# US 2025/0154394 A1 · One-component toughened epoxy adhesives with improved humidity resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154394 A1
- Document ID: US20250154394A1
- Status: Published application
- Kind: A1
- Application number: 19/022,532
- Filed: 2025-01-15
- Published: 2025-05-15
- Earliest claimed: 2019-06-18
- Assignees: Ddp Specialty Electronic Materials US, LLC
- Applicants: Ddp Specialty Electronic Materials US, LLC
- Inventors: ANDREAS LUTZ; DANIEL SCHNEIDER; JEANNINE FLUECKIGER; FELIX KOCH
- Web page: https://patentgrep.com/patent/US20250154394A1

## CPC

- C09J 163/00: Adhesives based on epoxy resins; Adhesives based on derivatives of epoxy resins
- C08G 18/242: {organometallic compounds containing tin-carbon bonds}
- C08G 18/2825: {having at least 6 carbon atoms}
- C08G 18/3215: {containing aromatic groups or benzoquinone groups}
- C08G 18/4854: {Polyethers containing oxyalkylene groups having four carbon atoms in the alkylene group}
- C08G 18/69: Polymers of conjugated dienes {(hydrogenated polymers of conjugated dienes C08G18/6208)}
- C08G 18/698: {Mixtures with compounds of group C08G18/40}
- C08G 18/73: acyclic
- C08G 59/686: {containing nitrogen}
- C08L 63/00: Compositions of epoxy resins; Compositions of derivatives of epoxy resins
- C08L 75/08: from polyethers
- C08L 2205/03: containing three or more polymers in a blend
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A toughened one component epoxy adhesive composition demonstrating improved resistance to humidity and the method of making thereof.

## Claims

### Claim 1

A one-part structural adhesive comprising:
A) a blocked PU-polymer toughener compound;
B) an epoxy resin component comprising a solid epoxy resin, a liquid epoxy resin, or mixture thereof;
C) a curing agent;
D) a urea compound present in an amount of about 0.1 wt. %, based on the total weight of the adhesive; and
E) optionally a filler,
wherein the blocked PU-polymer toughener (A) is a reaction product of a reaction mixture comprising:
i) a polyether,
ii) a hydroxyl-terminated polybutadiene,
iii) a polyisocyanate,
iv) a chain extender, and
v) a capping group.

### Claim 2 (depends on 1)

The one-part structural adhesive of claim 1 wherein the polyether (A) (i) is a polytetrahydrofuran-diol polymer.

### Claim 3 (depends on 1)

The one-part structural adhesive of claim 1 wherein the polyisocyanate (A) (iii) is 1,6-hexamethylene diisocyanate.

### Claim 4 (depends on 1)

The one-part structural adhesive of claim 1 wherein the capping group (A) (iv) is cashew nut shell liquid oil.

### Claim 5 (depends on 1)

The one-part structural adhesive of claim 1 wherein the urea compound (D) is a phenyl dimethyl urea.

### Claim 6 (depends on 1)

The one-part structural adhesive of claim 1 wherein the filler (E) is one or more of fumed silica, calcium carbonate, calcium oxide, wollastonite, talc, glass beads, and hollow glass spheres.

### Claim 7 (depends on 1)

The one-part structural adhesive of claim 1 wherein:
A) 5 to 25 weight percent of the blocked PU-polymer toughener compound;
B) the epoxy resin component comprises 1 to 10 weight percent of a solid epoxy resin and 30 to 60 weight percent of a liquid epoxy resin;
C) 1 to 8 weight percent of the curing agent;
D) About 0.1 weight percent of the urea compound;
and
E) 0 to 30 weight percent of the filler,
wherein weight percents are based on the total weight of the one-part structural adhesive.

### Claim 8 (depends on 1)

The one-part structural adhesive of claim 1 wherein the blocked PU-polymer toughener (A) reaction mixture comprises:
i) 10 to 95 weight percent of the polyether,
ii) 2 to 60 weight percent of the hydroxyl-terminated polybutadiene,
iii) 2 to 40 weight percent the polyisocyanate,
iv) more than zero but no more than 20 weight percent chain extender,
and
v) 0.1 to 50 weight percent the capping group,
wherein weight percents are based on the total weight of the reaction mixture.