# US 2025/0153467 A1 · Laminate for vehicle interior material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153467 A1
- Document ID: US20250153467A1
- Status: Published application
- Kind: A1
- Application number: 18/436,672
- Filed: 2024-02-08
- Published: 2025-05-15
- Earliest claimed: 2023-11-13
- Assignees: Hyundai Motor Company; Kia Corporation; Hanwha Advanced Materials Corporation
- Applicants: Hyundai Motor Company; Kia Corporation; Hanwha Advanced Materials Corporation
- Inventors: Eun Ju Noh; Jae Hyun An; In Soo Han; Ju Wan Lim; Jong Taek Na; Je Beom Yeon; Min Hyuk Kim
- Web page: https://patentgrep.com/patent/US20250153467A1

## CPC

- B32B 27/08: of synthetic resin
- B32B 3/30: characterised by a layer formed with recesses or projections, e.g. {hollows, grooves, protuberances, ribs (apertured layer B32B3/266; layer with cavities or internal voids B32B3/26)}
- B32B 5/18: characterised by features of a layer {of} foamed material
- B32B 5/245: {another layer next to it being a foam layer}
- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- B32B 27/18: characterised by the use of special additives
- B32B 27/30: comprising vinyl {(co)polymers; comprising acrylic (co)polymers}
- B32B 27/308: {comprising acrylic (co)polymers}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/322: {comprising halogenated polyolefins, e.g. PTFE}
- B32B 27/40: comprising polyurethanes
- B32B 37/1284: {Application of adhesive}
- B32B 37/153: {at least one layer is extruded and immediately laminated while in semi-molten state}
- B32B 38/164: {Drying}
- B32B 2250/05: 5 or more layers
- B32B 2250/24: All layers being polymeric
- B32B 2305/022: Foam
- B32B 2307/30: having particular thermal properties
- B32B 2307/3065: Flame resistant or retardant, fire resistant or retardant
- B32B 2307/536: Hardness
- B32B 2307/538: Roughness
- B32B 2307/54: Yield strength; Tensile strength
- B32B 2307/7376: Thickness
- B32B 2369/00: Polycarbonates
- B32B 2375/00: Polyureas; Polyurethanes
- B32B 2605/003: Interior finishings
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

Proposed is a laminate including a base layer, a second layer positioned on the base layer, and a first layer positioned on the second layer, in which the first layer includes a polycarbonate-based polyurethane, and the second layer includes a thermoplastic polyurethane. The thermoplastic polyurethane has an elongation at break of 400% or less and a melt index of 80 to 140 g/10 min at a temperature of 185° C. and a load of 2.16 kg.

## Claims

### Claim 1

A laminate comprising:
a base layer;
a second layer positioned on the base layer; and
a first layer positioned on the second layer,
wherein the first layer comprises a polycarbonate-based polyurethane,
wherein the second layer comprises a thermoplastic polyurethane, and
wherein the thermoplastic polyurethane has an elongation at break of 400% or less and a melt index of 80 to 140 g/10 min at a temperature of 185° C. and a load of 2.16 kg.

### Claim 2 (depends on 1)

The laminate of claim 1, wherein the thermoplastic polyurethane has an elongation at break of 250% to 370%.

### Claim 3 (depends on 1)

The laminate of claim 1, wherein the second layer comprises 5 to 20 parts by weight of a phosphorus-based flame retardant with respect to 100 parts by weight of the thermoplastic polyurethane.

### Claim 4 (depends on 1)

The laminate of claim 1, wherein the second layer has a thickness of 0.15 to 0.45 mm.

### Claim 5 (depends on 1)

The laminate of claim 1, wherein the first layer has a thickness of 0.03 to 0.25 mm.

### Claim 6 (depends on 1)

The laminate of claim 1, wherein a certain laminate comprising the first layer positioned on the second layer has a Shore A 15 hardness of 55 to 80.

### Claim 7 (depends on 1)

The laminate of claim 1, wherein a certain laminate comprising the first layer positioned on the second layer has a Young's modulus at 100% elongation of 58 to 82 kgf/cm2 and a tensile strength of 100 to 151 kgf/cm2.

### Claim 8 (depends on 1)

The laminate of claim 1, wherein a certain laminate comprising the first layer positioned on the second layer has an elongation at break of 204% to 400%.

### Claim 9 (depends on 1)

The laminate of claim 1, wherein the laminate has a tensile strength of 17 to 39 kgf/cm2 and an elongation at break of 207% to 300%.

### Claim 10 (depends on 1)

The laminate of claim 1, wherein the laminate excluding the base layer has a thickness of 0.25 to 0.6 mm.

### Claim 11 (depends on 1)

The laminate of claim 1, further comprising an adhesive layer positioned between the base layer and the second layer.

### Claim 12

A laminate for a vehicle interior material, the laminate comprising:
a back layer;
a foam layer positioned on the back layer;
an adhesive layer positioned on the foam layer;
a second layer positioned on the adhesive layer;
a first layer positioned on the second layer; and
a surface treatment layer positioned on the first layer,
wherein the first layer comprises a polycarbonate-based polyurethane,
wherein the second layer comprises a thermoplastic polyurethane, and
wherein the thermoplastic polyurethane has an elongation at break of 400% or less and a melt index of 140 g/10 min or less at a temperature of 185° C. and a load of 2.16 kg.

### Claim 13 (depends on 12)

The laminate of claim 12, wherein the laminate is applied to a crash pad of a vehicle.

### Claim 14 (depends on 12)

The laminate of claim 12, wherein the back layer comprises any one selected from the group consisting of a polyurethane resin, a chlorinated polypropylene resin, an acrylic resin, and combinations thereof.

### Claim 15 (depends on 12)

The laminate of claim 12, wherein the surface treatment layer has an uneven surface having a plurality of protrusions and depressions.

### Claim 16 (depends on 12)

The laminate of claim 12, wherein the back layer has a thickness of 0.001 to 0.5 mm, or 0.001 to 0.1 mm.

### Claim 17 (depends on 12)

The laminate of claim 12, wherein the surface treatment layer has a thickness of 0.001 to 0.5 mm.

### Claim 18 (depends on 12)

A method of manufacturing the laminate of claim 12, the method comprising:
(a) extruding a second raw material mixed with a thermoplastic polyurethane resin;
(b) rolling a resulting extruded product into a second layer having a predetermined thickness;
(c) forming a first layer by adding a first raw material mixed with a polycarbonate-based polyurethane resin to the second layer and then processing a resulting product;
(d) performing surface treatment on the first layer and then forming a back layer on one side of a base layer; and
(e) applying an adhesive on the one side of the base layer and then bonding a resulting layer to a lower surface of the second layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein an extrusion temperature in the (a) is in a range of 150° C. to 180° C.

### Claim 20 (depends on 18)

The method of claim 18, wherein the (c) included applying the first raw material on the moving second layer and drying the resulting product at a temperature of 50° C. to 150° C.