# US 2025/0153419 A1 · Thermoforming of pla-based articles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153419 A1
- Document ID: US20250153419A1
- Status: Published application
- Kind: A1
- Application number: 18/957,346
- Filed: 2024-11-22
- Published: 2025-05-15
- Earliest claimed: 2019-01-09
- Assignees: Purac Biochem B.V.
- Applicants: Purac Biochem B.V.
- Inventors: Martin Doornheim
- Web page: https://patentgrep.com/patent/US20250153419A1

## CPC

- B29C 51/002: {characterised by the choice of material}
- B29C 51/08: Deep drawing or matched-mould forming, i.e. using mechanical means only
- B29C 51/421: {of preforms, specially adapted for thermoforming (preheating sheets in general B29B13/023; B29C51/427 takes precedence)}
- B29C 51/426: {Producing specific thermal regimes during thermoforming to obtain particular properties}
- B29C 51/46: Measuring, controlling or regulating
- B29K 2067/046: {PLA, i.e. polylactic acid or polylactide}
- B29K 2511/00: Use of natural products or their composites, not provided for in groups {B29K2401/00 - B29K2509/00,} as filler
- B29K 2995/0012: having particular thermal properties
- B29K 2995/0039: Amorphous
- B29K 2995/0041: Crystalline
- B29K 2995/0089: Impact strength or toughness
- B29L 2031/7132: {Bowls, Cups, Glasses}
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS
- B29L: INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULAR ARTICLES

## Abstract

A method for producing a polylactic acid (PLA) shaped article by thermoforming and thermoformed PLA articles. The method for producing a shaped article includes: heating a sheet of crystallizable polylactic acid (PLA)-based resin having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.70 as determined by differential scanning calorimetry (DSC), wherein heating includes a heating step the sheet is heated from a surface temperature of at most 80° C. to a surface temperature of at least 90° C. to at most 150° C. at heating rate of 5° C. to 25° C. per second, to provide heated sheet having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.5 as determined by DSC; and immediately after heating, forming heated sheet to provide a shaped article by means of a mold having a temperature of at least 70° C. and at most 120° C.

## Claims

### Claim 1

A shaped article, obtained by:
heating a sheet of crystallizable polylactic acid (PLA)-based resin having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.7 as determined by differential scanning calorimetry (DSC),
wherein the heating comprises a preheating step prior to a heating step,
wherein in the preheating step, the sheet is subjected to heating to a temperature from at least 40° C. to at most 80° C.,
wherein in the heating step, the sheet is heated from a surface temperature of at most 80° C. to a surface temperature of at least 90° C. to at most 150° C. at a heating rate of 5° C. to 25° C. per second,
wherein in the preheating step, the heating is at a heating rate different from the heating rate of the heating step and/or the sheet is kept at the temperature of the preheating for a period of time prior to commencement of the heating step, to provide a heated sheet having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.6 as determined by DSC; and,
immediately after the heating of the sheet, forming the heated sheet to provide the shaped article by means of a mold, wherein the mold has a temperature of at least 70° C. and at most 120° C.

### Claim 2 (depends on 1)

The shaped article of claim 1, wherein the crystallizable PLA-based resin comprises:
from 50 to 100 wt. % of a poly L-lactic acid (PLLA) polymer having an optical purity of at least 95%, based on the weight of L-lactoyl units over the total weight of lactoyl units in the PLLA polymer; or
from 50 to 100 wt. % of a poly D-lactic acid (PDLA) polymer having an optical purity of at least 95% based on the weight of D-lactoyl units over the total weight of lactoyl units in the PDLA polymer.

### Claim 3 (depends on 1)

The shaped article of claim 1, wherein in the heating step the sheet is heated to a surface temperature of at least 100° C. to at most 145° C.

### Claim 4 (depends on 1)

The shaped article of claim 1, wherein in the heating step the heating rate is of 6 to 25° C./s.

### Claim 5 (depends on 1)

The shaped article of claim 1, wherein the heated sheet has a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.7 as determined by DSC.

