# US 2025/0154690 A1 · Manufacturing method of photochromic thermal insulation fiber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154690 A1
- Document ID: US20250154690A1
- Status: Published application
- Kind: A1
- Application number: 19/021,466
- Filed: 2025-01-15
- Published: 2025-05-15
- Earliest claimed: 2021-05-28
- Assignees: Taiwan Textile Research Institute
- Applicants: Taiwan Textile Research Institute
- Inventors: Jo-Cheng CHIANG; Chao-Huei LIU
- Web page: https://patentgrep.com/patent/US20250154690A1

## CPC

- D01D 5/34: Core-skin structure; Spinnerette packs therefor
- D01F 1/06: Dyes
- C08J 3/22: using masterbatch techniques
- C08K 3/013: Fillers, pigments or reinforcing additives
- C08K 3/22: of metals
- C08K 5/0041: {Optical brightening agents, organic pigments}
- C08K 5/005: {Stabilisers against oxidation, heat, light, ozone}
- C08K 5/3492: Triazines
- C08L 23/12: Polypropene
- D01D 1/04: Melting filament-forming substances
- D01D 5/10: using organic materials
- D01F 1/10: Other agents for modifying properties
- D01F 1/106: {Radiation shielding agents, e.g. absorbing, reflecting agents}
- D01F 8/06: with at least one polyolefin as constituent
- D01F 8/12: with at least one polyamide as constituent
- C08K 2003/2241: {Titanium dioxide}
- D10B 2321/022: polypropylene
- D10B 2401/20: optical
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES

## Abstract

This disclosure provides a manufacturing method of a photochromic thermal insulation fiber, which includes preparing a photochromic masterbatch by including mixing 5 parts by weight of a photochromic dye and 95 parts by weight of polypropylene, preparing a near-infrared reflecting masterbatch by including mixing 15 parts by weight of a near-infrared reflecting dye and 85 parts by weight of nylon, preparing a first mixture by including mixing 10 parts by weight of the photochromic masterbatch and 75 parts by weight to 115 parts by weight of polypropylene, preparing a second mixture by including mixing 10 parts by weight of the near-infrared reflecting masterbatch and 65 parts by weight to 140 parts by weight of nylon, and performing a core-sheath melt spinning process with the first mixture and the second mixture to form a core layer and a sheath layer of the photochromic thermal insulation fiber.

## Claims

### Claim 1

A manufacturing method of a photochromic thermal insulation fiber, comprising:
preparing a photochromic masterbatch, comprising uniformly mixing 5 parts by weight of a photochromic dye and 95 parts by weight of polypropylene, and performing a powder refining process, a powder dispersion process, and a kneading and granulation process to obtain the photochromic masterbatch;
preparing a near-infrared reflecting masterbatch, comprising uniformly mixing 15 parts by weight of a near-infrared reflecting dye and 85 parts by weight of nylon, and performing a powder refining process, a powder dispersion process, and a kneading and granulation process to obtain the near-infrared reflecting masterbatch;
preparing a first mixture, comprising mixing 10 parts by weight of the photochromic masterbatch and 75 parts by weight to 115 parts by weight of polypropylene to obtain the first mixture;
preparing a second mixture, comprising mixing 10 parts by weight of the near-infrared reflecting masterbatch and 65 parts by weight to 140 parts by weight of nylon to obtain the second mixture; and
performing a core-sheath melt spinning process with the first mixture and the second mixture to form a core layer and a sheath layer of the photochromic thermal insulation fiber, wherein the first mixture forms the core layer, and wherein the second mixture forms the sheath layer.

### Claim 2 (depends on 1)

The manufacturing method of claim 1, further comprising:
preparing an ultraviolet absorber masterbatch, comprising uniformly mixing 10 parts by weight of an ultraviolet absorber and 90 parts by weight of nylon, and performing a powder refining process, a powder dispersion process, and a kneading and granulation process to obtain the ultraviolet absorber masterbatch; and
when preparing the second mixture, adding 1.5 parts by weight to 3 parts by weight of the ultraviolet absorber masterbatch to obtain the second mixture.

### Claim 3 (depends on 1)

The manufacturing method of claim 1, further comprising:
preparing a titanium dioxide masterbatch, comprising uniformly mixing 30 parts by weight of titanium dioxide and 70 parts by weight of nylon, and performing a powder refining process, a powder dispersion process, and a kneading and granulation process to obtain the titanium dioxide masterbatch; and
when preparing the second mixture, adding 2.5 parts by weight to 5 parts by weight of the titanium dioxide masterbatch to obtain the second mixture.

### Claim 4 (depends on 1)

The manufacturing method of claim 1, wherein preparing the photochromic masterbatch further comprises uniformly mixing 0.1 parts by weight to 0.3 parts by weight of a first dispersant with the photochromic dye and the polypropylene to obtain the photochromic masterbatch.

### Claim 5 (depends on 4)

The manufacturing method of claim 4, wherein preparing the near-infrared reflecting masterbatch further comprises uniformly mixing 0.1 parts by weight to 0.3 parts by weight of a second dispersant with the near-infrared reflecting dye and the nylon to obtain the near-infrared reflecting masterbatch, and the second dispersant is different from the first dispersant.

### Claim 6 (depends on 1)

The manufacturing method of claim 1, wherein performing the core-sheath melt spinning process comprises forming 40 parts by weight to 60 parts by weight of the core layer with the first mixture and forming 40 parts by weight to 60 parts by weight of the sheath layer with the second mixture.

### Claim 7 (depends on 1)

The manufacturing method of claim 1, wherein the photochromic dye and the polypropylene are ground to 300 nm to 400 nm of particle sizes after the powder refining process of preparing the photochromic masterbatch.

### Claim 8 (depends on 1)

The manufacturing method of claim 1, wherein a kneading temperature of the kneading and granulation process of preparing the near-infrared reflecting masterbatch is higher than a kneading temperature of the kneading and granulation process of preparing the photochromic masterbatch.

### Claim 9 (depends on 1)

The manufacturing method of claim 1, wherein a spinning temperature of the core-sheath melt spinning process is higher than a kneading temperature of the kneading and granulation process of preparing the photochromic masterbatch.

### Claim 10 (depends on 1)

The manufacturing method of claim 1, further comprising:
drying the first mixture before the core-sheath melt spinning process, wherein a drying temperature for the first mixture is lower than a kneading temperature of the kneading and granulation process of preparing the photochromic masterbatch; and
drying the second mixture before the core-sheath melt spinning process, wherein a drying temperature for the second mixture is lower than a kneading temperature of the kneading and granulation process of preparing the near-infrared reflecting masterbatch.