# US 2025/0149450 A1 · Thinned semiconductor package and related methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149450 A1
- Document ID: US20250149450A1
- Status: Published application
- Kind: A1
- Application number: 19/011,366
- Filed: 2025-01-06
- Published: 2025-05-08
- Earliest claimed: 2018-03-15
- Assignees: Semiconductor Components Industries, LLC
- Applicants: Semiconductor Components Industries, LLC
- Inventors: Yusheng LIN; Takashi NOMA; Francis J. CARNEY
- Web page: https://patentgrep.com/patent/US20250149450A1

## CPC

- H10W 20/4424: {Copper alloys}
- H10W 74/014: {using batch processing}
- H10W 20/40: Interconnections external to wafers or substrates, e.g. back-end-of-line [BEOL] metallisations or vias connecting to gate electrodes
- H10W 72/012: {of bump connectors, dummy bumps or thermal bumps}
- H10W 72/019: {of bond pads}
- H10W 72/20: Bump connectors, e.g. solder bumps or copper pillars; Dummy bumps; Thermal bumps
- H10W 72/30: Die-attach connectors
- H10W 72/90: Bond pads, in general
- H10W 74/129: {forming a chip-scale package [CSP]}
- H10W 74/141: {the encapsulations being on at least the sidewalls of the semiconductor body}
- H10W 72/01251: {Changing the shapes of bumps}
- H10W 72/926: {Multiple bond pads having different sizes}
- H10W 72/944: {Dispositions of multiple bond pads}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

Implementations of semiconductor packages may include a die having a first side and a second side opposite the first side, a first metal layer coupled to the first side of the die, a tin layer coupled to the first metal layer, the first metal layer between the die and the tin layer, a backside metal layer coupled to the second side of the die, and a mold compound coupled to the die. The mold compound may cover a plurality of sidewalls of the first metal layer and a plurality of sidewalls of the tin layer and a surface of the mold compound is coplanar with a surface of the tin layer.

## Claims

### Claim 1

A method for forming a thinned semiconductor device, the method comprising:
providing a semiconductor device comprising:
a wafer comprising a first side and a second side;
a plurality of recesses extending into the first side of the wafer;
a plurality of bumps coupled to the first side of the wafer; and
a mold compound coupled over the plurality of bumps and within the plurality of recesses;
thinning the second side of the wafer to the plurality of recesses;
coupling a backside metal layer to the second side of the wafer, wherein the backside metal layer is patterned and provides structural support for the wafer; and
thinning the mold compound to expose the plurality of bumps.

### Claim 2 (depends on 1)

The method of claim 1, further comprising singulating the thinned semiconductor device through the mold compound to form a plurality of singulated semiconductor packages.

### Claim 3 (depends on 2)

The method of claim 2, wherein an outermost perimeter of the backside metal layer coupled to each singulated semiconductor package is less than an outermost perimeter of each semiconductor package.

### Claim 4 (depends on 1)

The method of claim 1, wherein the thinned semiconductor device comprises a plurality of steps between the backside metal layer and the wafer.

### Claim 5 (depends on 1)

The method of claim 1, wherein an outer surface of the mold compound is coplanar with an outer surface of the plurality of bumps.

### Claim 6 (depends on 1)

The method of claim 1, wherein the plurality of bumps comprises three metal layers.

### Claim 7 (depends on 2)

The method of claim 2, wherein at least one singulated semiconductor package comprises two or more die.

### Claim 8

A method for forming a semiconductor package, the method comprising:
forming one or more contacts on a first side of a wafer;
forming a plurality of recesses into the first side of the wafer;
applying a mold compound to the first side of the wafer, wherein the mold compound at least partially encapsulates the one or more contacts and fills the plurality of recesses;
backgrinding a second side of the wafer to reach the plurality of recesses and separate a plurality of die from the wafer;
coupling a backside metal layer comprising multiple layers to a second side of the plurality of die;
grinding the mold compound; and
singulating the mold compound at the plurality of recesses to form a plurality of semiconductor packages;
wherein the backside metal layer extends to an outermost sidewall of each semiconductor package of the plurality of semiconductor packages.

### Claim 9 (depends on 8)

The method of claim 8, wherein the backside metal layer contacts the mold compound.

### Claim 10 (depends on 8)

The method of claim 8, wherein the backside metal layer comprises at least three metal layers.

### Claim 11 (depends on 8)

The method of claim 8, wherein the mold compound is directly coupled to a sidewall of each singulated semiconductor package.

### Claim 12 (depends on 8)

The method of claim 8, wherein grinding the mold compound comprises grinding the mold compound to form a planar surface between the mold compound and the one or more contacts.

### Claim 13 (depends on 8)

The method of claim 8, wherein the backside metal layer covers an entire backside of the plurality of die.

### Claim 14 (depends on 8)

The method of claim 8, wherein the one or more contacts comprise two or more metal layers.

### Claim 15 (depends on 8)

The method of claim 8, wherein at least one singulated semiconductor package comprises a second die.

### Claim 16

A method for forming a thinned semiconductor device, the method comprising:
providing a semiconductor device comprising:
a wafer comprising a first side and a second side;
a plurality of recesses extending into the first side of the wafer;
a plurality of bumps coupled to the first side of the wafer; and
a mold compound coupled over the plurality of bumps and within the plurality of recesses;
thinning the second side of the wafer to the plurality of recesses;
coupling a backside metal layer to the second side of the wafer, wherein the backside metal layer comprises a plurality of metal layers.

### Claim 17 (depends on 16)

The method of claim 16, further comprising singulating the thinned semiconductor device into a plurality of singulated semiconductor packages.

### Claim 18 (depends on 17)

The method of claim 17, wherein the backside metal layer covers an entire backside of each singulated semiconductor package.

### Claim 19 (depends on 16)

The method of claim 16, wherein the backside metal layer comprises three metal layers.

### Claim 20 (depends on 16)

The method of claim 16, wherein an outer surface of the mold compound is coplanar with an outer surface of the plurality of bumps.