# US 2025/0149492 A1 · Copper paste for pressure bonding, semiconductor device, method for preparing copper paste for pressure bonding, and method for manufacturing semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149492 A1
- Document ID: US20250149492A1
- Status: Published application
- Kind: A1
- Application number: 18/838,020
- Filed: 2023-02-28
- Published: 2025-05-08
- Earliest claimed: 2022-03-31
- Assignees: Mitsui Mining & Smelting Co., Ltd.
- Applicants: Mitsui Mining & Smelting Co., Ltd.
- Inventors: Kei ANAI; Jo NISHIKAWA
- Web page: https://patentgrep.com/patent/US20250149492A1

## CPC

- H01B 1/22: the conductive material comprising metals or alloys
- H10W 72/30: Die-attach connectors
- B22F 1/052: characterised by a mixture of particles of different sizes or by the particle size distribution
- B22F 1/065: Spherical particles
- B22F 1/068: Flake-like particles
- B22F 1/09: {Mixtures of metallic powders}
- B22F 1/107: containing organic material comprising solvents, e.g. for slip casting
- B22F 7/04: with one or more layers not made from powder, e.g. made from solid metal
- H10W 72/013: {of die-attach connectors}
- H10W 72/071: {Connecting or disconnecting}
- H10W 72/073: {of die-attach connectors}
- B22F 2007/042: {characterised by the layer forming method}
- C22C 2200/04: Nanocrystalline
- H10W 72/01361: {Chemical or physical modification, e.g. by sintering or anodisation (patterning H10W72/01351)}
- H10W 72/07331: {Connecting techniques}
- H10W 72/07332: {Compression bonding, e.g. thermocompression bonding}
- H10W 72/325: {Die-attach connectors having a filler embedded in a matrix}
- H10W 72/352: {comprising metals or metalloids, e.g. solders}
- H10W 72/353: {not comprising solid metals or solid metalloids, e.g. ceramics}
- H10W 72/871: {Bond wires and strap connectors}
- H10W 72/884: {Die-attach connectors and bond wires}
- H10W 74/00: Encapsulations, e.g. protective coatings
- H10W 90/734: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/736: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H10W 90/754: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10W 90/756: {between a chip and a stacked lead frame, conducting package substrate or heat sink}
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Provided is a copper paste for pressure bonding, the copper paste at least containing two or more copper powders having different shapes and/or particle sizes and a solvent. The copper paste has a viscosity of 10 Pa·s or more and 200 Pa·s or less. The ratio of the total mass of the two or more copper powders to the mass of the copper paste, A, is 0.60 or more and less than 0.82. When the index of bulkiness, H, is defined as H=C/(A×B), H is 0.75 or more and 1.00 or less, wherein A is as defined above, B represents the film thickness of a coating film formed by applying the copper paste to a substrate, and C represents the film thickness of a dried coating film formed by drying the coating film in an air atmosphere at 110° C. for 20 minutes.

## Claims

### Claim 1

A copper paste for pressure bonding, at least comprising: two or more copper powders having different shapes and/or particle sizes; and a solvent;
wherein the copper paste has a viscosity of 10 Pa·s or more and 200 Pa·s or less at 25° C.,
A is 0.60 or more and less than 0.82, and
H is 0.75 or more and 1.00 or less,
wherein A represents a ratio of a total mass of the two or more copper powders to a mass of the copper paste, and
H represents an index of bulkiness defined as H=C/(A×B),
wherein B represents a film thickness of a coating film formed by applying the copper paste to a member to be bonded, and
C represents a film thickness of a dried coating film formed by drying the coating film in an air atmosphere at 110° C. for 20 minutes.

### Claim 2 (depends on 1)

The copper paste for pressure bonding according to claim 1,
wherein the two or more copper powders having different shapes and/or particle sizes contain spherical copper particles and non-spherical copper particles,
the spherical copper particles have a cumulative volume particle size at a cumulative volume of 50 vol %, DSEM50, of 60 nm or more and 300 nm or less, as determined by image analysis using a scanning electron microscope, and
the non-spherical copper particles have a cumulative volume particle size at a cumulative volume of 50 vol %, D50, of 0.1 μm or more and 50 μm or less, as determined by a laser diffraction scattering particle size distribution measurement method.

### Claim 3 (depends on 2)

The copper paste for pressure bonding according to claim 2,
wherein the non-spherical copper particles are flat copper particles, and
the flat copper particles have a length of a major axis, a, of 1 μm or more and 50 μm or less, as determined by image analysis using a scanning electron microscope.

### Claim 4 (depends on 2)

The copper paste for pressure bonding according to claim 2,
wherein the non-spherical copper particles are flat copper particles, and
the flat copper particles have an aspect ratio of 2 or more and 80 or less.

### Claim 5 (depends on 1)

The copper paste for pressure bonding according to claim 1,
wherein at least one of the two or more copper powders has a crystallite size ratio E/D of 1.1 or greater, wherein D represents a crystallite size at 100° C. and E represents a crystallite size at 300° C., as determined by high-temperature X-ray diffractometry.

### Claim 6 (depends on 1)

The copper paste for pressure bonding according to claim 1, wherein the copper paste is used for bonding a member to be bonded having a thickness of not more than 10 times the film thickness of the dried coating film, C.

### Claim 7 (depends on 1)

The copper paste for pressure bonding according to claim 1,
wherein the solvent has a boiling point of 180° C. or higher.

### Claim 8 (depends on 1)

A semiconductor device comprising: a semiconductor element having a thickness of 0.25 mm or less, and a substrate; wherein the semiconductor element and the substrate are bonded to each other with the copper paste for pressure bonding according to claim 1.

### Claim 9 (depends on 1)

A semiconductor device comprising: a first substrate on which a semiconductor element having an area of more than 25 mm2 is mounted, and a second substrate; wherein the first substrate and the second substrate are bonded to each other with the copper paste for pressure bonding according to claim 1.

### Claim 10 (depends on 1)

A method for producing a semiconductor device,
the method comprising:
providing a stack in which a member to be bonded, the copper paste for pressure bonding according to claim 1, and another member to be bonded are put in this order, and
firing the copper paste for pressure bonding while a pressure of 0.1 MPa or more is applied;
wherein at least one of the members to be bonded includes a semiconductor element.

### Claim 11

A method for producing a copper paste for pressure bonding,
the method comprising: mixing two or more copper powders having different shapes and/or particle sizes, and a solvent,
wherein the mixing step is regulated such that the copper paste has a viscosity of 10 Pa·s or more and 200 Pa·s or less at a shear rate of 10 s−1, and
the mixing step is further regulated such that A is 0.60 or more and less than 0.82, and H is 0.75 or more and 1.00 or less,
wherein A represents a ratio of a total mass of the two or more copper powders having different shapes and/or particle sizes to a mass of the copper paste, and
H represents an index of bulkiness defined as H=C/(A×B),
wherein B represents a film thickness of a coating film formed by applying the copper paste to a member to be bonded, and
C represents a film thickness of a dried coating film formed by drying the coating film in an air atmosphere at 110° C. for 20 minutes.