# US 2025/0154313 A1 · Polymer, resin composition, article comprising the same, and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154313 A1
- Document ID: US20250154313A1
- Status: Published application
- Kind: A1
- Application number: 18/435,724
- Filed: 2024-02-07
- Published: 2025-05-15
- Earliest claimed: 2023-11-09
- Assignees: Elite Electronic Material (Kunshan) Co., Ltd.
- Applicants: Elite Electronic Material (Kunshan) Co., Ltd.
- Inventors: Yahui MA; Rongtao WANG; Diya LIU
- Web page: https://patentgrep.com/patent/US20250154313A1

## CPC

- C08G 61/02: Macromolecular compounds containing only carbon atoms in the main chain of the macromolecule, e.g. polyxylylenes
- C08J 5/24: Impregnating materials with prepolymers which can be polymerised in situ, e.g. manufacture of prepregs
- C08J 5/244: {using glass fibres}
- C08J 5/249: {characterised by the additives used in the prepolymer mixture}
- C08L 65/00: Compositions of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08L7/00 - C08L57/00, C08L61/00 take precedence); Compositions of derivatives of such polymers
- C08L 71/126: {modified by chemical after-treatment}
- C08J 2465/00: Characterised by the use of macromolecular compounds obtained by reactions forming a carbon-to-carbon link in the main chain (C08J2407/00 - C08J2457/00, C08J2461/00 take precedence); Derivatives of such polymers
- C08L 2203/16: used for films
- C08L 2203/20: use in electrical or conductive gadgets
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A polymer is disclosed, having a structure represented by Formula (1), wherein in Formula (1), X is adamantyl group, each of R1-R4 is independently hydrogen atom or C1-C3 alkyl group, and n is an integer of 2-50. A resin composition is also disclosed, comprising: (A) an unsaturated carbon-carbon double bond-containing polyphenylene ether resin, and (B) the above polymer. In addition, an article made from the above polymer or the above resin composition is also disclosed. The article comprises a prepreg, a resin film, a laminate or a printed circuit board and has improvements in one or more of the following properties: glass transition temperature, T300 thermal resistance, percent thermal expansion at Z-axis, dissipation factor, dissipation factor variation rate under moisture and heat, dissipation factor variation rate under heat and water absorption rate.

## Claims

### Claim 1

A polymer, having a structure represented by Formula (1):
wherein in Formula (1), X is adamantyl group, each of R1-R4 is independently hydrogen atom or C1-C3 alkyl group, and n is an integer of 2-50.

### Claim 2 (depends on 1)

The polymer of claim 1, wherein X is monoadamantyl group, diamantyl group or polyamantyl group.

### Claim 3 (depends on 1)

The polymer of claim 1, wherein the polymer represented by Formula (1) comprises a polymer represented by Formula (1-1), a polymer represented by Formula (1-2), a polymer represented by Formula (1-3) or a combination thereof:
wherein each of n1-n3 is independently an integer of 2-50.

### Claim 4 (depends on 1)

The polymer of claim 1, wherein the polymer has a number average molecular weight of 800-17000.

### Claim 5 (depends on 1)

A resin composition, comprising:
(A) an unsaturated carbon-carbon double bond-containing polyphenylene ether resin, and
(B) a polymer of claim 1.

### Claim 6 (depends on 5)

The resin composition of claim 5, wherein with respect to 100 parts by weight of the unsaturated carbon-carbon double bond-containing polyphenylene ether resin, the amount of the polymer is 10-80 parts by weight.

### Claim 7 (depends on 5)

The resin composition of claim 5, wherein with respect to 100 parts by weight of the unsaturated carbon-carbon double bond-containing polyphenylene ether resin, the amount of the polymer is 20-70 parts by weight.

### Claim 8 (depends on 5)

The resin composition of claim 5, wherein the unsaturated carbon-carbon double bond-containing polyphenylene ether resin comprises a (meth)acryloyl group-containing polyphenylene ether resin, a vinylbenzyl group-containing polyphenylene ether resin, a vinyl group-containing polyphenylene ether resin or a combination thereof.

### Claim 9 (depends on 5)

The resin composition of claim 5, wherein the resin composition further comprises an unsaturated carbon-carbon double bond-containing crosslinking agent, the unsaturated carbon-carbon double bond-containing crosslinking agent is bis(vinylphenyl)ethane, bis(vinylbenzyl)ether, divinylbenzene, divinylnaphthalene, divinylbiphenyl, triallyl isocyanurate, triallyl cyanurate, vinylbenzocyclobutene, trivinyl cyclohexane, diallyl bisphenol A, butadiene, decadiene, octadiene, two or more-functional acrylate or a combination thereof.

