# US 2025/0154006 A1 · Manufacture of an anode material with similar soft carbon and an application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0154006 A1
- Document ID: US20250154006A1
- Status: Published application
- Kind: A1
- Application number: 18/508,044
- Filed: 2023-11-13
- Published: 2025-05-15
- Earliest claimed: 2023-11-13
- Assignees: Glory Material Co., Ltd.
- Applicants: Glory Material Co., Ltd.
- Inventors: SHIAN-TSUNG CHOU; YU-SHIANG WU
- Web page: https://patentgrep.com/patent/US20250154006A1

## CPC

- C01B 32/05: Preparation or purification of carbon not covered by groups C01B32/15, C01B32/20, C01B32/25, C01B32/30
- H01M 10/05: Accumulators with non-aqueous electrolyte (H01M10/39 takes precedence)
- C01P 2004/02: obtained by optical microscopy
- C01P 2004/03: obtained by SEM
- C01P 2004/61: Micrometer sized, i.e. from 1-100 micrometer
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention is a manufacture of the anode material with similar soft carbon and an application thereof, which includes: using the isotropic coke to be heated through calcining; using the isotropic coke after calcining and heating, and then crushing the isotropic coke into particulate form, using the isotropic coke in particulate form and heating it under the heat treatment range of 2100 degrees Celsius to 2600 degrees Celsius to form the similar soft carbon; and using the similar soft carbon after mixing and sieving, the similar soft carbon is used the particle mean size 2 μm to 15 μm as the anode material.

## Claims

### Claim 1

A manufacture of an anode material with similar soft carbon, comprising:
step 1: using isotropic coke and heating the isotropic coke through calcination;
step 2: using the isotropic coke heated to calcine in step 1, and then grinding the isotropic coke in step 1 into particulate form;
step 3: using the isotropic coke in the form of particles in step 2 to be heated to the heat treatment range from 2100 degrees Celsius to 2600 degrees Celsius to form a type of said similar soft carbon; and
step 4: using the similar soft carbon in step 3, wherein the similar soft carbon has a particle mean size of 2 μm to 15 μm after mixing and sieving which is configured for the anode material.

### Claim 2 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein the heat treatment in step 3 raises the temperature and the holding time in the range from 2100 degrees Celsius to 2600 degrees Celsius is 8 hours.

### Claim 3 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein the degree of graphitization (g) of the similar soft carbon,
(
g
)
=
0.344
-
d
⁢
002
0.344
-
0.3354
×
100
⁢
%
=
70
⁢
%
⁢
to
⁢
82
⁢
%
,
wherein d002 is the interlayer spacing of the similar soft carbon, where the interlayer spacing of the similar soft carbon ranges from 0.33798 nm to 0.33695 nm.

### Claim 4 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein the charging rate of the similar soft carbon is 0.2 C to 10 C, the charging capacity ratio is between 100% and 88% thereof.

### Claim 5 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein a discharge rate of the similar soft carbon is 0.2 C to 10 C, a discharge capacity ratio is between 100% and 97% thereof.

### Claim 6 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein the similar soft carbon has a capacity retention of 99% to 90% after 200 to 600 cycles of charge and discharge in an environment of 45 degrees Celsius.

### Claim 7 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein the similar soft carbon has a capacity retention of 100% to 90% in an environment of 25 degrees Celsius to −10 degrees Celsius, wherein the capacity retention of the similar soft carbon is 90% to 85% in an environment of −10 degrees Celsius to −20 degrees Celsius.

### Claim 8 (depends on 1)

The manufacture of the anode material with similar soft carbon as claimed in claim 1, wherein the similar soft carbon is applied to lithium ion batteries and sodium ion batteries.

### Claim 9 (depends on 1)

An application of an anode material with similar soft carbon, which is used from claim 1, wherein the application of the similar soft carbon is applied to a start-stop battery, a starting battery, and a high-power hybrid electric vehicle (HEV) battery.