# US 2025/0157952 A1 · Spacers for beol multi-patterning

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0157952 A1
- Document ID: US20250157952A1
- Status: Published application
- Kind: A1
- Application number: 18/917,894
- Filed: 2024-10-16
- Published: 2025-05-15
- Earliest claimed: 2023-11-15
- Assignees: ASM IP Holding B.V.; Imec Vzw
- Applicants: Asm IP Holding B.V.; Imec Vzw
- Inventors: Debanjan Jana; Yiting Sun; David De Roest; Daniele Piumi; Sara Paolillo; Philippe Bezard; Vincent Renaud
- Web page: https://patentgrep.com/patent/US20250157952A1

## CPC

- H10W 44/401: {Resistive arrangements (H10W44/20, H10W42/80 take precedence)}
- H10P 14/69394: {the material containing titanium, e.g. TiO2}
- H10P 50/285: {of materials not containing Si, e.g. PZT or Al2O3}
- H10P 50/287: {by chemical means}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming an intermediate in the multiple patterning lithographic formation of a semiconductor device mask involves: 1) Providing a target layer; 2) Using EUV lithography to form mandrels on the target layer, with a pitch of less than 40 nm; 3) Depositing a conformal spacer material on the mandrels, narrowing the gaps between them; 4) Performing a directional etch to expose the top surface of the mandrels. The spacer material has a resistivity lower than 104 Ω·cm at 20° C.

## Claims

### Claim 1

A method using EUV lithography for forming an intermediate (1) in the multiple patterning lithographic formation of a mask (2) for patterning a target layer (3) during the fabrication of a semiconductor device, comprising:
a) Providing the target layer (3), then
b) Forming mandrels (4) on the target layer (3) using EUV lithography, said mandrels (4) being separated by gaps (5), wherein the pitch (7) between the mandrels (4) is less than 40 nm, then
c) Conformally depositing a spacer material (6) on all exposed surfaces of the mandrels (4) and on exposed top surfaces of the target layer (3) present in the gaps (5), thereby partly narrowing the gaps (5), and then
d) Performing a directional etch of the spacer material (6) so as to expose a top surface (8) of the mandrels (4) and a top surface of the target layer (3) present in the gaps (5),
wherein the spacer material (6) has a resistivity lower than 104 Ω·cm at 20° C.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the spacer material (6) has a resistivity lower than 1 Ω·cm, preferably lower than 1 mΩ·cm at 20° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the spacer material (6) is a ceramic material.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the ceramic material is a nitride.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the nitride is selected from TiN, TaN, ZrN, and Cu3N.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the spacer material (6) is TiN.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the pitch (7) between the mandrels (4) is less than 25 nm, preferably less than 20 nm, more preferably less than 18 nm.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the directional etch comprises contacting the spacer material (6) with an ionized gas.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the directional etch comprises a vertical bombardment of the spacer material (6) with ions.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the vertical bombardment is followed by a wet etch.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the vertical bombardment is part of a vertical reactive ion etching process.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the ion energies in the reactive ion etching process are from 20 to 50 eV.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the target layer (3) is a hard mask layer (3).

### Claim 14 (depends on 1)

The method according to claim 1, performed during the Back-End-of-Line stage of the semiconductor device fabrication.

### Claim 15 (depends on 1)

The method according to claim 1, wherein step b) of forming the mandrels (4) on the target layer (3) comprises:
b1) Forming over the target layer (3) a mandrel material layer;
b2) Forming a layer of EUV-sensitive resist over the mandrel material layer;
b3) Exposing the EUV-sensitive resist to EUV light through a mask, said mask containing a pattern designed to achieve a pitch of less than 40 nm between the mandrels after step b5;
b4) Developing the exposed EUV-sensitive resist, thereby forming a resist mask having a pattern;
b5) Etching the mandrel material layer using the resist mask as an etching mask, thereby transferring the pattern into the mandrel material layer; and
b6) Removing the resist mask.

### Claim 16 (depends on 1)

The method according to claim 1, wherein step d is performed so as to also expose a top surface of the target layer.

### Claim 17 (depends on 1)

The method according to claim 1, followed by the following steps:
e) Filling the narrowed gaps (5) with a filling material (9) so that the top surface (8) of the spacer is exposed;
f) Removing the spacer material (6), thereby leaving on the layer a mask (2) formed by the combination of the mandrels (4) and of the filling material (9); and
g) Patterning the target layer (3) by using the mask (2).

### Claim 18

An intermediate (1) in the multiple patterning lithographic formation of a mask (2) for patterning a target layer (3) during the fabrication of a semiconductor device, comprising:
a) a target layer (3);
b) mandrels (4) on the target layer (3), wherein the pitch (7) between the mandrels (4) is less than 40 nm; and
c) spacers (6) on side walls of the mandrels (4),
wherein spacers (6) on neighboring mandrels (4) are separated by a gap (5),
wherein the top of the mandrels (4) is exposed, and
wherein the spacer material (6) has a resistivity lower than 104 Ω·cm at 20° C.