# US 2025/0158012 A1 · Electrode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158012 A1
- Document ID: US20250158012A1
- Status: Published application
- Kind: A1
- Application number: 18/274,691
- Filed: 2022-01-28
- Published: 2025-05-15
- Earliest claimed: 2021-01-29
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Ho Chan LEE; In Taek SONG; Il Ha LEE; Geun Sung LEE; Ki Hwan KIM; Yeong Bong MOK; Jin Woo PARK
- Web page: https://patentgrep.com/patent/US20250158012A1

## CPC

- H01M 4/0435: {Rolling or calendering}
- H01M 4/13: Electrodes for accumulators with non-aqueous electrolyte, e.g. for lithium-accumulators; Processes of manufacture thereof
- H01M 4/02: Electrodes composed of, or comprising, active material
- H01M 4/04: Processes of manufacture in general
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/139: Processes of manufacture
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/622: {being polymers}
- H01M 4/623: {fluorinated polymers}
- H01M 4/66: Selection of materials
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/052: Li-accumulators
- H01M 4/662: {Alloys (collectors of lead alloys H01M4/685)}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application relates to an electrode comprising a current collector and an active material layer, which can provide an electrode capable of securing a high level of adhesion force between particles and adhesion force between the active material layer and the current collector relative to the content of binder in the active material layer. The present application can also provide a use of the electrode.

## Claims

### Claim 1

An electrode, comprising:
a current collector; and
an active material layer on one or both sides of the current collector,
wherein the active material layer comprises an electrode active material and a particulate binder,
wherein a ratio (A/W) of an area ratio (A) of an occupied region of the binder on the current collector relative to a binder content (W) in the active material layer is 17 or more, which is confirmed according to the following standard peel test, and
wherein a ratio of a height of the occupied region of the binder relative to an average particle diameter of the particulate binder is 0.5 or more:
Standard peel test: a process of attaching a Scotch Magic Tape Cat. 810R on the active material layer, and then peeling off it is repeated until no component of the active material layer is observed on the Scotch Magic Tape Cat. 810R.

### Claim 2 (depends on 1)

The electrode according to claim 1, further comprising a silicon-containing layer between the active material layer and the current collector.

### Claim 3 (depends on 1, 2)

The electrode according to claim 1 or 2, wherein the current collector is a film, sheet or foil made of one or more selected from the group consisting of stainless steel, aluminum, nickel, titanium, baked carbon, copper, carbon, stainless steel surface-treated with nickel, titanium or silver, and an aluminum-cadmium alloy.

### Claim 4 (depends on 1, 2, 3)

The electrode according to any one of claims 1 to 3, wherein the binder comprises one or more selected from the group consisting of PVDF (poly (vinylidene fluoride)), PVA (poly (vinyl alcohol)), polyvinylpyrrolidone, tetrafluoroethylene, polyethylene, polypropylene, an ethylene-propylene-diene terpolymer (EPDM), a sulfonated EPDM, SBR (styrene-butadiene rubber), and fluororubber.

### Claim 5 (depends on 1, 2, 3, 4)

The electrode according to any one of claims 1 to 4, wherein the binder has an average particle diameter of 50 to 500 nm.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The electrode according to any one of claims 1 to 5, wherein the electrode active material and the binder are particulates, and the ratio (D1/D2) of the average particle diameter (D1) of the electrode active material to the average particle diameter (D2) of the binder is in a range of 10 to 1000.

### Claim 7 (depends on 6)

The electrode according to claim 6, wherein the electrode active material has an average particle diameter in a range of 1 μm to 100 μm.

### Claim 8 (depends on 6)

The electrode according to claim 6, wherein the ratio (D90/D10) of the 90% volume cumulative particle diameter (D90) to the 10% volume cumulative particle diameter (D10) in the electrode active material is 15 or less.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The electrode according to any one of claims 1 to 8, wherein the binder in the active material layer has a content in a range of 0.5 to 10 weight %.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

The electrode according to any one of claims 1 to 9, wherein the electrode active material is included in the active material layer in an amount of 1000 to 10000 parts by weight relative to 100 parts by weight of the binder.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The electrode according to any one of claims 1 to 10, wherein the active material layer has a thickness in a range of 10 μm to 500 μm.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

A method for manufacturing the electrode of any one of claims 1 to 11 comprising:
forming a layer of slurry on the current collector,
wherein the slurry comprises a solvent having a dipole moment of 1.3D or more, the binder, and the electrode active material, and
wherein a silicon-containing layer is on the surface of the current collector on which the layer of the slurry is formed.

### Claim 13 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

A method for manufacturing the electrode of any one of claims 1 to 11 comprising:
forming a layer of slurry on the current collector,
wherein the slurry comprises a solvent having a dipole moment of 1.3D or more, a binder having a solubility parameter in a range of 10 to 30 MPa1/2, and the electrode active material, and
wherein a surface of the current collector on which the layer of the slurry is formed has a water contact angle of 50 degrees or more.

### Claim 14 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

An electrochemical element comprising the electrode of any one of claims 1 to 11 as a positive electrode or a negative electrode.

### Claim 15 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

A secondary battery comprising the electrode of any one of claims 1 to 11 as a negative electrode or a positive electrode.