# US 2025/0154024 A1 · Composition, methods for its production, and its use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154024 A1
- Document ID: US20250154024A1
- Status: Published application
- Kind: A1
- Application number: 19/021,332
- Filed: 2025-01-15
- Published: 2025-05-15
- Earliest claimed: 2018-04-03
- Assignees: Ilika Technologies Limited
- Applicants: Ilika Technologies Limited
- Inventors: Laura Perkins; William Richardson; Louise Turner; Thomas Risbridger; Samuel Guerin; Brian Hayden; Owain Clark; Robert Noble; Jean-Philippe Soulié; Patrick Casey; Kyriakos Giagloglou
- Web page: https://patentgrep.com/patent/US20250154024A1

## CPC

- C01G 51/42: containing alkali metals, e.g. LiCoO2
- C23C 14/085: {of iron group metals}
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- H01M 4/0421: {involving vapour deposition}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0562: Solid materials
- H01M 10/0565: Polymeric materials, e.g. gel-type or solid-type
- C01P 2002/74: by peak-intensities or a ratio thereof only
- C01P 2002/82: by IR- or Raman-data
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a composition comprising: (a) a principal phase that is provided by a layered mixed metal oxide having a rocksalt structure belonging to the R-3m space group; the layered mixed metal oxide comprising the following component elements: 45 to 55 atomic % lithium; 20 to 55 atomic % of one or more transition metals selected from the group consisting of chromium, manganese, iron, nickel, cobalt, and combinations thereof; and 0 to 25 atomic % of one or more additional dopant elements selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, copper, ruthenium, zinc, molybdenum, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium; wherein said atomic % is expressed as a % of total atoms of said layered oxide, excluding oxygen; (b) a minor phase that is provided by a metal oxide that does not have the crystal structure of the layered mixed metal oxide, the minor phase comprising one or more of the transition metals contained in the layered mixed metal oxide, the transition metals being selected from the group consisting of chromium, manganese, iron, nickel, and cobalt. Methods of making the composition and electrodes and cells, especially solid-state batteries, containing the composition are also provided. The rough morphology of the crystals confers advantages compared with smoother crystals of similar chemical composition, particularly in solid-state batteries.

## Claims

### Claim 1

A method of preparing a composition comprising:
(a) a principal phase that is provided by a layered mixed metal oxide having a rocksalt structure belonging to the R-3m space group; the layered mixed metal oxide comprising the following component elements:
45 to 55 atomic % lithium;
20 to 55 atomic % of one or more transition metals selected from the group consisting of chromium, manganese, iron, nickel, cobalt, and combinations thereof; and
0 to 25 atomic % of one or more additional dopant elements selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, copper, ruthenium, zinc, molybdenum, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium;
wherein said atomic % is expressed as a % of total atoms of said layered oxide, excluding oxygen;
(b) a minor phase that is provided by a metal oxide that does not have the crystal structure of the layered mixed metal oxide, the minor phase comprising one or more of the transition metals contained in the layered mixed metal oxide, the transition metals being selected from the group consisting of chromium, manganese, iron, nickel, and cobalt;
wherein the principal phase provides 90% to 99.5% of the total mass of the composition, and the minor phase provides 0.5% to 10% of the total mass of the composition;
wherein the method is a sputtering deposition method comprising:
providing a sputtering target comprising a mixed metal oxide comprising lithium, one or more transition metals selected from the group consisting of chromium, manganese, iron, nickel, cobalt, and combinations thereof; and optionally one or more dopant elements selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, copper, ruthenium, zinc, molybdenum, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium;
providing a further sputtering target comprising a metal oxide phase comprising one or more of the transition metals contained in the first sputtering target, the transition metals being selected from the group consisting of chromium, manganese, iron, nickel, and cobalt;
sputtering said sputtering target and said further sputtering target to produce the composition.

### Claim 2 (depends on 1)

The method according to claim 1, comprising the step of sputtering the sputtering target to produce a film of the first phase, this step being preceded by the step of sputtering the further sputtering target to produce a film of the second phase.

### Claim 3 (depends on 1)

The method according to claim 1, further comprising the step of annealing the composition.