### Claim 6 (depends on 1)

The shaped article of claim 1, wherein the heated sheet has a melting enthalpy (ΔHm,0) of less than 25 J/gram as determined by DSC.

### Claim 7 (depends on 1)

The shaped article of claim 1, wherein the crystallizable PLA-based resin comprises a nucleation package and
wherein if the crystallizable PLA-based resin comprises PLLA polymer, the nucleation package comprises PDLA as nucleating agent; or
if the crystallizable PLA-based resin comprises PDLA polymer, the nucleation package comprises PLLA as nucleating agent,
the PLLA or PDLA as nucleating agent being present in an amount of 0.1-10 wt. % based on the total amount of PLA present in the crystallizable PLA-based resin.

### Claim 8 (depends on 1)

The shaped article of claim 1, wherein the crystallizable PLA-based resin comprises a nucleation package comprising at least one mineral as a nucleating agent and present in an amount of 0.1-30 wt. % based on the amount of PLA present in the crystallizable PLA-based resin.

### Claim 9 (depends on 1)

The shaped article of claim 1, wherein the PLA-based resin comprises a filler and/or an impact modifier.

### Claim 10 (depends on 1)

The shaped article of claim 1, wherein the mold has a temperature of greater than 75° C. and at most 120° C.

### Claim 11 (depends on 1)

The shaped article of claim 1, wherein the shaped article has a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) of less than 0.5 as determined by DSC and has a melting enthalpy (ΔHm,0) greater than 15 J/gram as determined by DSC.

### Claim 12 (depends on 1)

The shaped article of claim 1, wherein the shaped article is thermo-resistant and displays a shrinking of less than 2% when immersed in water at a temperature from 60 to 100° C. for 5 minutes.

### Claim 13 (depends on 1)

The shaped article of claim 1, wherein in the heating step, the sheet is heated to a surface temperature of at least 100° C. to at most 135° C.

### Claim 14 (depends on 4)

The shaped article of claim 4, wherein in the heating step, the heating rate is from 7 to 20° C./s.

### Claim 15 (depends on 14)

The shaped article of claim 14, wherein in the heating step, the heating rate is from 8 to 15° C./s.

### Claim 16 (depends on 1)

The shaped article of claim 1, wherein the heated sheet has a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.75 as determined by DSC.

### Claim 17 (depends on 8)

The shaped article of claim 8, wherein the at least one mineral is selected from among talc and kaolin.

### Claim 18 (depends on 1)

The shaped article of claim 1, wherein the mold has a temperature of from 70° C. to less than 95° C.

### Claim 19

A shaped article, obtained by:
heating a sheet of crystallizable polylactic acid (PLA)-based resin having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.7 as determined by differential scanning calorimetry (DSC),
wherein the heating comprises a preheating step prior to a heating step,
wherein in the preheating step, the sheet is subjected to heating to a temperature from at least 40° C. to at most 80° C.,
wherein in the heating step, the sheet is heated from a surface temperature of at most 80° C. to a surface temperature of at least 90° C. to at most 150° C. at a heating rate of 5° C. to 25° C. per second, to provide a heated sheet having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.6 as determined by DSC; and,
immediately after the heating, forming the heated sheet to provide the shaped article by means of a mold, wherein the mold has a temperature of from 70° C. to 85° C.

### Claim 20

A shaped article, obtained by:
heating a sheet of crystallizable polylactic acid (PLA)-based resin having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.7 as determined by differential scanning calorimetry (DSC),
wherein the heating comprises a preheating step prior to a heating step,
wherein in the preheating step, the sheet is subjected to heating to a temperature from at least 40° C. to at most 80° C.,
wherein in the heating step, the sheet is heated from a surface temperature of at most 80° C. to a surface temperature of at least 115° C. to at most 150° C. at a heating rate of 5° C. to 25° C. per second, to provide a heated sheet having a ratio of cold crystallization over total melting enthalpy (ΔHcc/ΔHm) greater than 0.6 as determined by DSC; and,
immediately after the heating, forming the heated sheet to provide the shaped article by means of a mold, wherein the mold has a temperature of at least 70° C. and at most 120° C.