# US 2025/0149378 A1 · Semiconductor Device, Method of Manufacture by Monitoring Relative Humidity, and System of Manufacture Thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149378 A1
- Document ID: US20250149378A1
- Status: Published application
- Kind: A1
- Application number: 19/014,922
- Filed: 2025-01-09
- Published: 2025-05-08
- Earliest claimed: 2021-08-27
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Yun Chen Teng; Chen-Fong Tsai; Han-De Chen; Jyh-Cherng Sheu; Huicheng Chang; Yee-Chia Yeo
- Web page: https://patentgrep.com/patent/US20250149378A1

## CPC

- H10P 72/0456: {in-line arrangement}
- H10P 90/1914: {using bonding}
- H10D 30/0195: {forming inner spacers between adjacent channels, e.g. changing their shapes or sizes}
- H10D 30/0198: {forming source or drain electrodes wherein semiconductor bodies are replaced by dielectric layers and the source or drain electrodes extend through the dielectric layers}
- H10D 30/031: {of thin-film transistors [TFT]}
- H10D 30/507: {characterised by inner spacers between adjacent channels}
- H10D 30/6729: {characterised by the electrodes}
- H10D 30/6733: {Multi-gate TFTs}
- H10D 30/6735: {having gates fully surrounding the channels, e.g. gate-all-around}
- H10D 62/118: {Nanostructure semiconductor bodies}
- H10D 62/121: {oriented parallel to substrates}
- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10D 64/01: Manufacture or treatment
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10P 10/12: {Bonding of semiconductor wafers or semiconductor substrates to semiconductor wafers or semiconductor substrates (preparing SOI wafers using bonding H10P90/1914)}
- H10P 72/0428: {Apparatus for mechanical treatment or grinding or cutting}
- H10P 72/0604: {Process monitoring, e.g. flow or thickness monitoring}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/364: {of IGFETs}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/251: {Source or drain electrodes for field-effect devices}
- H10D 84/0149: {Manufacturing their interconnections or electrodes, e.g. source or drain electrodes}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 86/201: {the substrates comprising an insulating layer on a semiconductor body, e.g. SOI (H10D86/40 take precedence)}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

A method of forming a semiconductor device includes loading a first wafer and a second wafer into a wafer bonding system. A relative humidity within the wafer bonding system is measured a first time. After measuring the relative humidity, the relative humidity within the wafer bonding system may be adjusted to be within a desired range. When the relative humidity is within the desired range, the first wafer is bonded to the second wafer.

## Claims

### Claim 1

A method of forming a semiconductor device, the method comprising:
moving a first wafer and a second wafer through a first load lock into a treatment area using a first transfer robot;
moving the first wafer and the second wafer to a surface treatment station in the treatment area using a second transfer robot;
performing a plasma activation step on the first wafer and the second wafer, while maintaining a relative humidity in the treatment area in a range of 20% to 60%;
moving the first wafer and the second wafer from the treatment area through a second load lock into a bonding area;
moving the first wafer and the second wafer to a cleaning station using a third transfer robot, the cleaning station being in the bonding area;
dispensing a cleaning agent over the first wafer and the second wafer;
moving the first wafer and the second wafer to a bonding station using the third transfer robot, the bonding station being in the bonding area; and
bonding the first wafer and the second wafer to each other.

### Claim 2 (depends on 1)

The method of claim 1, further comprising:
maintaining a relative humidity in the bonding area in a range of 20% to 70% while bonding the first wafer to the second wafer.

### Claim 3 (depends on 1)

The method of claim 1, further comprising:
maintaining a relative humidity in the bonding area in a range of 35% to 60% while bonding the first wafer to the second wafer.

### Claim 4 (depends on 1)

The method of claim 1, further comprising:
maintaining a relative humidity in the bonding area in a range of 39% to 45% while bonding the first wafer to the second wafer.

### Claim 5 (depends on 1)

The method of claim 1, further comprising:
maintaining a relative humidity in the treatment area in a range of 20% to 60% prior to moving the first wafer and the second wafer to the surface treatment station.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
maintaining a temperature in the bonding area in a range of 15° C. to 45° C. while bonding the first wafer and the second wafer.

### Claim 7

A method of forming a semiconductor device, the method comprising:
moving a first wafer and a second wafer into a surface treatment station;
performing a plasma activation step on the first wafer and the second wafer, wherein the plasma activation step is performed in a relative humidity in a range of 20% to 60%;
moving the first wafer and the second wafer to a cleaning station;
dispensing a cleaning agent over the first wafer and the second wafer;
moving the first wafer and the second wafer to a bonding station; and
bonding the first wafer and the second wafer to each other, wherein bonding the first wafer and the second wafer is performed in a relative humidity in a range of 20% to 70%.

### Claim 8 (depends on 7)

The method of claim 7, wherein moving the first wafer and the second wafer to the cleaning station includes moving the first wafer and the second wafer to a bonding area through a load lock.

### Claim 9 (depends on 7)

The method of claim 7, wherein the cleaning station and the bonding station are in a same load-lock chamber.

### Claim 10 (depends on 9)

The method of claim 9, wherein the surface treatment station is in a different load-lock chamber than the cleaning station and the bonding station.

### Claim 11 (depends on 7)

The method of claim 7, wherein bonding the first wafer and the second wafer is performed in a relative humidity in a range of 35% to 60%.

### Claim 12 (depends on 7)

The method of claim 7, wherein bonding the first wafer and the second wafer is performed in a relative humidity in a range of 39% to 45%.

### Claim 13 (depends on 7)

The method of claim 7, further comprising:
prior to performing the plasma activation step, maintaining a relative humidity in a range of 20% to 60% in the surface treatment station.

### Claim 14

A method of forming a semiconductor device, the method comprising:
moving a first wafer and a second wafer into a surface treatment station;
performing a plasma activation step on the first wafer and the second wafer in a treatment area;
moving the first wafer and the second wafer to a cleaning station in a bonding area;
dispensing a cleaning agent over the first wafer and the second wafer;
moving the first wafer and the second wafer to a bonding station; and
bonding the first wafer and the second wafer to each other, wherein bonding the first wafer and the second wafer is performed in a relative humidity in a range of 20% to 70%.

### Claim 15 (depends on 14)

The method of claim 14, further comprising:
maintaining a relative humidity in a range of 20% to 60% in the treatment area while performing the plasma activation step.

### Claim 16 (depends on 14)

The method of claim 14, wherein the bonding area and the treatment area are separated by a load-lock.

### Claim 17 (depends on 14)

The method of claim 14, wherein bonding the first wafer and the second wafer is performed in a relative humidity in a range of 42%+3%.

### Claim 18 (depends on 14)

The method of claim 14, wherein a temperature of the bonding area is in a range of 15° C. to 45° C. while bonding the first wafer and the second wafer.

### Claim 19 (depends on 14)

The method of claim 14, wherein the relative humidity is in a range of 35% to 60%.

### Claim 20 (depends on 14)

The method of claim 14, further comprising:
prior to performing the plasma activation step, maintaining a relative humidity in a range of 20% to 60% in the treatment area.