### Claim 4

A method of preparing a composition comprising:
(a) Co3O4, and
(b) crystalline lithium cobalt oxide or crystalline doped lithium cobalt oxide; said crystalline oxide comprising the following component elements:
45 to 55 atomic % lithium;
20 to 55 atomic % cobalt; and
0 to 25 atomic % of at least one additional dopant element selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, chromium, manganese, iron, copper, ruthenium, nickel, zinc, molybdenum, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium;
wherein said atomic % is expressed as a % of total atoms of said crystalline oxide, excluding oxygen;
wherein 0.01% to 10% total mass of said composition is Co3O4;
wherein 90% to 99.99% total mass of said composition is crystalline lithium cobalt oxide or crystalline doped lithium cobalt oxide;
wherein said composition has a bottom surface and a top surface;
where said crystalline lithium cobalt oxide or crystalline doped lithium cobalt oxide has a crystalline structure characterized by at least one of the following parameters (a) to (c):
(a) at least a portion of the crystalline structure has a crystal orientation, relative to a plane parallel to the bottom surface, selected from the group consisting of: (101), (104), (110) and (012);
(b) a Raman spectrum comprising bands at 484 cm−1, 593 cm−1, and at least one band selected from the group consisting of: 690 cm−1, 526 cm−1, and 625 cm−1 (each of said band ±25 cm−1);
(c) at least one X-ray powder diffraction peak measured using a Cu Kα X-ray source selected from the group consisting of: 2θ (±0.2°) 37.4°, 39.1°, 45.3° and 66.4°;
wherein the method is a sputtering deposition method comprising:
providing a first sputtering target comprising cobalt oxide;
providing a second sputtering target comprising a source of (a) lithium cobalt oxide or (b) lithium cobalt oxide comprising at least one dopant element selected from the group consisting of magnesium, calcium, strontium, titanium, zirconium, vanadium, chromium, manganese, iron, ruthenium, copper, molybdenum, nickel, zinc, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium;
sputtering said first sputtering target and said second sputtering target to produce the composition.

### Claim 5 (depends on 4)

A method according to claim 4, wherein the method is a sputtering deposition method comprising:
sputtering said first target to produce a thin-film layer of CO3O4 followed by sputtering said second target to produce a thin-film crystalline oxide of lithium and cobalt, optionally doped with at least one of said dopant elements.

### Claim 6 (depends on 4)

A method according to claim 4, wherein the method is a sputtering deposition method comprising:
sputtering said first target to produce a thin-film layer of CO3O4 with a top surface and a bottom surface; and
sputtering said second target to produce a thin-film crystalline oxide of lithium and cobalt, optionally doped with at least one of said dopant elements, on the top surface of said thin-film layer of CO3O4.

### Claim 7 (depends on 5)

A method according to claim 5, wherein the first sputtering target comprises CO3O4.

### Claim 8 (depends on 4)

The method according to claim 4, wherein said method further comprises annealing said crystalline oxide of lithium and cobalt, optionally doped with at least one of said dopant elements.

### Claim 9 (depends on 4)

A method according to claim 4, wherein said method comprises the step of providing a source of high energy ions, and generating a flux of said high energy ions.

### Claim 10 (depends on 1)

A method of making a solid-state electrochemical cell, comprising depositing an electrode of the cell using a method according to claim 1.

### Claim 11 (depends on 4)

The method of claim 4, wherein said crystalline oxide is HT-LiCoO2.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the minor phase comprises less than 1 atomic % lithium.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the minor phase is essentially free of lithium.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the layered mixed metal oxide comprises:
45 to 55 atomic % lithium;
40 to 55 atomic % of one or more transition metals selected from the group consisting of chromium, manganese, iron, nickel, cobalt, and combinations thereof; and
0 to 5 atomic % of one or more additional dopant elements selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, copper, ruthenium, zinc, molybdenum, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the layered mixed metal oxide comprises:
45 to 55 atomic % lithium;
45 to 55 atomic % of one or more transition metals selected from the group consisting of chromium, manganese, iron, nickel, cobalt, and combinations thereof.

### Claim 16 (depends on 4)

The method according to claim 4, wherein the crystalline oxide comprises:
45 to 55 atomic % lithium;
40 to 55 atomic % cobalt; and
0 to 5 atomic % of at least one dopant element selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, chromium, manganese, iron, copper, ruthenium, nickel, molybdenum, zinc, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium;
wherein said atomic % is expressed as a % of total atoms of said crystalline oxide, excluding oxygen.

### Claim 17 (depends on 4)

The method according to claim 4, wherein the crystalline oxide comprises:
45 to 55 atomic % lithium;
42.5 to 55 atomic % cobalt; and
0 to 2.5 atomic % of at least one dopant element selected from the group consisting of: magnesium, calcium, strontium, titanium, zirconium, vanadium, chromium, manganese, iron, copper, ruthenium, nickel, molybdenum, zinc, boron, aluminium, gallium, tin, lead, bismuth, lanthanum, cerium, gadolinium and europium;
wherein said atomic % is expressed as a % of total atoms of said crystalline oxide, excluding oxygen.

### Claim 18 (depends on 4)

The method according to claim 4, wherein the crystalline oxide comprises:
45 to 55 atomic % lithium; and
45 to 55 atomic % cobalt;
wherein said atomic % is expressed as a % of total atoms of said crystalline oxide, excluding oxygen.

### Claim 19 (depends on 4)

The method according to claim 4, wherein the crystalline oxide comprises:
47.0 to 53.0 atomic % lithium; and
47.0 to 53.0 atomic % cobalt;
wherein said atomic % is expressed as a % of total atoms of said crystalline oxide, excluding oxygen.

### Claim 20 (depends on 4)

The method according to claim 4, wherein the crystalline oxide comprises:
47.5 to 49.1 atomic % lithium; and
50.9 to 52.5 atomic % cobalt;
wherein said atomic % is expressed as a % of total atoms of said crystalline oxide, excluding oxygen.