# US 2025/0154636 A1 · Method for manufacturing plated steel having excellent processability and corrosion resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154636 A1
- Document ID: US20250154636A1
- Status: Published application
- Kind: A1
- Application number: 18/572,431
- Filed: 2022-12-15
- Published: 2025-05-15
- Earliest claimed: 2022-04-29
- Assignees: Hyundai Steel Company
- Applicants: Hyundai Steel Company
- Inventors: Seon Jin Kim; Jae Min Lee
- Web page: https://patentgrep.com/patent/US20250154636A1

## CPC

- C23C 2/26: After-treatment (C23C2/14 takes precedence)
- C23C 2/29: {Cooling or quenching}
- C22C 18/00: Alloys based on zinc
- C22C 18/04: with aluminium as the next major constituent
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/20: Strips; Plates
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/40: Plates; Strips
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a method of manufacturing a plated steel material having excellent workability and corrosion resistance according to an exemplary embodiment of the present disclosure and the method includes steps of immersing a base steel in a hot-dip alloy plating bath; and forming a hot-dip alloy-plated layer on the base steel by drawing the immersed base steel from the hot-dip alloy plating bath and performing a cooling process. A first average cooling rate in the cooling process varies depending on a difference between a first temperature that is a temperature of the hot-dip alloy plating bath and a second temperature that is a solidification start temperature of a MgZn2 phase constituting the hot-dip alloy-plated layer.

## Claims

### Claim 1

A method of manufacturing a plated steel material having excellent workability and corrosion resistance, the method comprising:
immersing a base steel in a hot-dip alloy plating bath; and
forming a hot-dip alloy-plated layer on the base steel by drawing the immersed base steel from the hot-dip alloy plating bath and performing a cooling process,
wherein a first average cooling rate in the cooling process varies depending on a difference between a first temperature that is a temperature of the hot-dip alloy plating bath and a second temperature that is a solidification start temperature of a MgZn2 phase continuing the hot-dip alloy-plated layer.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein when the difference between the first temperature and the second temperature is less than 50° C., the first average cooling rate is 10 to 20° C./s,
wherein when the difference between the first temperature and the second temperature is 50° C. or higher and less than 100° C., the first average cooling rate is 15 to 35° C./s, and
wherein when the difference between the first temperature and the second temperature is 100° C. or higher, the first average cooling rate is 20 to 50° C./s.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the first average cooling rate is an average cooling rate from a time point at which the immersed base steel is drawn from the hot-dip alloy plating bath to a time point at which the MgZn2 phase starts to solidify.

### Claim 4 (depends on 1)

The method according to claim 1, wherein a second average cooling rate in the cooling process from a time point at which the MgZn2 phase starts to solidify to a time point at which the solidification is completed satisfies a relationship of Formula 1 below.
0.0114×T−0.2841≤second average cooling rate≤0.025×T+10 (T: solidification start temperature of MgZn2 phase). <Formula 1>

### Claim 5 (depends on 1)

The method according to claim 1, wherein the hot-dip alloy plating bath is a Zn plating bath comprising, by wt. %, 6 to 23% of Al, 3 to 7% of Mg, and inevitable impurities.

### Claim 6 (depends on 1)

The method according to claim 1, wherein an area fraction of a MgZn2 phase here a ratio of an average minor axis length (a) to an average major axis length (b) is 0.5 or less in the entire MgZn2 phase on a surface of the hot-dip alloy-plated layer formed on the base steel is 70% or less.