# US 2025/0158022 A1 · Positive Electrode Material, and Positive Electrode and Lithium Secondary Battery Which Include the Same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158022 A1
- Document ID: US20250158022A1
- Status: Published application
- Kind: A1
- Application number: 18/838,147
- Filed: 2023-02-15
- Published: 2025-05-15
- Earliest claimed: 2022-02-15
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Kang Joon Park; So Ra Baek; Wang Mo Jung; Sin Young Park; Hyuck Hur; Dong Hwi Kim; Min Kwak; Seul Ki Chae
- Web page: https://patentgrep.com/patent/US20250158022A1

## CPC

- H01M 4/364: {as mixtures}
- C01G 53/42: containing alkali metals, e.g. LiNiO2
- C01G 53/504: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.5, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.5
- C01G 53/506: with the molar ratio of nickel with respect to all the metals other than alkali metals higher than or equal to 0.8, e.g. Li(MzNixCoyMn1-x-y-z)O2 with x ≥ 0.8
- H01M 4/02: Electrodes composed of, or comprising, active material
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2002/72: by d-values or two theta-values, e.g. as X-ray diagram
- C01P 2004/45: Aggregated particles or particles with an intergrown morphology
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A positive electrode material for a lithium secondary battery includes: a first positive electrode active material and a second positive electrode active material. The first positive electrode active material includes a lithium transition metal oxide in which a molar ratio of nickel among transition metals is 70 mol % or more, the second positive electrode active material includes a lithium transition metal oxide in which a molar ratio of nickel among transition metals is 25 mol % or more less than the molar ratio of the nickel among the transition metals of the first positive electrode active material, an average particle diameter of primary particles constituting the second positive electrode active material is larger than an average particle diameter of primary particles constituting the first positive electrode active material, and D50 of the second positive electrode active material is smaller than D50 of the first positive electrode active material.

## Claims

### Claim 1

A positive electrode material for a lithium secondary battery, comprising:
a first positive electrode active material and a second positive electrode active material,
wherein the first positive electrode active material comprises a first lithium transition metal oxide having a molar ratio of nickel of 70 mol % or more relative to a total amount of transition metals of the first lithium transition metal oxide,
wherein the second positive electrode active material comprises a second lithium transition metal oxide having a molar ratio of nickel of 25 mol % or more less than the molar ratio of the nickel of the first lithium transition metal oxide,
wherein an average particle diameter of primary particles constituting the second positive electrode active material is larger than an average particle diameter of primary particles constituting the first positive electrode active material, and
wherein D50 of the second positive electrode active material is smaller than D50 of the first positive electrode active material.

### Claim 2 (depends on 1)

The positive electrode material of claim 1, wherein the molar ratio of the nickel in the second lithium transition metal oxide relative to a total amount of transition metals of the second lithium transition metal oxide is from 40 mol % to 65 mol %.

### Claim 3 (depends on 1)

The positive electrode material of claim 1, wherein the first lithium transition metal oxide is represented by Formula 1:
Li1+x(NiaCObMncMd)O2 [Formula 1]
wherein,
M is at least one of W, Cu, Fe, V, Cr, Ti, Zr, Zn, Al, In, Ta, Y, La, Sr, Ga, Sc, Gd, Sm, Ca, Ce, Nb, Mg, B, or Mo, and
x, a, b, c, and d respectively satisfy −0.2≤x≤0.2, 0.70≤a<1, 0<b≤0.20, 0<c≤0.20, 0≤d≤0.10, and a+b+c+d=1.

### Claim 4 (depends on 1)

The positive electrode material of claim 1, wherein the second lithium transition metal oxide is represented by Formula 2:
Li1+y(NieCofMngM′h)O2 [Formula 2]
wherein,
M′ is at least one doping element of W, Cu, Fe, V, Cr, Ti, Zr, Zn, Al, In, Ta, Y, La, Sr, Ga, Sc, Gd, Sm, Ca, Ce, Nb, Mg, B, or Mo, and
y, e, f, g, and h respectively satisfy −0.2≤y≤0.2, 0.40≤e≤0.65, 0.10≤f≤0.40, 0.10≤g≤0.40, 0≤h≤0.10, and e+f+g+h=1.

### Claim 5 (depends on 1)

The positive electrode material of claim 1, wherein the average particle diameter of the primary particles constituting the first positive electrode active material is from 0.1 μm to 1 μm.

### Claim 6 (depends on 1)

The positive electrode material of claim 1, wherein the average particle diameter of the primary particles constituting the second positive electrode active material is 1 μm to 3 μm.

### Claim 7 (depends on 1)

The positive electrode material of claim 1, wherein the D50 of the first positive electrode active material is from 8 μm to 20 μm.

### Claim 8 (depends on 1)

The positive electrode material of claim 1, wherein the D50 of the second positive electrode active material is from 1 μm to less than 8 μm.

### Claim 9 (depends on 1)

The positive electrode material of claim 1, wherein an absolute value of a difference between a rate of change in c-axis length according to Equation 1 of the first positive electrode active material and a rate of change in c-axis length according to Equation 1 of the second positive electrode active material is from 0% to 10%:
Rate
⁢
of
⁢
change
⁢
in
⁢
c
-
axis
⁢
length
⁢
(
%
)
=
{
(
C
o
⁢
1
-
C
1
⁢
o
)
/
C
o
)
×
1
⁢
0
⁢
0
}
[
Equation
⁢
1
]
wherein,
Co is a c-axis length of the positive electrode active material in an uncharged state, and C1 is a c-axis length of the positive electrode active material in a state of being charged to 4.2 V.

### Claim 10 (depends on 1)

The positive electrode material of claim 1, wherein the positive electrode material comprises the first positive electrode active material and the second positive electrode active material in a weight ratio of from 50:50 to 99:1.

### Claim 11 (depends on 1)

A positive electrode for a lithium secondary battery, comprising the positive electrode material of claim 1.

### Claim 12 (depends on 11)

A lithium secondary battery comprising the positive electrode of claim 11.