# US 2025/0153268 A1 · Method for friction stir processing for the end surface of age-hardening aluminum alloy plates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153268 A1
- Document ID: US20250153268A1
- Status: Published application
- Kind: A1
- Application number: 19/024,282
- Filed: 2025-01-16
- Published: 2025-05-15
- Earliest claimed: 2024-01-24
- Assignees: Jimei University
- Applicants: Jimei University
- Inventors: Wenhui LIU; Lingji ZHANG; Qiuping YI; Yufeng SONG; Hao HUANG; Fan YE; Jianfeng CAO
- Web page: https://patentgrep.com/patent/US20250153268A1

## CPC

- B23K 20/1255: {Tools therefor, e.g. characterised by the shape of the probe}
- B23K 20/122: {using a non-consumable tool, e.g. friction stir welding}
- B23K 20/1265: {Non-butt welded joints, e.g. overlap-joints, T-joints or spot welds}
- B23K 20/1275: {involving metallurgical change}
- B23K 20/2336: {both layers being aluminium}
- B23K 2103/10: Aluminium or alloys thereof
- B23K 2103/14: Titanium or alloys thereof
- B23K 2103/20: Ferrous alloys and aluminium or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for friction stir processing of an end surface of an age-hardening aluminum alloy plate is provided, in which a solid-solution state age-hardening aluminum alloy plate is butt-joined to and clamped with a dissimilar plate to obtain a combined plate; two sides of the combined plate are respectively provided with a weld-start plate and a lead-out plate; a bottom end of a stirring head is provided with a stirring pin; a distance between the outer edge of the stirring pin and the end surface of the age-hardening aluminum alloy plate is maintained to be 0.01-5 mm; the stirring pin is rotated into the weld-start plate; the age-hardening aluminum alloy plate is subjected to friction stir processing underwater or in a liquid nitrogen cooling condition; and the processed age-hardening aluminum alloy plate is separated and subjected to aging treatment.

## Claims

### Claim 1

A method for friction stir processing of an end surface of an age-hardening aluminum alloy plate, comprising:
(1) butt-joining an age-hardening aluminum alloy plate in a solid-solution state onto a dissimilar plate followed by clamp fixing to obtain a combined plate, and arranging a weld-start plate at a first side of the combined plate and a lead-out plate at a second side of the combined plate;
(2) arranging a stirring pin at a bottom end of a stirring head, maintaining a distance between an outer edge of the stirring pin and an end surface of the age-hardening aluminum alloy plate to be 0.01-5 mm, and rotating the stirring pin into the weld-start plate;
(3) performing friction stir processing on the age-hardening aluminum alloy plate in an underwater condition or a liquid nitrogen cooling condition; and
(4) separating the age-hardening aluminum alloy plate from the weld-start plate, the lead-out plate and the dissimilar plate, and performing aging treatment on the age-hardening aluminum alloy plate.

### Claim 2 (depends on 1)

The method of claim 1, wherein in step (1), the age-hardening aluminum alloy plate is a solid-solution quenched age-hardening aluminum alloy plate or a laminated aluminum alloy plate; the dissimilar plate is a high-melting-point steel plate or titanium plate material; a thickness of the dissimilar plate is 0.001-1 mm less than a thickness of the age-hardening aluminum alloy plate; the weld-start plate and the lead-out plate respectively on both sides of the age-hardening aluminum alloy plate have the same thickness.

### Claim 3 (depends on 1)

The method of claim 1, wherein the stirring pin is threaded.

### Claim 4 (depends on 2)

The method of claim 2, wherein the stirring head is configured to be tilted toward a direction opposite to a feeding direction of the stirring head at an angle of 1-3° during operation; a plunge depth of the stirring head is greater than or equal to a thickness difference between the age-hardening aluminum alloy plate and the dissimilar plate; and a feeding speed of the stirring head is 50-250 mm/min, and a rotational speed of the stirring head is 500-2500 r/min.

### Claim 5 (depends on 1)

The method of claim 1, wherein in step (4), the aging treatment is carried out at 110-190° C. for 8-36 h.