# US 2025/0155796 A1 · Optical member and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0155796 A1
- Document ID: US20250155796A1
- Status: Published application
- Kind: A1
- Application number: 18/833,406
- Filed: 2022-11-22
- Published: 2025-05-15
- Earliest claimed: 2022-02-04
- Assignees: Nippon Light Metal Company, Ltd.
- Applicants: Nippon Light Metal Company, Ltd.
- Inventors: Takeshi OSHIMA; Norihito SUZUKI
- Web page: https://patentgrep.com/patent/US20250155796A1

## CPC

- C23C 18/1241: {Metallic substrates}
- G03F 1/64: characterised by the frames, e.g. structure or material, including bonding means therefor
- C23C 18/12: characterised by the deposition of inorganic material other than metallic material
- C23C 18/1216: {Metal oxides (C23C18/1212 takes precedence)}
- C23C 18/1254: {Sol or sol-gel processing}
- G03F 7/70916: {Pollution mitigation, i.e. mitigating effect of contamination or debris, e.g. foil traps}
- G03F 7/70983: {Optical system protection, e.g. pellicles or removable covers for protection of mask}
- G03F 1/84: Inspecting
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A lightweight optical member can be manufactured at relatively low cost, the optical member having minimal distortion due to temperature increase and having excellent low dust generation and low outgassing properties. A pellicle frame is characterized by having a base material composed of titanium or a titanium alloy and a TiO2 coating layer formed on the surface of the base material. The TiO2 coating layer preferably contains nitrogen.

## Claims

### Claim 1

An optical member, which comprises:
a base material made of titanium or a titanium alloy, and
a TiO2 coating layer formed on the surface of the base material.

### Claim 2 (depends on 1)

The optical member according to claim 1, wherein the TiO2 coating layer contains nitrogen.

### Claim 3 (depends on 1)

The optical member according to claim 1, wherein
a through hole is present in the base material, and
the TiO2 coating layer is also formed on the inner surface of the through hole.

### Claim 4 (depends on 1)

The optical member according to claim 1, wherein an amount of hydrogen gas generated by irradiation with an extreme ultraviolet ray is 1.2 times or less an amount of hydrogen gas generated when the base material is irradiated with the extreme ultraviolet ray under the same conditions.

### Claim 5 (depends on 1)

The optical member according to claim 1, wherein, when the optical member is immersed in 3 L of pure water and irradiated with an ultrasonic wave for 1 minute, the number of particles having a particle size of 1 to 15 μm present in 50 ml of the pure water is 600 particles/68 cm2 or less.

### Claim 6 (depends on 1)

The optical member according to claim 1, wherein, when the optical member is immersed in 3 L of pure water and irradiated with an ultrasonic wave for 1 minute, the number of particles having a particle size of 0.5 to 1 μm present in 50 ml of the pure water is 2000 particles/68 cm2 or less.

### Claim 7

A method for producing an optical member, comprising:
a step for preparing a base material for an optical member, in which the base material made of titanium or a titanium alloy is processed into the shape of the base material for the optical member; and
a coating step for forming a TiO2 coating layer on the surface of the base material for the optical member by a sol-gel method,
wherein a nitrogen-containing salt catalyst is used in the coating step.

### Claim 8 (depends on 7)

The method for producing an optical member according to claim 7, wherein
a through hole is formed in the base material for the optical member in the step for preparing the base material for the optical member, and
the TiO2 coating layer is also formed on the inner surface of the through hole in the coating step.