# US 2025/0158047 A1 · Aluminum battery and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158047 A1
- Document ID: US20250158047A1
- Status: Published application
- Kind: A1
- Application number: 18/764,331
- Filed: 2024-07-04
- Published: 2025-05-15
- Earliest claimed: 2023-11-10
- Assignees: APh ePower Co., Ltd.
- Applicants: APh ePower Co., Ltd.
- Inventors: Jui-Hsuan Wu; Shih Po Ta Tsai; Wei-Ting Chen; Kuan-Ting Chen; Fei-Yi Hung
- Web page: https://patentgrep.com/patent/US20250158047A1

## CPC

- H01M 4/463: {Aluminium based}
- H01M 4/0419: {involving spraying}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

An aluminum battery includes a negative electrode structure. The negative electrode structure includes a substrate and an aluminum alloy layer located on the substrate. The aluminum alloy layer includes an aluminum element and a non-aluminum element. A content of the aluminum element in the aluminum alloy layer is greater than or equal to 85 wt % and less than 100 wt %, while a content of the non-aluminum element in the aluminum alloy layer is less than or equal to 15 wt % and greater than 0 wt %. A manufacturing method of the aluminum battery is also provided.

## Claims

### Claim 1

An aluminum battery, comprising:
a negative electrode structure, comprising:
a substrate; and
an aluminum alloy layer, located on the substrate, wherein the aluminum alloy layer comprises an aluminum element and a non-aluminum element, a content of the aluminum element in the aluminum alloy layer is greater than or equal to 85 wt % and less than 100 wt %, while a content of the non-aluminum element in the aluminum alloy layer is less than or equal to 15 wt % and greater than 0 wt %.

### Claim 2 (depends on 1)

The aluminum battery as claimed in claim 1, wherein the non-aluminum element comprises silicon (Si), magnesium (Mg), nickel (Ni), copper (Cu), zinc (Zn) or combinations thereof.

### Claim 3 (depends on 1)

The aluminum battery as claimed in claim 1, wherein a thickness of the aluminum alloy layer ranges from 50 μm to 500 μm.

### Claim 4 (depends on 1)

The aluminum battery as claimed in claim 1, wherein the aluminum alloy layer is composed of solid alloy powder particles of the aluminum element and the non-aluminum element.

### Claim 5 (depends on 4)

The aluminum battery as claimed in claim 4, wherein an average particle size of the solid alloy powder particles ranges from 10 μm to 200 μm.

### Claim 6

A manufacturing method of an aluminum battery, comprising:
providing a substrate; and
performing a thermal spray process to spray aluminum alloy powder on the substrate to form an aluminum alloy layer and obtain a negative electrode structure of the aluminum battery.

### Claim 7 (depends on 6)

The manufacturing method of the aluminum battery as claimed in claim 6, wherein after performing the thermal spray process, the aluminum alloy powder is melted and sintered and stacked on the substrate.

### Claim 8 (depends on 6)

The manufacturing method of the aluminum battery as claimed in claim 6, wherein after performing the thermal spray process, the aluminum alloy powder is staggered and stacked on the substrate.

### Claim 9 (depends on 6)

The manufacturing method of the aluminum battery as claimed in claim 6, wherein a temperature range of the thermal spray process is 1000° C. to 2000° C., and the thermal spray process is performed for 10 seconds to 120 seconds.

### Claim 10 (depends on 6)

The manufacturing method of the aluminum battery as claimed in claim 6, wherein before performing the thermal spray process, the method further comprises performing a surface treatment process on the substrate.