# US 2025/0153475 A1 · Fire resistant composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153475 A1
- Document ID: US20250153475A1
- Status: Published application
- Kind: A1
- Application number: 18/939,778
- Filed: 2024-11-07
- Published: 2025-05-15
- Earliest claimed: 2023-11-09
- Assignees: Milliken & Company
- Applicants: Milliken & Company
- Inventors: Shulong Li; Todd Moore; David Eskew
- Web page: https://patentgrep.com/patent/US20250153475A1

## CPC

- B32B 27/12: next to a fibrous or filamentary layer
- B32B 5/022: {Non-woven fabric}
- B32B 5/024: {Woven fabric}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/40: comprising polyurethanes
- B32B 2255/02: on fibrous or filamentary layer
- B32B 2255/24: Organic non-macromolecular coating
- B32B 2255/26: Polymeric coating
- B32B 2262/0269: Aromatic polyamide fibres
- B32B 2305/188: Woven fabrics
- B32B 2305/20: in the form of a non-woven mat
- B32B 2307/3065: Flame resistant or retardant, fire resistant or retardant
- B32B 2307/71: Resistive to light or to UV
- B32B 2307/728: Hydrophilic
- B32B 2307/7376: Thickness
- B32B 2375/00: Polyureas; Polyurethanes
- B32B 2437/00: Clothing
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

The application relates to a fire resistant composite containing a first textile, a first adhesive layer, a polyurethane membrane, a second adhesive layer, and a nonwoven textile. The first textile contains at least about 40% by weight inherently flame resistant fibers. The polyurethane membrane has a softening temperature of least about 210° C. according to ASTM E2347 test method and is non-melting according to ASTM F2894 test method. The polyurethane membrane contains a phosphor-based flame retardant. The nonwoven textile is a spunlace nonwoven textile and contains a plurality of staple fibers being at least about 40% by weight inherently flame resistant fibers. The second adhesive layer contains a discontinuous coating of a hot melt adhesive in a pattern of discrete elements, where the average distance between one element and a neighboring element is less than 1/10th the average fiber length of the fibers in the nonwoven textile.

## Claims

### Claim 1

A fire resistant composite comprising:
a first textile having a first surface and a second surface and a plurality of interstices, wherein the first textile comprises at least about 40% by weight inherently flame resistant fibers;
a polyurethane membrane on the second surface of the first textile having a softening temperature of least about 210° C. according to ASTM E2347 test method and is non-melting according to ASTM F2894 test method, and wherein the polyurethane membrane comprises a phosphor-based flame retardant;
a first adhesive layer located between the polyurethane membrane and the first textile;
a nonwoven textile located on the polyurethane membrane opposite to the first textile, wherein the nonwoven textile is a spunlace nonwoven textile and comprises a plurality of staple fibers being at least about 40% by weight inherently flame resistant fibers and having an average staple length of between about 20 and 60 mm, wherein the nonwoven textile has an areal weight of between about 0.2 and 2 oz/yd2; and,
a second adhesive layer located between the polyurethane membrane and the nonwoven textile, wherein the second adhesive layer comprises a discontinuous coating of a hot melt adhesive in a pattern of discrete elements, wherein the average distance between one element and a neighboring element is less than 1/10th the average fiber length of the fibers in the nonwoven textile.

### Claim 2 (depends on 1)

The fire resistant composite of claim 1, wherein at least one of the first adhesive layer or the second adhesive layer comprise a phosphor-based flame retardant.

### Claim 3 (depends on 1)

The fire resistant composite of claim 1, wherein both the first adhesive layer and the second adhesive layer comprise a phosphor-based flame retardant.

### Claim 4 (depends on 1)

The fire resistant composite of claim 1, wherein the first textile comprises a fire resistant coating, wherein the fire resistant coating is located on at least the first surface of the first textile and in at least a portion of the interstices of the first textile, wherein the fire resistant coating comprises a phosphor-based flame retardant.

### Claim 5 (depends on 1)

The fire resistant composite of claim 1, wherein the phosphor-based flame retardant is phosphorus-nitrogen compound or a phosphate ester compound.

### Claim 6 (depends on 5)

The fire resistant composite of claim 5, wherein the phosphate ester compound is selected from the group consisting of a cyclic phosphate ester, an organic phosphinate, an organic phosphonate, phosphorus polyols and mixtures thereof.

### Claim 7 (depends on 5)

The fire resistant composite of claim 5, wherein the phosphorus-nitrogen compound is selected from the group consisting of a phosphonium-nitrogen compound, a phosphonate-nitrogen compound, an organic phosphinate-nitrogen compound, a phosphate amide compound, a phosphine oxide-nitrogen compound, and mixtures thereof.

### Claim 8 (depends on 1)

The fire resistant composite of claim 1, wherein the fire resistant composite comprises less than about 5 ppm by weight organic fluorine.

### Claim 9 (depends on 1)

The fire resistant composite of claim 1, wherein the nonwoven textile has a thickness of is less than 1/10th of the average fiber length of the fibers in the nonwoven textile.

### Claim 10 (depends on 1)

The fire resistant composite of claim 1, wherein the first textile comprises at least about 80% by weight aramid fibers.

### Claim 11 (depends on 8)

The fire resistant composite of claim 8, wherein the aramid fibers in the first textile comprise between about 70 and 98% by weight meta-aramid fibers and about 2 and 30% by weight para-aramid fibers.

### Claim 12 (depends on 1)

The fire resistant composite of claim 1, wherein the first textile is a woven textile.

### Claim 13 (depends on 1)

The fire resistant composite of claim 1, wherein the first textile has an areal weight of between about 2 and 8 oz/yd2.

### Claim 14 (depends on 1)

The fire resistant composite of claim 1, wherein the polyurethane membrane comprises aromatic isocyanate and polyethylene oxide monomer units.

### Claim 15 (depends on 1)

The fire resistant composite of claim 1, wherein the polyurethane membrane is hydrophilic and has a swelling ratio in water of about 20-150%.

### Claim 16 (depends on 1)

The fire resistant composite of claim 1, wherein the polyurethane membrane comprises an opacifying agent having a UV absorbing property.

### Claim 17 (depends on 1)

The fire resistant composite of claim 1, wherein the polyurethane membrane has an average thickness of between about 10 and 32 micrometers.

### Claim 18 (depends on 1)

The fire resistant composite of claim 1, wherein the polyurethane membrane has an average thickness of between about 30 and 50 micrometers.

### Claim 19 (depends on 1)

The fire resistant composite of claim 1, wherein the nonwoven textile has a thickness less than about 1.5 mm.

### Claim 20 (depends on 1)

The fire resistant composite of claim 1, wherein the second surface of the nonwoven textile layer comprises a hydrophilic coating.

### Claim 21 (depends on 1)

The fire resistant composite of claim 1, wherein at least one of the first adhesive and the second adhesive comprise a thermoset polymer.

### Claim 22 (depends on 1)

The fire resistant composite of claim 1, wherein both the first adhesive and the second adhesive comprise a thermoset polymer.

### Claim 23 (depends on 1)

A garment comprising:
a plurality of fire resistant composites of claim 1 joined together by at least one sewn seam; and,
an adhesive tape disposed over the at least one sewn seam to provide liquid tight seal of the sewn seam, wherein the adhesive tape comprises a backing film layer and a tape adhesive layer, wherein the backing film layer comprises a polyurethane having a softening point of greater than 140° C., and the tape adhesive layer comprises a polyurethane or polyolefin having a softening point between 60° C. and 120° C.