# US 2025/0158011 A1 · Lithium secondary battery and preparation method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0158011 A1
- Document ID: US20250158011A1
- Status: Published application
- Kind: A1
- Application number: 18/414,343
- Filed: 2024-01-16
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: Shenzhen Huineng Energy Storage Materials Engineering Research Center Co., LTD.; National Engineering Research Center of Advanced Energy Storage Materials (Shenzhen) Co., Ltd.
- Applicants: Shenzhen Huineng Energy Storage Materials Engineering Research Center Co., LTD.; National Engineering Research Center of Advanced Energy Storage Materials (Shenzhen) Co., Ltd.
- Inventors: Faping ZHONG; Chihuan HE; Subin JIANG; Hongbing LIU; Jiqun ZHU; Shuifa TAN
- Web page: https://patentgrep.com/patent/US20250158011A1

## CPC

- C23C 6/00: Coating by casting molten material on the substrate
- H01M 4/0426: {Sputtering}
- C23C 14/06: characterised by the coating material ({C23C14/0021} , C23C14/04 take precedence)
- C23C 14/0676: {Oxynitrides}
- C23C 14/185: {by cathodic sputtering}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/5806: {Thermal treatment}
- C23C 24/06: Compressing powdered coating material, e.g. by milling
- C23C 28/32: {including at least one pure metallic layer}
- C23C 28/34: {including at least one inorganic non-metallic material layer, e.g. metal carbide, nitride, boride, silicide layer and their mixtures, enamels, phosphates and sulphates}
- H01M 4/0407: {by coating on an electrolyte layer}
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/0471: {involving thermal treatment, e.g. firing, sintering, backing particulate active material, thermal decomposition, pyrolysis}
- H01M 4/0485: {Casting}
- H01M 4/136: Electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/1397: of electrodes based on inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 4/625: {Carbon or graphite}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 10/0585: of accumulators having only flat construction elements, i.e. flat positive electrodes, flat negative electrodes and flat separators
- H01M 10/4235: {Safety or regulating additives or arrangements in electrodes, separators or electrolyte (H01M10/4242 takes precedence)}
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0068: inorganic
- H01M 2300/008: Halides
- H01M 2300/0094: in the form of layered products, e.g. coatings
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention provides a lithium secondary battery and a preparation method thereof.

## Claims

### Claim 1

A preparation method for a lithium secondary battery, comprising:
(1) carrying out magnetron sputtering in a nitrogen atmosphere by using a sulfide solid electrolyte layer as a base material and using Li3PO4 as a target material, to sputter a LiPON thin film layer on one surface of the base material;
(2) vacuumizing a magnetron sputtering chamber, then introducing argon, and sputtering a Li3PO4 thin film layer on the other surface of the base material by using the Li3PO4 as the target material;
(3) maintaining an argon atmosphere, simultaneously co-sputtering three target materials: a Li3PO4 target, a Fe2O3 target, and a carbon target, and depositing a composite material layer on the Li3PO4 thin film layer to obtain a multilayer material with the composite material layer/Li3PO4 thin film layer/sulfide solid electrolyte layer/LiPON thin film layer;
(4) transferring the multilayer material into sintering equipment, and carrying out high-temperature calcination in the argon atmosphere to transform the composite material layer into a positive active material layer through a high-temperature solid-phase reaction;
(5) carrying out magnetron sputtering on the material subjected to the high-temperature calcination by using an aluminum target, to sputter and deposit an aluminum current collector layer on a surface of the positive active material layer;
(6) uniformly dropwise coating a surface of the LiPON thin film layer with molten metal lithium under an argon protection atmosphere, applying a pressure after cooling to flatten a metal lithium layer, and compressing a battery core; and
(7) packaging the battery core in a battery shell to obtain the lithium secondary battery.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein a purity of the target material used is greater than or equal to 99.9%.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein the sulfide solid electrolyte in step (1) is one or more of Li2S P2S5, Li10GeP2S12, Li7P2S8X, and Li6PS5X, and X is one or more of Cl, Br, and I; and the sulfide solid electrolyte layer is prepared by tabletting sulfide solid electrolyte powder.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the LiPON thin film layer in step (1) has a thickness of 5 to 10 μm.

### Claim 5 (depends on 1)

The preparation method according to claim 1, wherein the Li3PO4 thin film layer in step (2) has a thickness of 0.1 to 1 μm.

### Claim 6 (depends on 1)

The preparation method according to claim 1, wherein the composite material layer in step (3) has a thickness of 5 to 10 μm.

### Claim 7 (depends on 1)

The preparation method according to claim 1, wherein the high-temperature calcination in step (4) is two-stage sintering; in the first stage of sintering, a heating rate is 3 to 5° C./min, a sintering temperature is 350 to 450° C., and the temperature is kept for 3 to 6 h; and in the second stage of sintering, a heating rate is 5 to 10° C./min, a sintering temperature is 650 to 900° C., and the temperature is kept for 6 to 18 h.

### Claim 8 (depends on 1)

The preparation method according to claim 1, wherein the aluminum current collector layer in step (5) has a thickness of 1 to 10 μm.

### Claim 9 (depends on 1)

The preparation method according to claim 1, wherein the metal lithium layer in step (6) has a thickness of 1 to 5 μm; and the applying a pressure is performed by applying a pressure of 5 to 10 MPa to one side of the metal lithium layer using a polyimide plate.

### Claim 10 (depends on 1)

A lithium secondary battery, wherein the lithium secondary battery is prepared by the preparation method according to claim 1.
