# US 2025/0153141 A1 · Lithium adsorbent, and preparation method and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0153141 A1
- Document ID: US20250153141A1
- Status: Published application
- Kind: A1
- Application number: 18/936,689
- Filed: 2024-11-04
- Published: 2025-05-15
- Earliest claimed: 2023-11-14
- Assignees: Sunresin New Materials Co. Ltd.
- Applicants: Sunresin New Materials Co. Ltd.
- Inventors: Heng LIU; Qiong LIU; Suidang LI; Xiaokang KOU
- Web page: https://patentgrep.com/patent/US20250153141A1

## CPC

- B01J 20/3064: {Addition of pore forming agents, e.g. pore inducing or porogenic agents}
- B01J 20/04: comprising compounds of alkali metals, alkaline earth metals or magnesium
- B01J 20/041: {Oxides or hydroxides}
- B01J 20/08: comprising aluminium oxide or hydroxide; comprising bauxite
- B01J 20/22: comprising organic material
- B01J 20/262: {obtained otherwise than by reactions only involving carbon to carbon unsaturated bonds, e.g. obtained by polycondensation (macromolecular compounds obtained otherwise than by reactions only involving unsaturated carbon-to-carbon bonds per se C08G)}
- B01J 20/3007: {Moulding, shaping or extruding}
- B01J 20/3071: {Washing or leaching}
- B01J 20/3078: {Thermal treatment, e.g. calcining or pyrolizing}
- B01J 20/3085: {Chemical treatments not covered by groups B01J20/3007 - B01J20/3078}
- B01J 2220/46: Materials comprising a mixture of inorganic and organic materials (materials coated or impregnated on a carrier B01J20/32)
- Y02P 10/20: Recycling
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Disclosed are a lithium adsorbent, and a preparation method and an application thereof, which relate to the technical of extraction of lithium. The method of the disclosure includes obtaining a lithium adsorbent intermediate by mixing an oil phase with an aqueous phase; and obtaining the lithium adsorbent by mixing the lithium adsorbent intermediate with an organic auxiliary agent; where the oil phase includes a lithium source, an aluminum source, an oil-phase matrix, and an oil-phase auxiliary agent, and the oil-phase matrix includes a high-molecular polymer and vinylidene fluoride; the mixing an oil phase with an aqueous phase includes performing gradient stirring on a mixture of the oil phase and the aqueous phase. According to the disclosure, the high-stability lithium adsorbent can be prepared by optimizing and screening the high-temperature resistant oil-phase matrix and a specific preparation process. Compared with an existing lithium adsorbent, the lithium adsorbent prepared through the disclosure has less degradation, better mechanical strength, and stronger corrosion resistance in a high-temperature environment, and therefore a way of effectively extracting lithium resources from high-temperature and high-salt brine is provided.

## Claims

### Claim 1

A method for preparing a lithium adsorbent, comprising: obtaining a lithium adsorbent intermediate by mixing an oil phase with an aqueous phase; and obtaining the lithium adsorbent by mixing the lithium adsorbent intermediate with an organic auxiliary agent; wherein
the oil phase comprises a lithium source, an aluminum source, an oil-phase matrix, and an oil-phase auxiliary agent, and the oil-phase matrix comprises a high-molecular polymer and vinylidene fluoride;
the step of mixing an oil phase with an aqueous phase comprises: performing gradient stirring on a mixture of the oil phase and the aqueous phase; and
the step of gradient stirring comprises: stirring the mixture at an initial stirring speed, wherein the initial stirring speed is in a range from 30 rpm to 190 rpm; stopping stirring the mixture for second set time each time after stirring the mixture for first set time; reducing the stirring speed by set rotation speed 1 after each stopping, then continuing stirring the mixture, and not stopping stirring the mixture until a stirring speed is less than or equal to set rotation speed 2, wherein set rotation speed 2 is in a range from 10 rpm to 30 rpm; and maintaining set rotation speed 2 and stirring at 40° C. to 120° C. for 20 min to 600 min.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first set time is in a range from 20 min to 120 min;
optionally, the second set time is in a range from 20 min to 120 min;
optionally, set rotation speed 1 is in a range from 10 rpm to 30 rpm; and
optionally, a stirring temperature before maintaining set rotation speed 2 is in a range from 40° C. to 80° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein a mass ratio of the high-molecular polymer to the vinylidene fluoride in the oil-phase matrix is 5:(1-10);
optionally, the high-molecular polymer comprises any one or more of polyacrylamide, polyacrylic acid, polyacrylate, polyurethane, polyester, polyether, polystyrene, polyenol, phenolic resin, and epoxy resin;
optionally, a mass ratio of the lithium source and the aluminum source in total to the oil-phase auxiliary agent is (3-18):10;
optionally, the oil-phase auxiliary agent comprises: N-methyl pyrrolidone and an organic solvent;
optionally, a mass ratio of the N-methyl pyrrolidone to the organic solvent is (1-5):1; and
optionally, the organic solvent in the oil-phase auxiliary agent comprises any one or more of methanol, ethanol, acetone, gasoline, N,N-dimethylformamide, ethyl acetate, dichloromethane, chloroform, benzene, toluene, isopropanol, and diethyl ether.

