# US 2025/0154301 A1 · Polyethylene Resin Having Excellent Thermal Resistance

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154301 A1
- Document ID: US20250154301A1
- Status: Published application
- Kind: A1
- Application number: 18/838,446
- Filed: 2023-10-16
- Published: 2025-05-15
- Earliest claimed: 2022-10-27
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Yutaek Sung; Joongsoo KIM; Hyojoon Lee
- Web page: https://patentgrep.com/patent/US20250154301A1

## CPC

- C08F 210/02: Ethene
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08F 4/65908: {in combination with an ionising compound other than alumoxane, e.g. (C6F5)4B-X+}
- C08F 4/65912: {in combination with an organoaluminium compound}
- C08F 4/65916: {supported on a carrier, e.g. silica, MgCl2, polymer}
- C08F 2420/02: Cp or analog bridged to a non-Cp X anionic donor
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

Provided is a polyethylene resin satisfying the following conditions 1) to 3), and being excellent in both mechanical properties and thermal resistance: 1) an inflection point exists in the range of −1.0≤log G*≤−0.5 in a modified VGP (Van Gurp Palmen) plot having an x-axis of log G* (G* is complex modulus, unit: dyne/cm2) and a y-axis of phase angle (unit: °); 2) Δ tan δ at 50 to 80° C. is less than 0.025 when measured by DMTA (Dynamic Mechanical Thermal Analysis); and 3) a melt index (MI2.16) measured at 190° C. under a load of 2.16 kg according to ASTM D1238 is 0.10 g/10 min or more.

## Claims

### Claim 1

A polyethylene resin satisfying the following conditions 1) to 3):
1) an inflection point exists in a range of −1.0≤log G*≤−0.5 in a modified Van Gurp Palmen (VGP) plot having an x-axis of log G*, wherein G* is complex modulus, with a unit of dyne/cm2, and a y-axis of phase angle with a unit of °;
2) Δ tan δ at 50 to 80° C. is less than 0.025 when measured by Dynamic Mechanical Thermal Analysis (DMTA); and
3) a melt index (MI2.16) measured at 190° C. under a load of 2.16 kg according to ASTM D1238 is 0.10 g/10 min or more.

### Claim 2 (depends on 1)

The polyethylene resin of claim 1,
wherein the Δ tan δ is calculated by the following Equation 1:
Δ tan δ=tan δ(@80° C.)−tan δ(@50° C.) [Equation 1]
in Equation 1,
tan δ (@80° C.) is a ratio of loss modulus (G′) to storage modulus (G″) at 80° C. (G″/G′, @80° C.), and
tan δ (@50° C.) is a ratio of loss modulus (G′) to storage modulus (G″) at 50° C. (G″/G′, @50° C.).

### Claim 3 (depends on 1)

The polyethylene resin of claim 1,
which has a bimodal molecular weight distribution.

### Claim 4 (depends on 1)

The polyethylene resin of claim 1,
wherein the melt index (MI2.16) is 0.10 to 2.0 g/10 min.

### Claim 5 (depends on 1)

The polyethylene resin of claim 1,
which has a density of 0.945 to 0.960 g/cm3.

### Claim 6 (depends on 1)

The polyethylene resin of claim 1,
which has a molecular weight distribution (Mw/Mn) of 7 to 20.

### Claim 7 (depends on 1)

The polyethylene resin of claim 1,
which has a melt flow rate ratio (MFRR, MI21.6/MI2.16) measured at 190° C. according to ASTM D1238 of 60 to 200.

### Claim 8 (depends on 1)

The polyethylene resin of claim 1,
which is an ethylene/1-hexene copolymer.

### Claim 9 (depends on 1)

The polyethylene resin of claim 1,
which has a S.H. (Strain Hardening) modulus measured at 80° C. according to ISO standards of 22.0 MPa or more.

### Claim 10 (depends on 1)

The polyethylene resin of claim 1,
wherein the Δ tan δ is 0 or more.

### Claim 11 (depends on 1)

The polyethylene resin of claim 1,
which has a S.H. (Strain Hardening) modulus measured at 80° C. according to ISO 18488 standards of 22.0 MPa to 35.0 MPa.