# US 2025/0158026 A1 · Negative Electrode For Secondary Battery And Manufacturing Method Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158026 A1
- Document ID: US20250158026A1
- Status: Published application
- Kind: A1
- Application number: 18/946,269
- Filed: 2024-11-13
- Published: 2025-05-15
- Earliest claimed: 2023-11-15
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Chang Ju Lee; Sung Min Park; Sang Wook Woo; Yong Ju Lee
- Web page: https://patentgrep.com/patent/US20250158026A1

## CPC

- H01M 4/364: {as mixtures}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/133: Electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/1393: of electrodes based on carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/583: Carbonaceous material, e.g. graphite-intercalation compounds or CFx
- H01M 4/587: for inserting or intercalating light metals
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A negative electrode for a secondary battery includes: a negative electrode current collector; and a negative electrode active layer provided on at least one surface of the negative electrode current collector and including a carbon-based negative electrode active material. The carbon-based negative electrode active material includes transition metal particles. The transition metal particles includes iron and nickel. The carbon-based negative electrode active material includes total transition metal particles including iron and nickel at a concentration of about 1,200 ppm or less. The concentration ratio of iron and nickel (Fe/Ni) included in the carbon-based negative electrode active material is about 2.5 to 13.0.

## Claims

### Claim 1

A negative electrode for a secondary battery, the negative electrode comprising:
a negative electrode current collector; and
a negative electrode active layer provided on at least one surface of the negative electrode current collector and including a carbon-based negative electrode active material,
wherein the carbon-based negative electrode active material includes transition metal particles,
the transition metal particles includes iron and nickel,
the carbon-based negative electrode active material includes total transition metal particles including iron and nickel at a concentration of about 1,200 ppm or less, and
the concentration ratio of iron and nickel (Fe/Ni) included in the carbon-based negative electrode active material is about 2.5 to 13.0.

### Claim 2 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein a concentration of iron included in the carbon-based negative electrode active material is about 0.1 ppm to 1,000 ppm.

### Claim 3 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein a concentration of nickel included in the carbon-based negative electrode active material is about 0.01 ppm to 500 ppm.

### Claim 4 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein the carbon-based negative electrode active material includes total transition metal particles including iron and nickel at a concentration of about 0.01 ppm to 1,100 ppm.

### Claim 5 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein the transition metal particles include about 50% or more of ion based on the total weight.

### Claim 6 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein the transition metal particles included in the carbon-based negative electrode active material further include at least one of cobalt, chromium, zinc, magnesium, manganese, and copper.

### Claim 7 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein the carbon-based negative electrode active material is an artificial graphite in a form of secondary particles assembled from primary particles.

### Claim 8 (depends on 1)

The negative electrode for a secondary battery according to claim 1, wherein the transition metal included in the negative active material includes a metal having magnetism and a metal having no magnetism, and
the metal having magnetism and the metal having no magnetism are present in a form of an alloy.

### Claim 9

A method of manufacturing a negative electrode for a secondary battery, the method comprising:
applying a negative electrode slurry including a carbon-based negative electrode active material to at least one surface of a negative electrode current collector, followed by drying the negative electrode slurry applied to the negative electrode current collector to form a negative electrode active layer,
wherein the carbon-based negative electrode active material includes transition metal particles,
the transition metal particles includes iron and nickel,
the carbon-based negative electrode active material includes total transition metal particles including iron and nickel at a concentration of about 1,200 ppm or less, and
a concentration ratio of iron and nickel (Fe/Ni) included in the carbon-based negative electrode active material is about 2.5 to 13.0.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the carbon-based negative electrode active material is prepared by
(S1) graphitizing a carbon raw material;
(S2) carbonizing the carbon raw material graphitized in (S1); and
(S3) adjusting a concentration of transition metal particles having magnetism present in the carbon raw material by applying a magnetic field to the carbon raw material at least once before and after (S2).

### Claim 11 (depends on 10)

The method according to claim 10, wherein, in (S3), the magnetic field is applied with a strength of about 1,000 G to 40,000 G for about 1 to 600 seconds.

### Claim 12 (depends on 10)

The method according to claim 10, wherein (S3) is performed before or after (S2).

### Claim 13 (depends on 9)

The method according to claim 9, wherein a concentration of iron included in the carbon-based negative electrode active material is about 0.1 ppm to 1,000 ppm.

### Claim 14 (depends on 9)

The method according to claim 9, wherein a concentration of nickel included in the carbon-based negative electrode active material is about 0.01 ppm to 500 ppm.

### Claim 15 (depends on 9)

The method according to claim 9, wherein the transition metal particles included in the carbon-based negative electrode active material further include at least one of cobalt, chromium, zinc, magnesium, manganese, and copper.

### Claim 16 (depends on 9)

The method according to claim 9, wherein the transition metal included in the negative active material includes a metal having magnetism and a metal having no magnetism, and
the metal having magnetism and the metal having no magnetism are present in a form of an alloy.