# US 2025/0154055 A1 · Method for preparing general-purpose cement by chlorination roasting of aluminosilicates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154055 A1
- Document ID: US20250154055A1
- Status: Published application
- Kind: A1
- Application number: 19/024,581
- Filed: 2025-01-16
- Published: 2025-05-15
- Earliest claimed: 2024-02-24
- Assignees: Hunan University of Science and Technology; Hunan Xiangchu Xianlu Environmental Protection Technology Co., Ltd.
- Applicants: Hunan University of Science and Technology; Hunan Xiangchu Xianlu Environmental Protection Technology Co., Ltd.
- Inventors: Meixun PENG; Qiming ZHAO; Yuanpeng ZHANG; Wenwei LIU; Meilin CHEN
- Web page: https://patentgrep.com/patent/US20250154055A1

## CPC

- C04B 7/24: Cements from oil shales, residues or waste other than slag
- C04B 7/243: {Mixtures thereof with activators or composition-correcting additives, e.g. mixtures of fly ash and alkali activators}
- C04B 7/434: {Preheating with addition of fuel, e.g. calcining}
- C04B 7/44: Burning; Melting
- C04B 7/52: Grinding {; After-treatment of ground cement}
- C04B 28/021: {Ash cements, e.g. fly ash cements (fly ash as filler C04B18/08); Cements based on incineration residues, e.g. alkali-activated slags from waste incineration (alkali-activated combustion residues as such C04B7/243; mixtures of the lime-pozzuolane type C04B28/18); Kiln dust cements}
- C04B 2103/10: Accelerators; Activators
- Y02P 40/10: Production of cement, e.g. improving or optimising the production methods; Cement grinding
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for preparing a general-purpose cement by chlorination roasting of aluminosilicates is provided, in which a mixture of aluminosilicates and sodium chloride is roasted in a steam atmosphere to obtain a roasted slag. The roasted slag is mixed with a material containing calcium oxide and magnesium oxide and ground to prepare a raw meal powder. The raw meal powder is subjected to oxidative calcination at a temperature not lower than 1240° C., followed by rapid cooling to obtain a calcined slag. The calcined slag is mixed with 0-3% by weight of caustic alkali and ground to obtain the general-purpose cement.

## Claims

### Claim 1

A method for preparing a general-purpose cement by chlorination roasting of aluminosilicates, comprising:
(1) roasting a mixture of the aluminosilicates and sodium chloride in a steam atmosphere followed by fume discharge to obtain a solid roasted slag, wherein main chemical components of the aluminosilicates are SiO2 and Al2O3;
(2) quantitatively mixing the solid roasted slag with a material containing CaO and MgO followed by grinding to obtain a powder mixture, or
grinding the solid roasted slag followed by washing, drying, and mixing with a powder material containing CaO and MgO to obtain a powder mixture;
(3) subjecting the powder mixture to oxidative calcination at a temperature not lower than 1240° C. until a stable state with liquid phase dominated is formed, and cooling to obtain a calcined slag; and
(4) mixing the calcined slag with an alkali followed by grinding to obtain the general-purpose cement in a powder form, wherein the alkali is sodium hydroxide, potassium hydroxide or a combination thereof; or
grinding the calcined slag separately to obtain an active powder component of the general-purpose cement for storage, and mixing the active powder component with an aqueous solution of the alkali to produce a slurry of the general-purpose cement for use.

### Claim 2 (depends on 1)

The method of claim 1, wherein in step (1), a steam flow rate is at least 60 g·min−1·m−2.

### Claim 3 (depends on 1)

The method of claim 1, wherein in step (1), a maximum roasting temperature is 800-1000° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein in step (1), a holding time at a maximum roasting temperature is at least 1 h.

### Claim 5 (depends on 1)

The method of claim 1, wherein in a slag produced from the aluminosilicates by oxidative calcination at 950° C., a total weight percentage of SiO2, Al2O3, Fe2O3, CaO, MgO, Na2O and K2O is greater than 90.0%, and a weight ratio of SiO2 to Al2O3 to Fe2O3 to CaO to MgO to a combination of Na2O and K2O is 49.0-82.5:10.0-46.0:0-8.1:0-5.0:0-9.5:0-12.2.

### Claim 6 (depends on 1)

The method of claim 1, wherein the mixture of the aluminosilicates and sodium chloride in step (1) is produced through steps of:
mixing the aluminosilicates with sodium chloride followed by grinding and sieving with an 80-μm square-hole sieve.

### Claim 7 (depends on 1)

The method of claim 1, wherein in step (1), the sodium chloride is 45.0% or less of a total weight of SiO2 and Al2O3 in the aluminosilicates.

### Claim 8 (depends on 1)

The method of claim 1, wherein in the calcined slag obtained in step (3), a weight ratio of SiO2 to Al2O3 to Fe2O3 to CaO to MgO to a combination of Na2O and K2O is 30.0-42.0:10.0-17.0:0-6.0:22.0-46.0:0-16.0:3.1-8.3.

### Claim 9 (depends on 1)

The method of claim 1, wherein in step (4), a mass of the alkali is calculated according to the following formula:
(NaOH+0.713KOH)/the calcined slag=0-3.0%.

### Claim 10 (depends on 1)

The method of claim 1, wherein in step (1), a discharged fume is introduced into water for dissolution and collection, and a resultant aqueous solution is used to produce HCl gas or hydrochloric acid, or for recovering valuable metals.