# US 2025/0153241 A1 · Permanent magnetic alloy powder and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153241 A1
- Document ID: US20250153241A1
- Status: Published application
- Kind: A1
- Application number: 18/506,560
- Filed: 2023-11-10
- Published: 2025-05-15
- Earliest claimed: 2023-11-10
- Assignees: Industrial Technology Research Institute
- Applicants: Industrial Technology Research Institute
- Inventors: Li-Shing Chou; Yu-Hsien Chou; Chi-San Chen
- Web page: https://patentgrep.com/patent/US20250153241A1

## CPC

- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/14: Treatment of metallic powder (mixing with lubricating or binding agents or with organic material B22F1/10)
- B22F 9/023: {Hydrogen absorption}
- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- C22C 33/0278: {with at least one alloying element having a minimum content above 5%}
- H01F 1/0573: {obtained by reduction or by hydrogen decrepitation or embrittlement}
- B22F 3/225: {by injection molding}
- B22F 2009/041: {by mechanical alloying, e.g. blending, milling}
- B22F 2201/11: Argon
- B22F 2301/355: Rare Earth - Fe intermetallic alloys
- B22F 2302/105: Silicium carbide (SiC)
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B33Y 70/00: Materials specially adapted for additive manufacturing
- C22C 2202/02: Magnetic
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

A permanent magnetic alloy powder includes rare earth elements, iron, boron, aluminum, copper and carbides. The rare earth elements include neodymium, and account for 24 to 30 parts by weight. Iron accounts for 65 to 72 parts by weight. Boron accounts for 0.8 to 1.2 parts by weight. Cobalt accounts for 2.8 to 3.2 parts by weight. Aluminum accounts for 0.2 to 0.6 parts by weight. Copper accounts for 0.1 to 0.4 parts by weight. The carbides account for 0.1 to 0.4 parts by weight. The particle size of the permanent magnetic alloy powders is 10 μm to 70 μm, and the grain size of NdFeB phase in the permanent magnetic alloy powders is less than 5 μm. Through the selection of alloy material ratio and manufacturing process, the processability and formability of permanent magnetic alloy materials can be effectively improved, suitable for metal injection molding and 3D printing production.

## Claims

### Claim 1

A permanent magnetic alloy powder, comprising:
a rare earth element comprising neodymium, and accounting for 24 to 30 parts by weight;
iron accounting for 68 to 72 parts by weight;
boron accounting for 0.8 to 1.2 parts by weight;
cobalt accounting for 2.8 to 3.2 parts by weight;
aluminum accounting for 0.2 to 0.6 parts by weight;
copper accounting for 0.1 to 0.4 parts by weight; and
a carbide comprising hafnium carbide, and accounting for 0.1 to 0.4 parts by weight,
wherein a particle size of the permanent magnetic alloy powder is 10 μm to 70 μm,
and a grain size of NdFeB phase in the permanent magnetic alloy powder is less than 5 μm.

### Claim 2 (depends on 1)

The permanent magnetic alloy powder according to claim 1, wherein the carbide further comprises silicon carbide.

### Claim 3 (depends on 1)

The permanent magnetic alloy powder according to claim 1, wherein the particle size of the permanent magnetic alloy powder is 10 μm to 25 μm.

### Claim 4 (depends on 1)

The permanent magnetic alloy powder according to claim 1, wherein the grain size of the NdFeB phase in the permanent magnetic alloy powder is 0.3 μm to 4 μm.

### Claim 5

A method for manufacturing a permanent magnetic alloy powder, comprising:
providing a raw material comprising:
a rare earth element comprising neodymium, and accounting for 24 to 30 parts by weight;
iron accounting for 68 to 72 parts by weight;
boron accounting for 0.8 to 1.2 parts by weight;
cobalt accounting for 2.8 to 3.2 parts by weight;
aluminum accounting for 0.2 to 0.6 parts by weight;
copper accounting for 0.1 to 0.3 parts by weight; and
a carbide comprising hafnium carbide, and accounting for 0.1 to 0.3 parts by weight;
atomizing and granulating a molten alloy raw material using a gas atomization method to obtain a plurality of permanent magnetic alloy primary powders;
performing a hydrogenation and disproportionation treatment on the permanent magnetic alloy primary powders; and
after the hydrogenation and disproportionation, performing a desorption treatment on the permanent magnetic alloy primary powders in an inert protective gas to obtain a plurality of permanent magnetic alloy powders, a particle size of the permanent magnetic alloy powders ranging from 10 μm to 70 μm, and a grain size of NdFeB phase of the permanent magnetic alloy powders being less than 5 μm.

### Claim 6 (depends on 5)

The method for manufacturing a permanent magnetic alloy powder according to claim 5, wherein the carbide further comprises silicon carbide.

### Claim 7 (depends on 5)

The method for manufacturing a permanent magnetic alloy powder according to claim 5, wherein the particle size of the permanent magnetic alloy powder is 10 μm to 25 μm.

### Claim 8 (depends on 5)

The method for manufacturing a permanent magnetic alloy powder according to claim 5, wherein the grain size of the NdFeB phase in the permanent magnetic alloy powder is 0.3 μm to 4 μm.

### Claim 9 (depends on 5)

The method for manufacturing a permanent magnetic alloy powder according to claim 5, wherein the hydrogenation and disproportionation is carried out at an operating temperature of 800° C. to 1000° C. and an operating pressure of 0.1 MPa to 0.3 MPa for 0.5 to 2 hours.

### Claim 10 (depends on 5)

The method for manufacturing a permanent magnetic alloy powder according to claim 5, wherein in the desorption treatment, the protective gas is argon and the operation lasts for 0.5 to 2 hours.