# US 2025/0154302 A1 · Polyethylene composition and biaxially stretched film comprising the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154302 A1
- Document ID: US20250154302A1
- Status: Published application
- Kind: A1
- Application number: 18/837,811
- Filed: 2023-11-02
- Published: 2025-05-15
- Earliest claimed: 2022-11-02
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Inkyo KIM; Youngsuk YOU; Taejin KIM; Sanghwa LEE; Cheol Hun PARK; Eun Yeob CHOI
- Web page: https://patentgrep.com/patent/US20250154302A1

## CPC

- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- B29C 55/12: biaxial
- C08J 5/18: Manufacture of films or sheets
- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- C08F 2420/02: Cp or analog bridged to a non-Cp X anionic donor
- C08F 2420/07: Heteroatom-substituted Cp, i.e. Cp or analog where at least one of the substituent of the Cp or analog ring is or contains a heteroatom
- C08F 2420/10: Heteroatom-substituted bridge, i.e. Cp or analog where the bridge linking the two Cps or analogs is substituted by at least one group that contains a heteroatom
- C08F 2800/20: as weight or mass percentages
- C08J 2323/08: Copolymers of ethene (C08J2323/16 takes precedence)
- C08L 2203/16: used for films
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present disclosure relates to a polyethylene composition suitable for a biaxially stretched film, which has excellent stretching stability and high shrinkage resistance while maintaining excellent mechanical properties, productivity and printability, and a biaxially stretched film including the same.

## Claims

### Claim 1

A polyethylene composition comprising an ethylene-alpha olefin copolymer,
wherein a fraction of molecules eluting at 90° C. or more (TREF≥90° C.) derived from Temperature rising elution fractionation (TREF) analysis of the polyethylene compostions is 55% or more, and
a fraction of molecules eluting below 35° C. (TREF<35° C.) derived from TREF analysis of the polyethylene compostions is 3.0% or less.

### Claim 2 (depends on 1)

The polyethylene composition of claim 1,
wherein a density of the polyethylene compostions measured according to ASTM D 1505 is 0.925 g/cm3 or more and 0.945 g/cm3 or less, and
a melt index (MI) of the polyethylene compostions measured in a condition at 190° C., 2.16 kg according to ASTM D 1238 is 0.3 g/10 min or more and 1.5 g/10 min or less.

### Claim 3 (depends on 1)

The polyethylene composition of claim 1,
wherein a number average molecular weight (Mn) of the polyethylene compostions is 20,000 g/mol or more and 100,000 g/mol or less,
a weight average molecular weight (Mw) of the polyethylene compostions is 100,000 g/mol or more and 500,000 g/mol or less, and
Mw/Mn is 1.0 or more and 10.0 or less.

### Claim 4 (depends on 1)

The polyethylene composition of claim 1,
wherein a melting point (Tm) of the polyethylene compostions is 127° C. or more and 130° C. or less,
a crystallization temperature (Tc) of the polyethylene compostions is 111° C. or more and 115° C. or less, and
a crystallinity (Xc) of the polyethylene compostions is 50% or more and 70% or less.

### Claim 5 (depends on 1)

The polyethylene composition of claim 1,
wherein the polyethylene composition comprises
a first ethylene-alpha olefin copolymer having a density of 0.930 g/cm3 to 0.960 g/cm3 and a melt index (MI2.16, 190° C., 2.16 kg load) of 0.2 g/10 min to 2.0 g/10 min; and
a second ethylene-alpha olefin copolymer having a density of 0.870 g/cm3 to 0.920 g/cm3 and a melt index (MI2.16, 190° C., 2.16 kg load) of 3.0 g/10 min to 10.0 g/10 min;
wherein the first ethylene-alpha olefin copolymer is included in an amount of 82 wt % or more and 97 wt % or less, and
the second ethylene-alpha olefin copolymer is included in an amount of 3 wt % or more and 18 wt % or less.

### Claim 6 (depends on 5)

The polyethylene composition of claim 5,
wherein the first ethylene-alpha olefin copolymer (a) has
a number average molecular weight (Mn) of 12,000 g/mol or more and 50,000 g/mol or less,
a weight average molecular weight (Mw) of 80,000 g/mol or more and 250,000 g/mol or less, and
a molecular weight distribution (Mw/Mn) of 3.0 or more and 20.0 or less.

### Claim 7 (depends on 5)

The polyethylene composition of claim 5,
wherein the first ethylene-alpha olefin copolymer comprises an ethylene/1-hexene copolymer.

### Claim 8 (depends on 5)

The polyethylene composition of claim 5,
wherein the second ethylene-alpha olefin copolymer has;
a number average molecular weight (Mn) of 20,000 g/mol or more and 50,000 g/mol or less,
a weight average molecular weight (Mw) of 50,000 g/mol or more and 100,000 g/mol or less, and
a molecular weight distribution (Mw/Mn) of 1.5 or more and 4.0 or less.

### Claim 9 (depends on 5)

The polyethylene composition of claim 5,
wherein the second ethylene-alpha olefin copolymer comprises an ethylene/1-octene copolymer.

### Claim 10 (depends on 1)

A biaxially stretched film comprising the polyethylene composition of claim 1.

### Claim 11 (depends on 1)

A biaxially stretched film comprising the polyethylene composition of claim 1,
wherein an average of a machine direction (MD) tensile strength and a traverse direction (TD) tensile strength of the biaxially stretched film is 120 MPa or more, when measured according to ASTM D 882.

### Claim 12 (depends on 1)

A biaxially stretched film comprising the polyethylene composition of claim 1,
wherein a sum of a machine direction (MD) shrinkage and a traverse direction (TD) shrinkage after shrinkage at 100° C. for 7 minutes of the biaxially stretched film according to the ASTM 1204 is 7.0% or less, or
a sum of MD shrinkage and TD shrinkage after shrinkage at 120° C. for 7 minutes is 20.0% or less.

### Claim 13 (depends on 1)

A biaxially stretched film comprising the polyethylene composition of claim 1,
wherein a puncture strength of the biaxially stretched film measured according to EN 14477 is 280 N/mm or more.

### Claim 14 (depends on 1)

A biaxially stretched film comprising the polyethylene composition of claim 1,
wherein an average of a machine direction (MD) tensile strength and a traverse direction (TD) tensile strength of the biaxially stretched film is 700 MPa or more, when measured according to ASTM D 882.