# US 2025/0153242 A1 · Powder mixtures for additive manufacture having an increased density

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153242 A1
- Document ID: US20250153242A1
- Status: Published application
- Kind: A1
- Application number: 18/839,400
- Filed: 2023-04-28
- Published: 2025-05-15
- Earliest claimed: 2022-04-29
- Assignees: EOS GmbH Electro Optical Systems
- Applicants: Eos GmbH Electro Optical Systems
- Inventors: Hannu HEIKKINEN; Antti SEPPÄLÄ; Aki KUKKONEN; Jukka SIMOLA; Olli NYRHILÄ; Visa LUOTONEN
- Web page: https://patentgrep.com/patent/US20250153242A1

## CPC

- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B22F 1/065: Spherical particles
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/34: of powder characteristics, e.g. density, oxidation or flowability
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are powder mixtures for use in additive manufacture, which comprise three particle fractions A, B and C with different median particle sizes, wherein the median particle sizes relate to each other as 0.2 to 0.5/1/1.2 to 2. These powder mixtures have higher apparent density and/or conditioned bulk density compared to conventional additive manufacture powders and thus allow for faster processing with less defects. Further disclosed is technology that relates to methods for the preparation of respective powder mixtures, methods and devices for the preparation of three-dimensional objects from such powder mixtures and three-dimensional objects, which have been prepared accordingly, as well as the use of the powder mixtures for reducing the amount of defects in additive manufacturing processes.

## Claims

### Claim 1

Powder mixture for use in an additive manufacturing process, wherein the powder mixture comprises a particle fraction A with a median particle size α, a particle fraction B with a median particle size ρ, which is smaller than the median particle size α, and a particle fraction C with a median particle size γ, which is larger than the median particle size α, wherein the particle size of the particle fractions B, A and C relate to each other as 0.2 to 0.5/1/1.2 to 2.

### Claim 2 (depends on 1)

Powder mixture according to claim 1, wherein the median particle size of the particle fractions B, A and C relate to each other as 0.25 to 0.4/1/1.4 to 1.8.

### Claim 3 (depends on 1)

Powder mixture according to claim 1, further comprising a particle fraction D with a median particle size δ, which is larger than the median particle size β but smaller than the median particle size α, and where the particle size of the particle fraction D relates to the particle size of the fraction A as 0.6 to 0.8/1 and preferably 0.65 to 0.76/1.

### Claim 4 (depends on 1)

Powder mixture according to claim 1, wherein the particle fractions A, B and C have essentially the same composition, and wherein the particle fractions A, B, C and D have essentially the same composition.

### Claim 5 (depends on 1)

Powder mixture according to claim 1, wherein the powder mixture has a relative density and/or a relative conditioned bulk density of at least 54% and/or less than 70%.

### Claim 6 (depends on 1)

Powder mixture according to claim 1, wherein the powder mixture has an apparent density of at least 4.6 g/cm3 and/or 4.85 g/cm3 or less.

### Claim 7 (depends on 1)

Powder mixture according to claim 1, wherein the particle fraction A has a particle size D50 in the range of at least 38 μm and/or 48 μm or less.

### Claim 8 (depends on 1)

Powder mixture according to claim 1, wherein the particle fraction B has a particle size D50 in the range of at least 12 μm and/or 17 μm or less.

### Claim 9 (depends on 1)

Powder mixture according to claim 1, wherein the particle fraction C has a particle size D50 in the range of at least 62 μm and/or 80 μm or less.

### Claim 10 (depends on 1)

Powder mixture according to claim 1, wherein the particle fraction A has a distribution width as indicated by the span of from 0.55 to 0.8, and/or the particle fraction B has a distribution width as indicated by the span of from 1.0 to 1.4 and/or the particle fraction C has a distribution width as indicated by the span of from 0.35 to 0.5.

### Claim 11 (depends on 1)

Powder mixture according to claim 1, wherein the particle fractions A and C have a sphericity of at least 0.9 and wherein the particle fraction B is irregular.

### Claim 12 (depends on 1)

Powder mixture according to claim 1, wherein the particle fraction B accounts for 10 to 20 parts by weight, the particle fraction A accounts for 50 to 70 parts by weight and the particle fraction C accounts for 10 to 40 parts by weight, based on the total weight of the mixture, or wherein the particle fraction B accounts for 2 to 20 parts by weight, the particle fraction A accounts for 10 to 25 parts by weight and the particle fraction C accounts for 55 to 80 parts by weight, based on the total weight of the mixture.

### Claim 13 (depends on 1)

Powder mixture according to claim 1, wherein the particles in the fractions A, B and C are steel particles.

### Claim 14 (depends on 1)

Method for the preparation of a powder mixture, as claimed in claim 1, comprising providing a particle fraction A with a median particle size α, a particle fraction B with a median particle size β, which is smaller than the median particle size α, and a particle fraction C with a median particle size γ, which is larger than the median particle size α, wherein the particle size of the particle fractions B, A and C relate to each other as 0.2 to 0.5:1:1.2 to 2, and mixing the particle fractions A, B and C to provide a powder mixture.

### Claim 15 (depends on 14)

Method for the manufacture of a three-dimensional object, comprising a powder mixture prepared according to the method of claim 14, and preparing the object by applying the mixture layer on layer and selectively consolidating the mixture by application of electromagnetic radiation, at positions in each layer, which correspond to the cross section of the object in this layer, wherein the positions are scanned in at least one radiation interaction zone of an energy beam bundle.

### Claim 16 (depends on 15)

Method according to claim 15, wherein the individual layers are applied at a thickness of 30 μm or more and/or 80 μm or less.

### Claim 17 (depends on 15)

Three-dimensional object prepared according to the method of claim 15.

### Claim 18 (depends on 1)

Use of powder mixture according to claim 1 for reducing the number of defects in a three-dimensional object, which is prepared from the powder mixture by an additive manufacturing process.

### Claim 19 (depends on 15)

Device for implementing a method according to claim 15, wherein the device comprises an irradiation unit emitting electromagnetic or particle irradiation, a laser sintering or laser melting device, a process chamber having an open container with a container wall, a support, which is inside the process chamber, wherein open container and support are moveable against each other in vertical direction, a storage container and a recoater, which is moveable in horizontal direction, and wherein the storage container is at least partially filled with a powder mixture.