# US 2025/0154620 A1 · Steel plate for pressure vessel with excellent cryogenic toughness and excellent ductility and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154620 A1
- Document ID: US20250154620A1
- Status: Published application
- Kind: A1
- Application number: 19/024,595
- Filed: 2025-01-16
- Published: 2025-05-15
- Earliest claimed: 2018-10-26
- Assignees: Posco
- Applicants: Posco Co., Ltd
- Inventors: Soon-Taik Hong
- Web page: https://patentgrep.com/patent/US20250154620A1

## CPC

- C21D 9/46: for sheet metals
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/185: {from an intercritical temperature}
- C21D 1/26: Methods of annealing
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0263: {following hot rolling}
- C22C 38/00: Ferrous alloys, e.g. steel alloys (cast-iron alloys C22C37/00)
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/08: containing nickel {(C22C38/105 takes precedence)}
- C21D 1/25: Hardening, combined with annealing between 300 degrees Celsius and 600 degrees Celsius, i.e. heat refining ("Vergüten")
- C21D 2211/002: Bainite
- C21D 2211/008: Martensite
- F17C 2203/0639: Steels
- F17C 2209/2181: Metal working processes, e.g. deep drawing, stamping or cutting
- Y02P 10/20: Recycling
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F17C: VESSELS FOR CONTAINING OR STORING COMPRESSED, LIQUEFIED OR SOLIDIFIED GASES; FIXED-CAPACITY GAS-HOLDERS; FILLING VESSELS WITH, OR DISCHARGING FROM VESSELS, COMPRESSED, LIQUEFIED, OR SOLIDIFIED GASES (storing fluids in natural or artificial cavities or chambers in the earth B65G5/00; construction or assembling of bulk storage containers employing civil-engineering techniques E04H7/00; variable-capacity gas-holders F17B; liquefaction or refrigeration machines, plants, or systems F25)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided are a steel plate for a pressure vessel with excellent cryogenic toughness and elongation resistance, and a manufacturing method thereof. The steel plate for a pressure vessel of the present invention comprises, in weight %, 0.05 to 0.15% of C; 0.20 to 0.40% of Si; 0.3 to 0.6% of Mn; 0.001 to 0.05% of Al; 0.012% or less of P; 0.015% or less of S; 4.0 to 5.0% of Ni; 0.001 to 0.10% of In; and the balance being Fe and unavoidable impurities, wherein a steel microstructure consists of 15 to 80 area % of tempered bainite and the balance being tempered martensite.

## Claims

### Claim 1

A method of manufacturing a steel plate for a low temperature pressure vessel having excellent cryogenic toughness and ductility, the method comprising:
reheating a steel slab at 1050 to 1250° C., the steel slab containing, in weight %, 0.05 to 0.15% of C, 0.20 to 0.40% of Si, 0.3 to 0.6% of Mn, 0.001 to 0.05% of Al, 0.012% or less of P, 0.015% or less of S, 4.0 to 5.0% of Ni, 0.001 to 0.10% of In, a balance of Fe, and unavoidable impurities;
hot rolling the reheated steel plate at a reduction ratio of 5 to 30% per pass, and terminating rolling at a temperature of 800° C. or higher;
primary cooling the hot-rolled steel plate at a cooling rate of 2.5 to 50° C./sec within 30 seconds after hot rolling;
performing an intermediate heat treatment on the cooled steel plate for {2.4×t+(10−30)} minutes at a temperature of 690 to 760° C., where t is a thickness (mm) of a steel plate, and then, secondary cooling the steel plate at a cooling rate of 2.5 to 50° C./sec; and
tempering the secondary cooled steel plate for {2.4×t+(10−30)} minutes at a temperature of 600 to 670° C., where t is a thickness (mm) of a steel plate.

### Claim 2 (depends on 1)

The method of manufacturing a steel plate for a low temperature pressure vessel having excellent cryogenic toughness and ductility, of claim 1, wherein a steel microstructure obtained by the tempering is comprised of 15 to 80 area % of tempered bainite and a remainder of tempered martensite.

### Claim 3 (depends on 1)

The method of manufacturing a steel plate for a low temperature pressure vessel having excellent cryogenic toughness and ductility, of claim 1. wherein the In is contained in an amount of 0.05 to 0.08%.