# US 2025/0158017 A1 · Magnesium secondary battery and method for manufacturing magnesium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158017 A1
- Document ID: US20250158017A1
- Status: Published application
- Kind: A1
- Application number: 18/928,279
- Filed: 2024-10-28
- Published: 2025-05-15
- Earliest claimed: 2023-11-13
- Assignees: The Furukawa Battery Co., Ltd.
- Applicants: THE FURUKAWA BATTERY CO., Ltd.
- Inventors: Naoki TAKEGUCHI
- Web page: https://patentgrep.com/patent/US20250158017A1

## CPC

- H01M 4/0445: {Forming after manufacture of the electrode, e.g. first charge, cycling}
- H01M 4/466: {Magnesium based}
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 10/446: {Initial charging measures}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A magnesium secondary battery includes: a positive electrode; a negative electrode having a magnesium layer made of a eutectic magnesium alloy; a separator; and an electrolytic solution, in which in powder X-ray diffraction measurement of the negative electrode using a CuKα ray, when an intensity ratio Y obtained from a diffraction peak representing a (100) plane within a range of 2θ=32°±5° and a diffraction peak representing a (002) plane within a range of 2θ=35°±5° is defined as a diffraction peak intensity ratio of (100)/(002), 15<Y is satisfied.

## Claims

### Claim 1

A magnesium secondary battery comprising:
a positive electrode;
a negative electrode having a magnesium layer made of a eutectic magnesium alloy;
a separator; and
an electrolytic solution, wherein
in powder X-ray diffraction measurement of the negative electrode using a Cukα ray, when an intensity ratio Y obtained from a diffraction peak representing a (100) plane within a range of 2θ=32°±5° and a diffraction peak representing a (002) plane within a range of 2θ=35°±5° is defined as a diffraction peak intensity ratio of (100)/(002), 15<Y is satisfied.

### Claim 2 (depends on 1)

The magnesium secondary battery according to claim 1, wherein
the magnesium alloy has a crystal structure in which a hexagonal closest-packed structure and a body-centered cubic structure are in a eutectic state.

### Claim 3 (depends on 2)

The magnesium secondary battery according to claim 2, wherein
the magnesium alloy contains lithium in a range of 6% by weight or more and 10.5% by weight or less.

### Claim 4

A method for manufacturing a magnesium secondary battery including a positive electrode, a negative electrode having a magnesium layer made of a magnesium alloy, a separator, and an electrolytic solution, the method comprising
an activation step of performing charging and discharging at 5 mA/cm2 or more.

### Claim 5 (depends on 4)

The method for manufacturing a magnesium secondary battery according to claim 4, wherein one charging and discharging cycle in which charging is performed for one hour or more and discharging is performed for one hour or more is performed for ten cycles or more.

### Claim 6 (depends on 4)

The method for manufacturing a magnesium secondary battery according to claim 4, further comprising one charging and discharging cycle in which an upper limit of SOC during charging is 2% or more and 10% or less.

### Claim 7 (depends on 4)

The method for manufacturing a magnesium secondary battery according to claim 4, wherein a negative electrode having a magnesium layer made of a magnesium alloy containing 3% by weight or more of other metals is used.

### Claim 8 (depends on 4)

The method for manufacturing a magnesium secondary battery according to claim 4, wherein a negative electrode having a magnesium layer made of a eutectic magnesium alloy is used.