# US 2025/0155341 A1 · Crack sensor, preparation method therefor, and application thereof in micro-force measurement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0155341 A1
- Document ID: US20250155341A1
- Status: Published application
- Kind: A1
- Application number: 19/021,368
- Filed: 2025-01-15
- Published: 2025-05-15
- Earliest claimed: 2022-07-15
- Assignees: Qilu University of Technology (Shandong Academy of Sciences)
- Applicants: Qilu University of Technology (Shandong Academy of Sciences)
- Inventors: Li WANG; Xingyuan XU; Jun CHEN; Weiguang SU; Anqing LI; Zhaoqiang CHEN; Chonghai XU
- Web page: https://patentgrep.com/patent/US20250155341A1

## CPC

- G01N 3/02: Details
- G01N 3/08: by applying steady tensile or compressive forces (G01N3/28 takes precedence)
- G01N 3/62: Manufacturing, calibrating, or repairing devices used in investigations covered by the preceding subgroups
- G01N 33/4833: {of solid biological material, e.g. tissue samples, cell cultures (tissue in vivo A61B5/00; cell suspensions G01N33/48735)}
- G01N 2203/0005: Repeated or cyclic
- G01N 2203/0019: Compressive
- G01N 2203/0062: Crack or flaws
- G01N 2203/0282: Two dimensional, e.g. tapes, webs, sheets, strips, disks or membranes
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A crack sensor, comprising a flexible film, wherein a first side of the flexible film is provided with a plurality of linear protrusions, and an opposite second side of the flexible film is configured with a linear structure; the linear structure comprises, in order from bottom to top, a silver layer, a chromium layer, and a CNT-PDMS layer, wherein the CNT-PDMS layer is composed of polydimethylsiloxane doped with carbon nanotubes; the silver layer is configured with a crack structure, the crack structure being a crack that changes in response to the deformation of the silver layer. The crack sensor effectively resists crack propagation, significantly improving the stability of the crack sensor while also exhibiting high sensitivity. Further provided is a preparation method for the crack sensor.

## Claims

### Claim 1

A crack sensor, comprising a flexible film, wherein a first side of the flexible film is provided with a plurality of linear protrusions, and an opposite second side of the flexible film is configured with a linear structure; the linear structure comprises, in order from bottom to top, a silver layer, a chromium layer, and a CNT-PDMS layer, wherein the CNT-PDMS layer is composed of polydimethylsiloxane (PDMS) doped with carbon nanotubes (CNT); the silver layer is configured with a crack structure, the crack structure being a crack that changes in response to the deformation of the silver layer;
wherein the flexible film is a polydimethylsiloxane (PDMS) film; the CNT-PDMS layer has a thickness of 5-20 μm; and
the CNT-PDMS layer contains carbon nanotubes in an amount of 0.01-5 wt %.

### Claim 2 (depends on 1)

The crack sensor according to claim 1, wherein the polydimethylsiloxane film has a thickness of 5-20 μm.

### Claim 3 (depends on 1)

The crack sensor according to claim 1, wherein the amount of carbon nanotubes is 2-4 wt %.

### Claim 4 (depends on 3)

The crack sensor according to claim 3, wherein the amount of carbon nanotubes is 2.5-3.5 wt %.

### Claim 5 (depends on 1)

The crack sensor according to claim 1, wherein the silver layer has a thickness of 90-110 nm.

### Claim 6 (depends on 1)

The crack sensor according to claim 1, wherein the chromium layer has a thickness of 2-10 nm.

### Claim 7 (depends on 1)

The crack sensor according to claim 1, wherein the CNT-PDMS layer is connected to an electrode.

### Claim 8 (depends on 1)

The crack sensor according to claim 1, wherein the linear structure is U-shaped.

### Claim 9 (depends on 1)

A method for preparing the crack sensor according to claim 1, comprising: coating a photoresist layer on a surface of a substrate; etching a plurality of microchannels on a surface of the photoresist layer; coating a layer of polydimethylsiloxane (PDMS) on the same surface, and curing to obtain a PDMS layer, wherein the PDMS layer has a first face with a plurality of linear protrusions and a second face that is smooth; covering the second face of the PDMS layer with a template having linear through-holes; successively forming a silver layer, a chromium layer, and a CNT-PDMS layer on a side of the template; removing the template to obtain a structure; and pre-stretching the structure to obtain the crack sensor.

### Claim 10 (depends on 9)

The method according to claim 9, wherein the substrate is glass, and before coating the photoresist layer, the substrate is treated with O2 plasma.

### Claim 11 (depends on 9)

The method according to claim 9, wherein the silver layer and the chromium layer are formed by vacuum evaporation.

### Claim 12 (depends on 9)

The method according to claim 9, wherein the CNT-PDMS layer is formed on a surface of the chromium layer by screen printing.

### Claim 13 (depends on 9)

The method according to claim 9, wherein the pre-stretching is conducted under a strain of 1.5-2.5%.

### Claim 14 (depends on 1)

A crack sensing device, comprising the crack sensor according to claim 1, a support, and a cell culture component, wherein the crack sensor is positioned between the support and the cell culture component, the support is provided with a groove or a through-hole, the crack sensor covers the groove or the through-hole, and a portion or the entirety of the linear structure of the crack sensor is located within the groove or the through-hole.

### Claim 15 (depends on 14)

The crack sensing device according to claim 14, wherein further comprising a glass substrate, wherein the support is bonded to the glass substrate.

### Claim 16 (depends on 15)

The crack sensing device according to claim 15, wherein the glass substrate is treated with O2 plasma.

### Claim 17 (depends on 14)

The crack sensing device according to claim 14, wherein the support is treated with O2 plasma.