### Claim 10 (depends on 5)

The resin composition of claim 5, wherein the resin composition further comprises a polyolefin, an organic silicone resin, a benzoxazine resin, an epoxy resin, a polyester resin, a phenol resin, an amine curing agent, a polyamide, a polyimide, a styrene maleic anhydride, a maleimide resin other than the polymer represented by Formula (1), a cyanate ester resin, a maleimide triazine resin or a combination thereof.

### Claim 11 (depends on 5)

The resin composition of claim 5, wherein the resin composition further comprises a curing accelerator, a polymerization inhibitor, a flame retardant, an inorganic filler, a surfactant, a coloring agent, a toughening agent, a solvent or a combination thereof.

### Claim 12 (depends on 1)

An article, wherein the article is made from a polymer of claim 1, and the article comprises a prepreg, a resin film, a laminate or a printed circuit board.

### Claim 13 (depends on 12)

The article of claim 12, wherein the article has one or more of the following properties:
a glass transition temperature as measured by reference to IPC-TM-650 2.4.24.4 of greater than or equal to 269° C.;
a T300 thermal resistance as measured by reference to IPC-TM-650 2.4.24.1 of greater than 70 minutes;
a percent thermal expansion at Z-axis as measured by reference to IPC-TM-650 2.4.24.5 of less than or equal to 1.2%;
a dissipation factor at 10 GHz as measured by reference to JISC2565 of less than or equal to 0.0018;
a dissipation factor variation rate under moisture and heat of less than or equal to 8%, calculated by a dissipation factor of the article placed at room temperature and a dissipation factor of the article placed at a temperature of 85° C. and a relative humidity of 85% for 120 hours respectively at 10 GHz as measured by reference to JISC2565;
a dissipation factor variation rate under heat of less than or equal to 8%, calculated by a dissipation factor of the article placed at room temperature and a dissipation factor of the article placed at a temperature of 125° C. for 120 hours respectively at 10 GHz as measured by reference to JISC2565; and
a water absorption rate as measured by reference to IPC-TM-650 2.6.2.1 and IPC-TM-650 2.6.16.1 of less than or equal to 0.25%.

### Claim 14 (depends on 5)

An article, wherein the article is made from a resin composition of claim 5, and the article comprises a prepreg, a resin film, a laminate or a printed circuit board.

### Claim 15 (depends on 14)

The article of claim 14, wherein the article has a glass transition temperature as measured by reference to IPC-TM-650 2.4.24.4 of greater than or equal to 269° C.

### Claim 16 (depends on 14)

The article of claim 14, wherein the article has a T300 thermal resistance as measured by reference to IPC-TM-650 2.4.24.1 of greater than 70 minutes.

### Claim 17 (depends on 14)

The article of claim 14, wherein the article has a percent thermal expansion at Z-axis as measured by reference to IPC-TM-650 2.4.24.5 of less than or equal to 1.2%.

### Claim 18 (depends on 14)

The article of claim 14, wherein the article has a dissipation factor at 10 GHz as measured by reference to JISC2565 of less than or equal to 0.0018.

### Claim 19 (depends on 14)

The article of claim 14, wherein the article has a dissipation factor variation rate under moisture and heat of less than or equal to 8%, calculated by a dissipation factor of the article placed at room temperature and a dissipation factor of the article placed at a temperature of 85° C. and a relative humidity of 85% for 120 hours respectively at 10 GHz as measured by reference to JISC2565.

### Claim 20 (depends on 14)

The article of claim 14, wherein the article has a dissipation factor variation rate under heat of less than or equal to 8%, calculated by a dissipation factor of the article placed at room temperature and a dissipation factor of the article placed at a temperature of 125° C. for 120 hours respectively at 10 GHz as measured by reference to JISC2565.

### Claim 21 (depends on 14)

The article of claim 14, wherein the article has a water absorption rate as measured by reference to IPC-TM-650 2.6.2.1 and IPC-TM-650 2.6.16.1 of less than or equal to 0.25%.

### Claim 22 (depends on 1)

A preparation method of a polymer of claim 1, comprising: firstly, mixing and reacting an aniline and/or its derivative and a dihalogen-substituted adamantane in a reaction vessel to obtain an intermediate product; and then adding a maleic anhydride to the reaction vessel containing the intermediate product to obtain the polymer.
