# US 2025/0154383 A1 · Water-based hot melt adhesive and nonwoven coated with the water-based hot melt adhesive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154383 A1
- Document ID: US20250154383A1
- Status: Published application
- Kind: A1
- Application number: 18/818,637
- Filed: 2024-08-29
- Published: 2025-05-15
- Earliest claimed: 2023-11-09
- Assignees: BenQ Materials Corporation
- Applicants: BenQ Materials Corporation
- Inventors: Ching-Huang CHEN; Kuo-Hsuan YU; Yen-Ling LIN
- Web page: https://patentgrep.com/patent/US20250154383A1

## CPC

- C09J 7/35: Heat-activated
- C09J 123/04: Homopolymers or copolymers of ethene
- C09J 123/06: Polyethylene
- C08L 2201/54: Aqueous solutions or dispersions
- C09J 2301/304: the adhesive being heat-activatable, i.e. not tacky at temperatures inferior to 30°C
- C09J 2301/408: additives as essential feature of the adhesive layer
- C09J 2400/263: in the substrate
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present disclosure is to provide a water-based hot melt adhesive for healthcare packaging. The water-based hot melt adhesive includes 100 weight parts of water-based polyolefin resin; 40 to 85 weight parts of wax particles; and 25 to 85 parts by weight of tackifier particles; wherein a total weight of the wax particles and the tackifier particles is from 45 wt % to 60 wt % of a total weight of the water-based hot melt adhesive. The coating layer coated by the water-based hot melt adhesive of the present disclosure on the healthcare packaging substrate has great gas-permeability, and satisfied seal strength and peelability after sealing with the periphery part of a flexible sheet or a blister container.

## Claims

### Claim 1

A water-based hot-melt adhesive, comprising: 100 weight parts of water-base polyolefin resin, 40 weight parts to 85 weight parts of wax particles, and 25 weight parts to 85 weight parts of tackifier particles, wherein a total amount of the wax particles and the tackifier particles is from 45 wt % to 60 wt % of a total weight of the water-based hot-melt adhesive.

### Claim 2 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein a particle size of each of the wax particles is from 3 μm to 20 μm.

### Claim 3 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein a particle size of each of the tackifier particles is from 3 μm to 35 μm.

### Claim 4 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein a weight ratio of the wax particles and the tackifier particles is from 0.6:1 to 3:1.

### Claim 5 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein the water-based hot-melt adhesive comprises: 100 weight parts of the water-base polyolefin resin, 45 weight parts to 80 weight parts of the wax particles, and 30 weight parts to 80 weight parts of the tackifier particles, wherein the total amount of the wax particles and the tackifier particles is from 48 wt % to 57 wt % of the total weight of the water-based hot-melt adhesive.

### Claim 6 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, further comprising water-based emulsion tackifier.

### Claim 7 (depends on 6)

The water-based hot-melt adhesive as claimed in claim 6, wherein the water-based emulsion tackifier is present in amount of from 10 weight parts to 60 weight parts.

### Claim 8 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein a glass transition temperature of the water-base polyolefin resin is less than 0° C. and a melting point of the water-base polyolefin resin is greater than 90° C., a glass transition temperature of the wax particles is less than 0° C. and a melting point of the wax particles is from 70° C. to 180° C., a glass transition temperature of the tackifier particles is greater than 0° C. and a melting point of the tackifier particles is from 90° C. to 160° C.

### Claim 9 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein a glass transition temperature of the water-based hot-melt adhesive is from −120° C. to −50° C.

### Claim 10 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein the water-base polyolefin resin is selected from the group consisting of water-based polyethylene resin, water-based polypropylene resin, water-based polybutylene resin, water-based oxidized polyethylene resin and combinations thereof.

### Claim 11 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein the wax particles is selected from the group consisting of Fischer-Tropsch synthetic wax particles, polypropylene wax particles, polyethylene wax particles, oxidized polyethylene wax particles, microcrystalline wax and combinations thereof.

### Claim 12 (depends on 1)

The water-based hot-melt adhesive as claimed in claim 1, wherein the tackifier particles is selected from the group consisting of C5 petroleum resin micropowders, C9 petroleum resin micropowders, C5/C9 copolymerized petroleum resin micropowders, hydrogenated C9 petroleum resin micropowders and combinations thereof.

### Claim 13 (depends on 6)

The water-based hot-melt adhesive as claimed in claim 6, wherein the water-based emulsion tackifier is selected from the group consisting of petroleum resin emulsion, rosin ester emulsion and derivatives thereof, terpene resin and modified resin derivatives thereof, thermoplastic phenol-formaldehyde resin emulsion, low-molecular polystyrene emulsion, vinyl acrylate copolymer emulsion and combinations thereof.

### Claim 14

A water-based hot-melt adhesive coated nonwoven fabric, comprising: a polyolefin spunbonded nonwoven fabric substrate and a water-based hot-melt adhesive coating formed on at least one side of the polyolefin spunbonded nonwoven fabric, wherein a water-based hot-melt adhesive for forming the water-based hot-melt adhesive coating comprises: 100 weight parts of water-base polyolefin resin, 40 weight parts to 85 weight parts of wax particles, and 25 weight parts to 85 weight parts of tackifier particles, wherein a total amount of the wax particles and the tackifier particles is from 45 wt % to 60 wt % of a total weight of the water-based hot-melt adhesive.

### Claim 15 (depends on 14)

The water-based hot-melt adhesive coated nonwoven fabric as claimed in claim 14, wherein a gas-permeability of the water-based hot-melt adhesive coated nonwoven fabric is less than 180 seconds and a seal strength thereof is more than 220 g/15 mm.

### Claim 16 (depends on 14)

The water-based hot-melt adhesive coated nonwoven fabric as claimed in claim 14, wherein a coating amount of the water-based hot-melt adhesive on the polyolefin spunbonded nonwoven fabric substrate is from 10 g/m2 to 20 g/m2.