# US 2025/0149474 A1 · Selective Dielectric Capping for Hybrid Bonding

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149474 A1
- Document ID: US20250149474A1
- Status: Published application
- Kind: A1
- Application number: 18/809,472
- Filed: 2024-08-20
- Published: 2025-05-08
- Earliest claimed: 2023-11-03
- Assignees: Applied Materials, Inc.; Nanyang Technological University
- Applicants: Applied Materials, Inc.; Nanyang Technological University
- Inventors: Prayudi LIANTO; Chuan Seng TAN
- Web page: https://patentgrep.com/patent/US20250149474A1

## CPC

- H10P 72/0416: {with the semiconductor substrates being dipped in baths or vessels}
- H10P 14/69391: {the material containing aluminium, e.g. Al2O3}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 90/12: {Preparing bulk and homogeneous wafers}
- H10P 90/1914: {using bonding}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10W 72/01904: {using temporary auxiliary members, e.g. using sacrificial coatings or handle substrates}
- H10W 72/01921: {using local deposition}
- H10W 72/01961: {Chemical or physical modification, e.g. by sintering or anodisation (patterning H10W72/01951)}
- H10W 72/07236: {Soldering or alloying}
- H10W 72/921: {Structures or relative sizes of bond pads}
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/934: {Cross-sectional shape, i.e. in side view}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10W 72/953: {not comprising solid metals or solid metalloids, e.g. polymers, ceramics or liquids}
- H10W 80/102: {Controlling the environment during the bonding, e.g. the temperature or pressure}
- H10W 80/301: {Bonding techniques, e.g. hybrid bonding}
- H10W 80/312: {characterised by the direct bonding of electrically conductive pads}
- H10W 80/327: {characterised by the direct bonding of insulating parts, e.g. of silicon oxide layers}
- H10W 80/721: {having structure or size changed during the connecting}
- H10W 80/732: {having shape changed during the connecting}
- H10W 90/792: {between multiple chips}
- H10W 90/794: {between a chip and a stacked insulating package substrate, interposer or RDL}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for increasing dielectric bonding strength during wafer-level processing is incorporated into a hybrid bonding process. A method may include immersing a substrate into a chemical bath at atmospheric conditions where the chemical bath forms a self-assembled monolayer on metal surfaces of the substrate and selectively depositing a high-k dielectric material to form a dielectric cap on dielectric surfaces of the substrate absent of the self-assembled monolayer.

## Claims

### Claim 1

A method for increasing dielectric bonding strength during wafer-level processing, comprising:
immersing a substrate into a chemical bath, wherein the chemical bath forms a self-assembled monolayer on at least one metal surface of the substrate; and
selectively depositing a dielectric material to form a dielectric cap on at least one dielectric surface of the substrate absent of the self-assembled monolayer.

### Claim 2 (depends on 1)

The method of claim 1, wherein immersing the substrate into the chemical bath occurs at atmospheric pressure and ambient temperature.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
removing the self-assembled monolayer from the substrate;
bonding the dielectric material of the substrate to another substrate with surfaces covered by the dielectric material by contacting substrates together; and
annealing substrates to bond metal surfaces together.

### Claim 4 (depends on 3)

The method of claim 3, further comprising:
removing the self-assembled monolayer using a plasma-based process for approximately 10 seconds to approximately 60 seconds.

### Claim 5 (depends on 3)

The method of claim 3, wherein the substrate is a die.

### Claim 6 (depends on 3)

The method of claim 3, wherein annealing occurs at a temperature of approximately 150 degrees Celsius.

### Claim 7 (depends on 1)

The method of claim 1, wherein the chemical bath includes an alkanethiol.

### Claim 8 (depends on 7)

The method of claim 7, wherein the alkanethiol has a linear structure or a benzene ring structure.

### Claim 9 (depends on 1)

The method of claim 1, wherein the dielectric material is a high-k dielectric material.

### Claim 10 (depends on 9)

The method of claim 9, wherein the high-k dielectric material is aluminum oxide or hafnium oxide.

### Claim 11 (depends on 1)

The method of claim 1, wherein the substrate is immersed in the chemical bath for approximately 10 minutes to approximately 30 minutes.

### Claim 12 (depends on 1)

The method of claim 1, wherein the metal surface is copper, silver, gold, palladium, platinum, cobalt, titanium, nickel, or combinations thereof.

### Claim 13 (depends on 1)

The method of claim 1, wherein a thickness of the dielectric material is greater than zero nm to approximately 10 nm.

### Claim 14

A method for increasing dielectric bonding strength during wafer-level processing, comprising:
immersing a substrate into a chemical bath, wherein the chemical bath forms a self-assembled monolayer on at least one metal surface of the substrate and wherein immersing the substrate into the chemical bath occurs at atmospheric pressure and ambient temperature; and
selectively depositing a high-k dielectric material to form a dielectric cap on at least one dielectric surface of the substrate absent of the self-assembled monolayer, wherein a thickness of the high-k dielectric material is greater than zero nm to approximately 10 nm.

### Claim 15 (depends on 14)

The method of claim 14, wherein the substrate is immersed in the chemical bath for approximately 10 minutes to approximately 30 minutes.

### Claim 16 (depends on 14)

The method of claim 14, further comprising:
removing the self-assembled monolayer from the substrate;
bonding the high-k dielectric material of the substrate to another substrate with surfaces covered by the high-k dielectric material by contacting substrates together; and
annealing substrates to bond metal surfaces together.

### Claim 17 (depends on 16)

The method of claim 16, further comprising:
removing the self-assembled monolayer using a plasma-based process for approximately 10 seconds to approximately 60 seconds.

### Claim 18 (depends on 14)

The method of claim 14, wherein the chemical bath includes an alkanethiol with a linear structure or a benzene ring structure.

### Claim 19 (depends on 14)

The method of claim 14, wherein the high-k dielectric material is aluminum oxide or hafnium oxide.

### Claim 20

A non-transitory, computer readable medium having instructions stored thereon that, when executed, cause a method for increasing dielectric bonding strength during wafer-level processing to be performed, the method comprising:
immersing a substrate into a chemical bath, wherein the chemical bath forms a self-assembled monolayer on at least one metal surface of the substrate and wherein immersing the substrate into the chemical bath occurs at atmospheric pressure and ambient temperature; and
selectively depositing a dielectric material to form a dielectric cap on at least one dielectric surface of the substrate absent of the self-assembled monolayer.