a chemical formula of the halide solid electrolyte is Li2+mZr1−mFemCl6−x−yBrxIy, and 0<m≤0.5; x=0 to 6, y=0 to 6, x+y≤6.

### Claim 2 (depends on 1)

The positive electrode material of claim 1, wherein a molar ratio of iron atoms at a surface of the positive electrode material measured by an energy dispersive X-ray spectrometer is 0.4% to 7%.

### Claim 3 (depends on 1)

The positive electrode material of claim 1, wherein a chemical formula of the halide solid electrolyte is Li2.3Zr0.7Fe0.3Cl6.

### Claim 4 (depends on 1)

The positive electrode material of claim 1, wherein the positive electrode active material is in a spherical shape.

### Claim 5 (depends on 4)

The positive electrode material of claim 4, wherein a median particle diameter D50 of the positive electrode active material in the spherical shape is 8 μm to 20 μm.

### Claim 6

A preparation method of a positive electrode material, at least comprising the following steps:
mixing corresponding amounts of compounds containing Li, Zr, and Fe elements and grinding and performing a first sintering to obtain a halide solid electrolyte according to a chemical formula of the halide solid electrolyte; and
blending and performing a second sintering on the halide solid electrolyte and a positive electrode active material according to a mass ratio to obtain a positive electrode material.

### Claim 7 (depends on 6)

The preparation method of the positive electrode material of claim 6, wherein a mass ratio of the halide solid electrolyte and the positive electrode active material is (0.2 to 6):(99.9 to 94).

### Claim 8 (depends on 6)

The preparation method of the positive electrode material of claim 6, wherein conditions of the blending comprise: a mixing speed of 100 rpm to 800 rpm, and a mixing time of 1 h to 6 h.

### Claim 9 (depends on 6)

The preparation method of the positive electrode material of claim 6, wherein a temperature of the second sintering is 950° C. to 1050° C., and a sintering time is 6 h to 18 h.

### Claim 10 (depends on 1)

A lithium-ion battery, comprising the positive electrode material of claim 1.

### Claim 11 (depends on 1)

An electronic equipment, comprising the positive electrode material of claim 1.