# US 2025/0154657 A1 · Plasma-resistant two-layer coating film structure and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154657 A1
- Document ID: US20250154657A1
- Status: Published application
- Kind: A1
- Application number: 18/707,027
- Filed: 2023-03-20
- Published: 2025-05-15
- Earliest claimed: 2022-03-24
- Assignees: Femvix Corp.
- Applicants: Femvix Corp.
- Inventors: Ok Ryul KIM; Ok Min KIM
- Web page: https://patentgrep.com/patent/US20250154657A1

## CPC

- C23C 28/042: {including a refractory ceramic layer, e.g. refractory metal oxides, ZrO2, rare earth oxides}
- C23C 4/11: Oxides
- C23C 16/44: characterised by the method of coating (C23C16/04 takes precedence)
- C23C 24/04: Impact or kinetic deposition of particles
- C23C 28/04: only coatings of inorganic non-metallic material
- H01J 37/32: Gas-filled discharge tubes (heating by discharge H05B)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Provided is a plasma-resistant two-layer coating film structure including: a ceramic or metal substrate having pits on a surface thereof; a first coating layer which is a ceramic coating layer formed without cracks on the surface of the substrate by a spray coating method other than thermal spray, the layer being coated to fill the pits on the surface of the substrate, fine pits accompanying ceramic particle bonding being formed on the surface, and the layer including ceramic polycrystalline bodies having a crystallite size of less than 300 nm; and a second coating layer which is a plasma resistant ceramic film, the layer being formed to have a surface roughness (Ra) of 0.2 μm or less without a separate grinding process and coated to cover the fine pits to form a surface in which positions that may serve as starting points of plasma etching are minimized.

## Claims

### Claim 1

A plasma-resistant two-layer coating film structure comprising:
a ceramic or metal substrate having pits on a surface thereof;
a first coating layer which is a ceramic coating layer formed without cracks on the surface of the substrate by a spray coating method other than thermal spray, the layer being coated to fill the pits on the surface of the substrate, fine pits accompanying ceramic particle bonding being formed on the surface, and the layer including ceramic polycrystalline bodies having a crystallite size of less than 300 nm; and
a second coating layer which is a plasma resistant ceramic film coated by one method of chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD), the layer being formed to have a surface roughness (Ra) of 0.2 μm or less without a separate grinding process and coated to cover the fine pits to form a surface in which positions that may serve as starting points of plasma etching are minimized, and the layer being crystalline or in a mixed state where both a crystalline phase and an amorphous phase are present.

### Claim 2 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the substrate is a semiconductor process component.

### Claim 3 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the first coating layer is formed of one or more of Al2O3, Y2O3, Tm2O3, Gd2O3, Dy2O3, Er2O3, and Sm2O3.

### Claim 4 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the first coating layer is free of cracks.

### Claim 5 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the first coating layer includes pores in an amount of 1% by volume or less.

### Claim 6 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the first coating layer has a thickness of 20 μm or less.

### Claim 7 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the second coating layer is a ceramic film including yttrium (Y) or a ceramic film including a metal oxide.

### Claim 8 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the second coating layer is formed of one or more of Y2O3, YF3, yttrium oxyfluoride (YOF), yttrium aluminum (YAG) yttrium aluminum perovskite (YAP), and yttrium aluminum monoclinic (YAM).

### Claim 9 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the second coating layer is formed of one or more of Tm2O3, Gd2O3, Dy2O3, Er2O3, and Sm2O3.

### Claim 10 (depends on 1)

The plasma-resistant two-layer coating film structure according to claim 1, wherein the second coating layer is free of pores.

### Claim 11 (depends on 10)

The plasma-resistant two-layer coating film structure according to claim 10, wherein the second coating layer has a thickness of 15 μm or less.

### Claim 12 (depends on 10)

The plasma-resistant two-layer coating film structure according to claim 10, wherein the surface hardness (Vickers hardness, Hv) of the second coating layer is Hv 500 to Hv 1,500.

### Claim 13

A manufacturing method of a plasma-resistant two-layer coating film structure, comprising:
(a) a step of forming a first coating layer by spraying ceramic powder by a spray coating method other than thermal spray onto a ceramic or metal substrate having pits on a surface thereof so that the layer is coated to fill the pits on the surface of the substrate, fine pits accompanying ceramic particle bonding being formed on the surface and the layer including ceramic polycrystalline bodies having a crystallite size of less than 300 nm; and
(b) a step of forming a second coating layer which is coated by one method of chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD) to cover the fine pits to form a surface in which positions that may serve as starting points of plasma etching are minimized, the layer being crystalline or in a mixed state where both a crystalline phase and an amorphous phase are present and made of a ceramic film including yttrium (Y) or a metal oxide and having surface roughness (Ra) of 0.2 μm or less.

### Claim 14 (depends on 13)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 13, further comprising Step (a-0) of grinding the surface of the substrate before the Step (a).

### Claim 15 (depends on 14)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 14, wherein in the Step (a-0), the surface of the substrate is ground to have a surface roughness (Ra) of 0.2 μm or less.

### Claim 16 (depends on 13)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 13, further comprising Step (a-1) of grinding the surface of the first coating layer between the Step (a) and the Step (b).

### Claim 17 (depends on 16)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 16, wherein in the Step (a-1), the surface of the first coating layer is ground to have a surface roughness (Ra) of 0.2 μm or less.

### Claim 18 (depends on 17)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 17, further comprising:
Step (a-2) of spraying ceramic powder by a spray coating method other than thermal spray to increase the thickness of the first coating layer; and
Step (a-3) of grinding the surface of the first coating layer with the increased thickness, following the Step (a-1).

### Claim 19 (depends on 18)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 18, wherein in the Step (a-3), the surface of the first coating layer with the increased thickness is ground to have a surface roughness (Ra) of 0.2 μm or less.

### Claim 20 (depends on 13)

The manufacturing method of a plasma-resistant two-layer coating film structure according to claim 13, further comprising:
Step (c) of heat-treating a two-layer coating film structure, following the Step (b).