# US 2025/0153264 A1 · Friction stir welding method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153264 A1
- Document ID: US20250153264A1
- Status: Published application
- Kind: A1
- Application number: 18/835,902
- Filed: 2023-02-07
- Published: 2025-05-15
- Earliest claimed: 2022-03-04
- Assignees: Osaka University
- Applicants: Osaka University
- Inventors: Hidetoshi FUJII; Muneaki MUKUDA; Yoshiaki MORISADA
- Web page: https://patentgrep.com/patent/US20250153264A1

## CPC

- B23K 20/1225: {Particular aspects of welding with a non-consumable tool}
- B23K 20/12: the heat being generated by friction; Friction welding
- B23K 20/1255: {Tools therefor, e.g. characterised by the shape of the probe}
- B23K 2103/10: Aluminium or alloys thereof
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The present invention provides a simple and efficient friction stir welding method that, in addition to enabling localized friction stir welding, makes it possible to obtain a smooth friction stir surface and increase tool lifespan. This friction stir welding method is characterized in that the tip end of a tool that is rotated at a prescribed speed is pressed into a material to be welded, a stir portion is formed by moving the tool in an arbitrary welding direction, and the tool is slanted toward the retreating side relative to the welding direction.

## Claims

### Claim 1

A friction stir welding method characterized by:
pressing a tip end of a tool that is rotated at a prescribed speed into a material to be welded,
forming a stir zone by moving the tool in an arbitrary welding direction, and
slanting the tool toward the retreating side relative to the welding direction during the moving.

### Claim 2 (depends on 1)

The friction stir welding method according to claim 1, wherein the tool does not have a shoulder portion.

### Claim 3 (depends on 1)

The friction stir welding method according to claim 1, wherein the tip portion is formed into a spherical crown shape or a conical shape.

### Claim 4 (depends on 1)

The friction stir welding method according to claim 1, wherein the slanting angle is 1 to 20°.

### Claim 5 (depends on 1)

The friction stir welding method according to claim 1, wherein an advance angle is provided to the tool.

### Claim 6 (depends on 1)

The friction stir welding method according to claim 1, wherein the diameter of the tool is 3 to 20 mm.

### Claim 7 (depends on 1)

The friction stir welding method according to claim 1, wherein
the material to be welded is aluminum material or an aluminum alloy material, and
the tool is made of tool steel.

### Claim 8 (depends on 1)

The friction stir welding method according to claim 1, wherein
the material to be welded is a steel material, and
the tool is made of cemented carbide or ceramics.

### Claim 9 (depends on 1)

The friction stir welding method according to claim 1, wherein a burr suppression jig is disposed on the outer edge of the tool.

### Claim 10 (depends on 1)

The friction stir welding method according to claim 1, wherein the advancing side of the tool plunged into the material to be welded is forcibly cooled.