# US 2025/0154059 A1 · Low-alkali accelerator and preparation method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154059 A1
- Document ID: US20250154059A1
- Status: Published application
- Kind: A1
- Application number: 19/021,057
- Filed: 2025-01-14
- Published: 2025-05-15
- Earliest claimed: 2023-06-09
- Assignees: China Railway No.4 Engineering Group Co., Ltd; Anhui Engineering Material Technology Co, Ltd of Ctce Group; Yunnan China Railway New Materials Technology Co., Ltd
- Applicants: China Railway No.4 Engineering Group Co., Ltd; Anhui Engineering Material Technology Co, Ltd of Ctce Group; Yunnan China Railway New Materials Technology Co., Ltd
- Inventors: Dongdong FAN; Chunhong LIN; Zongjian ZHU; Zhiyong WANG; Hai HUANG; Zhenghui XIA; Shuangchao LI; Zhonghan WANG; Yafei ZHANG
- Web page: https://patentgrep.com/patent/US20250154059A1

## CPC

- C04B 14/043: {Alkaline-earth metal silicates, e.g. wollastonite}
- C04B 40/0039: {Premixtures of ingredients}
- C04B 14/045: {Alkali-metal containing silicates, e.g. petalite (waterglass C04B12/04)}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

A low-alkali accelerator and a preparation method therefor are provided. The preparation method comprises: S1, preparing a sodium metaaluminate solution; S2, adding water to the sodium metaaluminate solution, stirring same until uniform, then adding aluminum sulfate thereto, and reacting same at 50-80° C. for 0.5-1 h under stirring conditions; S3, within 10-30 min after complete reaction of the aluminum sulfate, adding, in a dropwise manner, a regulator to regulate the pH value to a neutral state; S4, mixing a strong-alkali weak-acid salt and a silicon dioxide gel until uniform, then adding same to a fluoride salt, and mixing same until uniform, to obtain a modified fluoride salt; and adding the modified fluoride salt to a neutral solution obtained in S3, and reacting same for 1-1.5 h, with the temperature maintained at 50-80° C.; and S5, adding an organic alcohol amine thereto, and stirring same for 0.5-1 h, to obtain the low-alkali accelerator.

## Claims

### Claim 1

A preparation method for a low-alkali accelerator, comprising the following steps:
S1, preparing a sodium metaaluminate solution;
S2, adding water to the sodium metaaluminate solution, stirring same until uniform, then adding aluminum sulfate thereto, and reacting same at 50-80° C. for 0.5-1 h under stirring conditions;
S3, after complete dissolution of the aluminum sulfate, regulating a pH value to a neutral state, to obtain a neutral solution;
S4, mixing a strong-alkali weak-acid salt and a silicon dioxide gel until uniform, then adding same to a fluoride salt, and mixing same until uniform, so as to obtain a modified fluoride salt; and adding the modified fluoride salt to the neutral solution, and reacting same for 1-1.5 h, with a temperature maintained at 50-80° C.; and
S5, adding an organic alcohol amine thereto, and stirring same for 0.5-1 h, so as to obtain the low-alkali accelerator.

### Claim 2 (depends on 1)

The preparation method according to claim 1, wherein the silicon dioxide gel is hydrophilic.

### Claim 3 (depends on 1)

The preparation method according to claim 1, wherein a specific surface area of the silicon dioxide gel is 600-800 m2/g.

### Claim 4 (depends on 1)

The preparation method according to claim 1, wherein the sodium metaaluminate solution comprises sodium hydroxide and aluminum hydroxide, and a mass ratio of the sodium hydroxide to the aluminum hydroxide is 1:2.5-3.5.

### Claim 5

A low-alkali accelerator, comprising the following components in percentage by weight:
sodium metaaluminate: 7-16%;
aluminum sulfate: 35-40%;
a modifier: 1-5%;
a fluorine salt: 4-10%;
organic alcohol amine: 5-10%;
water: 20-36%;
a sum of all the components: 100%; and
the modifier comprises a strong-alkali weak-acid salt and silicon dioxide gel, and a mass ratio of the strong-alkali weak-acid salt to the silicon dioxide gel is 2-4:1.

### Claim 6 (depends on 5)

The low-alkali accelerator according to claim 5, wherein the strong-alkali weak-acid salt comprises at least one of sodium carbonate, sodium bicarbonate, potassium carbonate, sodium sulfite, sodium acetate, sodium sulfide, and sodium phosphate.

### Claim 7 (depends on 5)

The low-alkali accelerator according to claim 5, wherein the fluoride salt comprises at least one of sodium fluoride, sodium fluorosilicate and magnesium fluorosilicate.

### Claim 8 (depends on 5)

The low-alkali accelerator according to claim 5, wherein the fluoride salt comprises sodium fluoride, sodium fluorosilicate, and magnesium fluorosilicate.

### Claim 9 (depends on 8)

The low-alkali accelerator according to claim 8, wherein a mass ratio of the sodium fluoride to the sodium fluorosilicate and to the magnesium fluorosilicate is (1-2):(5-7):(2-3).

### Claim 10 (depends on 8)

The low-alkali accelerator according to claim 8, wherein a mass ratio of the sodium fluoride to the sodium fluorosilicate and to the magnesium fluorosilicate is 1.5:6:2.5.