# US 2025/0149351 A1 · High-pressure wafer processing method using dual high-pressure wafer processing facility

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2025/0149351 A1
- Document ID: US20250149351A1
- Status: Published application
- Kind: A1
- Application number: 18/832,141
- Filed: 2023-01-10
- Published: 2025-05-08
- Earliest claimed: 2022-01-24
- Assignees: HPSP Co., Ltd.
- Applicants: HPSP Co., Ltd.
- Inventors: Sung Kil CHO
- Web page: https://patentgrep.com/patent/US20250149351A1

## CPC

- H10P 72/32: {between different workstations}
- H10P 14/6304: {Formation by oxidation, e.g. oxidation of the substrate}
- H10P 14/6316: {Formation by nitridation, e.g. nitridation of the substrate}
- H10P 14/6519: {the substance being oxygen}
- H10P 14/6524: {the substance being nitrogen}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P 32/20: Diffusion for doping of insulating layers
- H10P 72/0402: {Apparatus for fluid treatment (H10P72/0441, H10P72/0448 take precedence)}
- H10P 72/0431: {Apparatus for thermal treatment}
- H10P 72/0462: {characterised by the construction of the processing chambers, e.g. modular processing chambers}
- H10P 72/0468: {comprising a chamber adapted to a particular process}
- H10P 95/90: Thermal treatments, e.g. annealing or sintering
- H10P 72/3311: {Horizontal transfer of a batch of workpieces}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention provides a high-pressure wafer processing using a dual high-pressure wafer method processing facility, the method comprising the steps of: disposing a wafer in a first processing chamber of a first high-pressure wafer processing module; performing a first process, which corresponds to one among high-pressure oxidation, high-pressure nitridation, high-pressure carbon doping, and high-pressure heat treatment, on the wafer in the first processing chamber; transferring the wafer to a second processing chamber of a second high-pressure wafer processing module; and performing a second process, which corresponds to another among the high-pressure oxidation, the high-pressure nitridation, the high-pressure carbon doping, and the high-pressure heat treatment, on the wafer in the second processing chamber.

## Claims

### Claim 1

A high-pressure wafer processing method using a dual high-pressure wafer processing facility, the method comprising:
disposing a wafer in a first processing area of a first high-pressure wafer processing module;
performing a first process, which corresponds to one among high-pressure oxidation, high-pressure nitridation, high-pressure carbon doping, and high-pressure annealing, on the wafer in the first processing area;
transferring the wafer to a second processing area of a second high-pressure wafer processing module; and
performing a second process, which corresponds to another one among the high-pressure oxidation, the high-pressure nitridation, the high-pressure carbon doping, and the high-pressure annealing, on the wafer in the second processing area,
wherein the first high-pressure wafer processing module and the second high-pressure wafer processing module are disposed in one accommodation space,
the wafer is transferred from the first processing area to the second processing area, in the accommodation space, and
the first process and the second process are performed at a reaction pressure higher than an atmospheric pressure.

### Claim 2 (depends on 1)

The method of claim 1, wherein the reaction pressure of the high-pressure oxidation, the high-pressure nitridation, or the high-pressure carbon doping is determined within a range of 5 ATM to 20 ATM.

### Claim 3 (depends on 1)

The method of claim 1, wherein the reaction pressure of the high-pressure annealing is determined within a range of 3 ATM to 20 ATM.

### Claim 4 (depends on 1)

The method of claim 1, wherein a reaction temperature of the high-pressure oxidation, the high-pressure nitridation, or the high-pressure annealing is determined within a range of 400° C. to 600° C.

### Claim 5 (depends on 1)

The method of claim 1, wherein source gas for each of the high-pressure oxidation and the high-pressure nitridation includes any one of oxygen gas, water vapor, and ammonia gas.

### Claim 6 (depends on 1)

The method of claim 1, wherein the high-pressure carbon doping is performed at a reaction temperature below a thermal decomposition temperature of source gas for carbon doping, thus causing the source gas to chemically react with an insulation film of the wafer in its molecular state.

### Claim 7 (depends on 6)

The method of claim 6, wherein the reaction temperature of the high-pressure carbon doping is determined within a range of 400° C. to 600° C.

### Claim 8 (depends on 6)

The method of claim 6, wherein the source gas for carbon doping includes any one of ethylene gas and propylene gas.

### Claim 9 (depends on 1)

The method of claim 1, further comprising performing the high-pressure annealing on the wafer by using an in-situ method after performing any one of the high-pressure oxidation, the high-pressure nitridation, and the high-pressure carbon doping.

### Claim 10 (depends on 9)

The method of claim 9, further comprising performing a purge between any one of the high-pressure oxidation, the high-pressure nitridation, the high-pressure carbon doping, and the high-pressure annealing,
wherein the purge is performed while maintaining the reaction pressure and a reaction temperature in a previous process.

### Claim 11 (depends on 1)

The method of claim 1, wherein each of the first high-pressure wafer processing module and the second high-pressure wafer processing module further includes a protective area accommodating any one of the first processing area and the second processing area and maintained at a protective pressure, and
the protective pressure in the protective area is adjusted in conjunction with the reaction pressure to be higher than the reaction pressure.

### Claim 12 (depends on 1)

The method of claim 1, wherein the accommodation space is maintained at a pressure higher than the atmospheric pressure.

### Claim 13 (depends on 1)

The method of claim 1, wherein the transferring of the wafer to the second processing area of the second high-pressure wafer processing module includes unloading the wafer from the first processing area and then loading the wafer into the second processing area without a cooling process.

### Claim 14 (depends on 1)

The method of claim 1, wherein the performing of the second process, which corresponds to another one among the high-pressure oxidation, the high-pressure nitridation, the high-pressure carbon doping, and the high-pressure annealing, on the wafer in the second processing area includes confirming a process condition by considering a queue time after completing the first process.

### Claim 15 (depends on 1)

The method of claim 1, wherein the first process is the high-pressure oxidation, the second process is the high-pressure carbon doping, and
the reaction pressure of the high-pressure oxidation and the high-pressure carbon doping is determined within a range of 5 ATM to 20 ATM.

### Claim 16 (depends on 15)

The method of claim 15, wherein the second process further includes the high-pressure annealing performed using an in-situ method after the high-pressure carbon doping, and
the reaction pressure of the high-pressure annealing is determined within the range of 5 ATM to 20 ATM.

### Claim 17 (depends on 1)

The method of claim 1, wherein the first process is the high-pressure annealing, the second process is the high-pressure oxidation, and
the reaction pressure of the high-pressure annealing and the high-pressure oxidation is determined within a range of 5 ATM to 20 ATM.

### Claim 18 (depends on 1)

The method of claim 1, wherein the first process is the high-pressure annealing, the second process is the high-pressure nitridation, and
the reaction pressure of the high-pressure annealing and the high-pressure nitridation is determined within a range of 5 ATM to 20 ATM.

### Claim 19 (depends on 1)

The method of claim 1, wherein the first process is the high-pressure oxidation, the second process is the high-pressure annealing,
the reaction pressure of the high-pressure oxidation is determined within a range of 5 ATM to 20 ATM, and
the reaction pressure of the high-pressure annealing is determined within a range of 3 ATM to 20 ATM.

### Claim 20 (depends on 1)

The method of claim 1, wherein the first process is the high-pressure nitridation, the second process is the high-pressure annealing,
the reaction pressure of the high-pressure nitridation is determined within a range of 5 ATM to 20 ATM, and
the reaction pressure of the high-pressure annealing is determined within a range of 10 ATM to 20 ATM.