# US 2025/0154069 A1 · Method and device for producing a silicon carbide containing workpiece

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154069 A1
- Document ID: US20250154069A1
- Status: Published application
- Kind: A1
- Application number: 18/832,962
- Filed: 2023-01-27
- Published: 2025-05-15
- Earliest claimed: 2022-02-01
- Assignees: The Yellow SiC Holding GmbH
- Applicants: The Yellow SiC Holding GmbH
- Inventors: Siegmund GREULICH-WEBER
- Web page: https://patentgrep.com/patent/US20250154069A1

## CPC

- C04B 35/573: obtained by reaction sintering {or recrystallisation}
- C04B 2235/614: Gas infiltration of green bodies or pre-forms
- C04B 2235/656: characterised by specific heating conditions during heat treatment
- C04B 2235/6582: Hydrogen containing atmosphere
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Disclosed are a method and an apparatus for producing a silicon carbide-containing workpiece, in which: a blank (2) is held in a heated reactor (1), a gas composition is fed into the reactor (1), the gas composition serving as a precursor for silicon carbide production and containing gaseous tetrachlorosilane as a silicon source and a hydrocarbon gas as a carbon source, and the silicon carbide-containing workpiece is produced from the blank (2) under the action of the gas composition.

## Claims

### Claim 1

A method for producing a silicon carbide-containing workpiece, comprising:
holding a blank (2) in a heated reactor (1),
feeding a gas composition into the reactor (1), said gas composition serving as a precursor for silicon carbide production and containing gaseous tetrachlorosilane as a silicon source and a hydrocarbon gas as a carbon source, and
producing the silicon carbide-containing workpiece from the blank (2) under the action of the gas composition.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the reactor (1) is heated to a temperature in the range from 900 to 1300° C.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the gas composition further comprises hydrogen as a carrier gas.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the blank (2) includes a carbon-containing material which is transformed into silicon carbide at least near its surface.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the blank (2) is porous, and components from the gas composition infiltrate the blank (2).

### Claim 6 (depends on 1)

A method according to claim 1, wherein the gas composition fed into the reactor (1) is controlled such that the proportion of hydrocarbon gas in the gas composition increases over time in relation to the proportion of tetrachlorosilane in the gas composition.

### Claim 7

An apparatus for producing a silicon carbide-containing workpiece, comprising:
a heatable reactor (1) which is configured to maintain a carbon-containing blank (2) at a temperature which permits its transformation into the silicon carbide-containing workpiece, and
a source (5), connected to the reactor (1), of a gas composition serving as a precursor for silicon carbide production and containing gaseous tetrachlorosilane as a silicon source and hydrocarbon gas as a carbon source.