### Claim 4 (depends on 1)

The method according to claim 1, wherein a mixing volume ratio of the oil phase to the aqueous phase is 1:(1-3);
optionally, a molar ratio of the lithium source to the aluminum source is 5:(1-10);
optionally, the lithium source comprises a lithium salt;
optionally, the lithium source comprises any one or more of lithium chloride, lithium nitrate, lithium carbonate, lithium sulfate, lithium hydroxide, lithium acetate, and lithium oxide;
optionally, the aluminum source comprises an aluminum salt; and
optionally, the aluminum source comprises any one or more of aluminum chloride, aluminum nitrate, aluminum carbonate, aluminum sulfate, aluminum hydroxide, aluminum acetate, and aluminum oxide.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the oil phase further comprises at least one of an initiator and a pore-forming agent;
optionally, the initiator comprises any one or more of benzoyl peroxide, cumene hydroperoxide, and tert-butyl hydroperoxide;
optionally, the pore-forming agent comprises any one or more of white oil, liquid wax, gasoline, and n-octane;
optionally, the aqueous phase comprises water and a dispersant;
optionally, a mass volume fraction of the dispersant in the aqueous phase is in a range from 0.10% to 2%.
optionally, the dispersant comprises any one or more of carboxymethyl cellulose and hydroxyethyl cellulose;
optionally, after the oil phase is mixed with the aqueous phase, before the mixing of the lithium adsorbent intermediate obtained with an organic auxiliary agent, the method further comprises: removing the pore-forming agent by washing a product obtained after the oil phase is mixed with the aqueous phase with detergent 1; and
optionally, detergent 1 comprises any one or more of methanol, ethanol, acetone, gasoline, N,N-dimethylformamide, ethyl acetate, dichloromethane, chloroform, benzene, toluene, isopropanol, and diethyl ether.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the organic auxiliary agent comprises any one or more of polyvinyl alcohol, polylactic acid, cellulose acetate, ethyl cellulose, polyvinyl chloride, polycarbonate, a vinyl alcohol-ethylene cellulose copolymer, and an ethylene-propylene polymer;
optionally, a mass ratio of the lithium adsorbent intermediate to the organic auxiliary agent is 20:(1-8); and
optionally, a condition of mixing the lithium adsorbent intermediate with the organic auxiliary agent comprises a temperature of 30° C. to 80° C., and time of 1 h to 6 h.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the method further comprises, during the mixing of the lithium adsorbent intermediate with the organic auxiliary agent, adding a polar organic solvent to the mixing system;
optionally, the polar organic solvent comprises any one or more of ethanol, N,N-dimethylformamide, acetonitrile, and isopropanol;
optionally, the method further comprises, after mixing the lithium adsorbent intermediate with the organic auxiliary agent, washing a product obtained after mixing the lithium adsorbent intermediate with the organic auxiliary agent with detergent 2;
optionally, detergent 2 comprises water and/or an organic solvent;
optionally, the organic solvent in detergent 2 comprises any one or more of methanol, ethanol, acetone, gasoline, N,N-dimethylformamide, ethyl acetate, dichloromethane, chloroform, benzene, toluene, isopropanol, N-methyl pyrrolidone, and diethyl ether; and
optionally, the method further comprises, after washing the product with detergent 2, drying the product washed with detergent 2 to obtain the lithium adsorbent.

### Claim 8 (depends on 1)

A lithium adsorbent, comprising the lithium adsorbent prepared through the method according to claim 1.

### Claim 9 (depends on 8)

An application of the lithium adsorbent according to claim 8 in extracting lithium or preparing a product used for extracting lithium.

### Claim 10 (depends on 9)

The application according to claim 9, wherein the extracting of lithium comprises extracting lithium at a high temperature; and
optionally, the extracting of lithium comprises extracting lithium from high-temperature geothermal brine.